Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Carbonate containing thermites
MeshPL
Hazard to Others
***




Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 11:13
Carbonate containing thermites


So I'm not really into pyrotechnics. But last video by Cody's Lab about copper thermite made me wonder "what if you put an easily decomposable compound into such an energetic thermite? Would that make the thermite more dangerous due to high amount of gases being produced?"

So what coulb be such a compound?
I have some ideas. Ammonium carbonate and bicarbonate are one. There is also sodium bicarbonate. One could also add some kind of formate or oxalate. Ammonium oxalate seems interesting. Oxalic acid itself may be a good idea too. Finally, we can add (basic) copper carbonate to the thermite. Or just use Copper carbonate as the main ingredient.

The idea is that copper thermite is energetic but unlike typical explosive it does not produce hot, expanding gases, which is one of the most dangerous things explosives do. We can add some compounds, which produce them when decomposed, however. Or we can use copper carbonate which shoul react like that (I'm aware that CuCO3 is an idealisation):

3CuCO3 + 2Al --> 3Cu + Al2O3 + 3CO2

So if we added such a compounds to our thermite, we would make it produce some gases. But what would be the disadvantages? Well, such a compounds are not very dense. Copper oxide has a density of about 6g/cm^3. Copper carbonate is about 3g/cm^3. What that means, such a thermite has a much lower energy density and may not explode/react as fast as we want. When it comes to other compounds mentioned before, only oxalic acid and sodium bicarbonate are above 2g/cm^3. So, basically , we would add a bunch of filler to our thermite.

All in all, would you rather I throw a regular Cu/Al containg bomb at you or would you rather I put some (how much?) gas producing filler inside? Let's assume you want to survive. :P

But seriously, is it a completly dumb idea?

Edit: Also what would happen if I made a thermite with something like iron carbonate or other carbonate instead of oxide?
[Edited on 18-6-2016 by MeshPL]

[Edited on 18-6-2016 by MeshPL]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 11:42


"But seriously, is it a completly dumb idea?"
Yes.
The hot gases would spatter white hot stuff everywhere.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 18-6-2016 at 11:48


There are plenty of thermites that produce gas and CuO/Al is one. The copper is given off as a gas in this case.

By using a carbonate instead of an oxide you will lower the energy density. This will slow the reaction down. You will need to do the calculations but you might also get it into the realm of thermodynamic infeasibility.

You should try and see -- but don't go putting anything into a pipe bomb before you know its characteristics well and until you have your own (guaranteed) deserted quarry and an excellent remote detonation system.

FTR, Extractions and Ire recently "liked" a nice thermite video: https://www.youtube.com/watch?v=GRSlGt26uUA
It shows the calculations you can do (although I have not checked his work.) It also illustrates that guessing at an outcome can leave you surprised. Calculations first is a good way to go.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 12:14


Quote: Originally posted by MeshPL  


But seriously, is it a completly dumb idea?

Edit: Also what would happen if I made a thermite with something like iron carbonate or other carbonate instead of oxide?


I wouldn't call it smart, no.

Adding fillers to thermites often turns them into fizzlers because of the heat sink effect.

Iron carbonate doesn't really exist.




View user's profile View All Posts By User
MeshPL
Hazard to Others
***




Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 12:37


Well, I don't really have the specific reagents needed to do tests... but I may eventually do some tests using reagents at school next term, since there will be holidays very soon.

Yeah that's true copper is given of as a gas. But I think copper gas has enough energy to convert other stuff into more gases.

It would be nice to see which is the critical amount of filler. And it's effect on the reaction.

The idea of hot metal splattering everywhere sounds nice. But I'm afraid, that spalattering will be kinda slow.

And sure, no pipe bombs.

So, all in all, that is a rather dumb idea.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 18-6-2016 at 12:44


I wouldn't call it a dumb idea. Some things are only found out by exploring ideas and experimentation.
Just stay safe.

I am not predicting you'll get anything more vigorous than a normal copper thermite. But it might eject reaction products further.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 13:10


Quote: Originally posted by j_sum1  
But it might eject reaction products further.


And the point to that would be?

Something that doesn't allow any metal recovery but isn't really an explosive either.

[Edited on 18-6-2016 by blogfast25]




View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 18-6-2016 at 13:30


I didn't say there was a point to it. I was saying what I anticipated might happen. In other words, stand well back. The sparks might not be as hot but they might possibly fly further. (Or they might not.)



View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 19-6-2016 at 05:30


Adding powdered Teflon to thermite is done industrially to "pressurize the effluent"- That is, blow white hot metal out of the reaction at high speed... A purpose being, pyronoll metal piercing torch or similarly purposed linear cutting devices.

http://www.google.com/patents/US5372069

Some people want to use the hot reaction products to do work, rather than recover the reduced metals.




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
Bert
Super Administrator
Thread Moved
19-6-2016 at 05:32
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2016 at 06:07


Quote: Originally posted by Bert  
Adding powdered Teflon to thermite is done industrially to "pressurize the effluent"- That is, blow white hot metal out of the reaction at high speed... A purpose being, pyronoll metal piercing torch or similarly purposed linear cutting devices.

http://www.google.com/patents/US5372069

Some people want to use the hot reaction products to do work, rather than recover the reduced metals.


In that case the Teflon is an active ingredient, oxidising the Mg or Al in a very exothermic reaction.

An SM thread on the subject:

http://www.sciencemadness.org/talk/viewthread.php?tid=16741




View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 19-6-2016 at 09:08


You would probably also get:
3CuCO3 + 6Al --> 3Cu + 3 Al2O3 + 3 C

It is already known that "moist" Fe2O3 (containing Fe(OH)3) gives troubles/danger with thermite since the H2O liberated as a gas forms at high temperature H2 + O2 then Al takes the O2 and the H2 explodes afterwards into the air.

Same should happen with CuO (containing Cu(OH)2)

For the beauty of it you may try Cu(O2C-CO2) (Cu (II) oxalate)




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2016 at 09:40


Quote: Originally posted by PHILOU Zrealone  


It is already known that "moist" Fe2O3 (containing Fe(OH)3) gives troubles/danger with thermite since the H2O liberated as a gas forms at high temperature H2 + O2 then Al takes the O2 and the H2 explodes afterwards into the air.



Got any references for that?




View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 19-6-2016 at 11:21


Quote: Originally posted by blogfast25  
Quote: Originally posted by Bert  
Adding powdered Teflon to thermite is done industrially to "pressurize the effluent"- That is, blow white hot metal out of the reaction at high speed... A purpose being, pyronoll metal piercing torch or similarly purposed linear cutting devices.

http://www.google.com/patents/US5372069

Some people want to use the hot reaction products to do work, rather than recover the reduced metals.


In that case the Teflon is an active ingredient, oxidising the Mg or Al in a very exothermic reaction.

An SM thread on the subject:

http://www.sciencemadness.org/talk/viewthread.php?tid=16741


I am aware of various Teflon oxidized photo flash mixtures, this is not one.

The original cutting mixture was Aluminum powder/Iron oxides, plus some Nickel oxide to add further heat liberated by alloying the two metals- And a small amount of PTFE powder, which certainly DOES react with some of the Al on decomposing, but also produces propellant gas.

https://books.google.com/books?id=AK8zAwAAQBAJ&pg=PA904&...




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2016 at 13:22


Quote: Originally posted by Bert  


I am aware of various Teflon oxidized photo flash mixtures, this is not one.

The original cutting mixture was Aluminum powder/Iron oxides, plus some Nickel oxide to add further heat liberated by alloying the two metals- And a small amount of PTFE powder, which certainly DOES react with some of the Al on decomposing, but also produces propellant gas.



I see.




View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-6-2016 at 04:37


Quote: Originally posted by blogfast25  
Quote: Originally posted by PHILOU Zrealone  


It is already known that "moist" Fe2O3 (containing Fe(OH)3) gives troubles/danger with thermite since the H2O liberated as a gas forms at high temperature H2 + O2 then Al takes the O2 and the H2 explodes afterwards into the air.



Got any references for that?

What "that"?

1°) Thermal decomposition of water (thermolysis) happens at elevated temperatures and water molecule split back into its atomic components H2 and O2.
It is very low yielding at ambiant T°, but increases with T° (about 3% at 2200°C and nearly 50% at 3000°C).
2 H2 + O2 --Ear--> 2 H2O + heat
2 H2O + heat --Ead--> 2 H2 + O2
Energy of activation of reaction (Ear) is much tinier than Energy of activation of decomposition (Ead) so when the system is at high T° Ear and Ead are negligible vs the energetical state of the molécules (Energy System > Ead > Ear) so reaction happens in both sides at the time with a theorical maximum at 50%.

2°) From https://en.wikipedia.org/wiki/Thermite - Hazards
If, for some reason, thermite is contaminated with organics, hydrated oxides and other compounds able to produce gases upon heating or reaction with thermite components, the reaction products may be sprayed.

Edit:
3°) From Abrstract https://www.researchgate.net/publication/245206622_A_kinetic...
"Systematic thermogravimetric measurements under isothermal and non-isothermal conditions were performed in order to characterize kinetically the thermal dehydration and dehydroxylation processes. The dehydration of the bound water on the surface of γ-FeO(OH) observed at around 150°C obeyed the first-order law with an apparent activation energy of about 100 kJ mol−1, being recognized as controlled by diffusional removal of evolved water vapor through the stacking assemblage of plate-like crystalline powders. As for the hydrated γ-FeO(OH), the thermal dehydroxylation process at around 280°C, "

So Fe(OH)3, Fe(O)OH dehydrate at relatively low temperature...



[Edited on 20-6-2016 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 05:03


Quote: Originally posted by PHILOU Zrealone  

1°) Thermal decomposition of water (thermolysis) happens at elevated temperatures and water molecule split back into its atomic components H2 and O2.
It is very low yielding at ambiant T°, but increases with T° (about 3% at 2200°C and nearly 50% at 3000°C).
2 H2 + O2 --Ear--> 2 H2O + heat
2 H2O + heat --Ead--> 2 H2 + O2
Energy of activation of reaction (Ear) is much tinier than Energy of activation of decomposition (Ead) so when the system is at high T° Ear and Ead are negligible vs the energetical state of the molécules (Energy System > Ead > Ear) so reaction happens in both sides at the time with a theorical maximum at 50%.

2°) From https://en.wikipedia.org/wiki/Thermite - Hazards
If, for some reason, thermite is contaminated with organics, hydrated oxides and other compounds able to produce gases upon heating or reaction with thermite components, the reaction products may be sprayed.


Those bits are well known and not disputed. But that moist thermites can cause secondary hydrogen explosions remains unproved speculation as far as I'm concerned.

[Edited on 20-6-2016 by blogfast25]




View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-6-2016 at 06:02


Quote: Originally posted by blogfast25  
Quote: Originally posted by PHILOU Zrealone  

1°) Thermal decomposition of water (thermolysis) happens at elevated temperatures and water molecule split back into its atomic components H2 and O2.
It is very low yielding at ambiant T°, but increases with T° (about 3% at 2200°C and nearly 50% at 3000°C).
2 H2 + O2 --Ear--> 2 H2O + heat
2 H2O + heat --Ead--> 2 H2 + O2
Energy of activation of reaction (Ear) is much tinier than Energy of activation of decomposition (Ead) so when the system is at high T° Ear and Ead are negligible vs the energetical state of the molécules (Energy System > Ead > Ear) so reaction happens in both sides at the time with a theorical maximum at 50%.

2°) From https://en.wikipedia.org/wiki/Thermite - Hazards
If, for some reason, thermite is contaminated with organics, hydrated oxides and other compounds able to produce gases upon heating or reaction with thermite components, the reaction products may be sprayed.


Those bits are well known and not disputed. But that moist thermites can cause secondary hydrogen explosions remains unproved speculation as far as I'm concerned.

[Edited on 20-6-2016 by blogfast25]

Ah OK got it.

I have trown a few drops of H2O on 3100°C overheated iron surface from acethylen/N2O blowtorch and it makes a nice explosion with a clearly visible flame...
If following you no H2 and O2 are produced... where does the flame come from?

For the rest:
http://www.sciencedirect.com/science/article/pii/0038092X779...
"Hydrogen production from water utilizing solar heat at high temperatures ..."
They mention a low temperature acheived with...iron oxyde...but to be practical, you need to flash cool the product of reaction below the explosion/inflamation T° of H2/O2 what is technically hard. This process would ensure the storage of solar energy into H2 with a good yield...although I think electrolysis is much safer and higher yielding.

This is also interesting http://www.eolss.net/sample-chapters/c08/e3-13-03-01.pdf
Especially the graphs of products of reaction at the end as the function of T°

But I'm a true believer :):D;):P and open minded about sceptical people :P
So here another possible explanation:
Overheated Al powder and H2O stil produces Al2O3 and H2 at high temperature...this explains that ultrafine Al powder water gels are detonable...or propellant (see ALICE tread).
So even if the decomposition of water into H2O doesn't happen stricto senso from the heat, it will from the heat of the Aluminium acting like Mg would or an alcaline metal...


[Edited on 20-6-2016 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 09:13


@Philou:

Again, that water can be thermally cracked and reacts with hot electropositive metals to form hydrogen and metal oxide is not in dispute here.

These would be necessary conditions needed to make happen what you claim. But are they also sufficient conditions?

That’s not clear when you look at the situation more closely.

Thermites ‘burn’ by means of a reaction front that propagates in spatial dimensions. For example, schematically in just one direction, the reaction zone propagates in the x-direction:

Thermite propagation.png - 5kB

Temperature gradients cause heat fluxes (the wider arrows) from the hottest to cooler zones, in particular to the unreacted zone (highest temperature gradient). This is of course needed to make the reaction self-sustaining.

T is a function of both time and x, probably something like:

$$\frac{\partial T}{\partial t}=v(x)\frac{\partial T}{\partial x}+\kappa \frac{\partial^2T}{\partial x^2}+\frac{1}{\rho c_p}Q(x)$$
... a heat conduction advection equation where v(x) is the propagation speed of the reaction zone, kappa(x) the thermal diffusivity of the material and Q(x) the heat generated by the reaction.

The point is though that the temperature profile of the unreacted zone could easily allow the water to evaporate off (at T<sub>w</sub>, about 100 C), well below the temperatures needed to thermally crack the water or for it to react significantly with any hot metal.

[Edited on 20-6-2016 by blogfast25]




View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-6-2016 at 11:32


Quote: Originally posted by blogfast25  
@Philou:

Again, that water can be thermally cracked and reacts with hot electropositive metals to form hydrogen and metal oxide is not in dispute here.

These would be necessary conditions needed to make happen what you claim. But are they also sufficient conditions?

That’s not clear when you look at the situation more closely.

Thermites ‘burn’ by means of a reaction front that propagates in spatial dimensions. For example, schematically in just one direction, the reaction zone propagates in the x-direction:



Temperature gradients cause heat fluxes (the wider arrows) from the hottest to cooler zones, in particular to the unreacted zone (highest temperature gradient). This is of course needed to make the reaction self-sustaining.

T is a function of both time and x, probably something like:

$$\frac{\partial T}{\partial t}=v(x)\frac{\partial T}{\partial x}+\kappa \frac{\partial^2T}{\partial x^2}+\frac{1}{\rho c_p}Q(x)$$
... a heat conduction advection equation where v(x) is the propagation speed of the reaction zone, kappa(x) the thermal diffusivity of the material and Q(x) the heat generated by the reaction.

The point is though that the temperature profile of the unreacted zone could easily allow the water to evaporate off (at T<sub>w</sub>, about 100 C), well below the temperatures needed to thermally crack the water or for it to react significantly with any hot metal.

[Edited on 20-6-2016 by blogfast25]

The cracking and crackling recombination explosion occurs almost instantaneously as compared to the typical reaction time of the thermite...there should be no delay H2 and O2 is a detonating mix so when slighly cooled and in contact with a hot spot it recombines immediately.
True that such an event is hard to prove because the witnesses leaves the crash site during the incident :(.

On an energitical level nothing should distinguish H2O explosion by vapourisation vs H2O vapourisation (explosion) then decomposition into H2 and O2 and recombination into H2O...

Sole solution to cut the debate is a good spectroscopic photographic device proving the presence of H2 into the burning flame/melt.
I don't have that :(.

Or a filmed carefull comparative study of the mechanical work of
-Fe2O3/Al thermite vs Fe2O3/Fe(OH)3/Al thermite
-CuO/Al thermite vs CuO/Cu(OH)2/Al thermite
With the very same ingredients and overal the same amounts of Al/Fe and Al/Cu.

The 1D idealisation is maybe good for an horizontal cigarette burning of low diameter. Nice equation and graph by the way!

In 3D, you have also to play with:
-heat flux going upside from air bubbles (gaps into the initial powder) (density gradient)
-radiative heat flow all direction with efficiency depending on heat capacity of the various medias (air, Al, Fe2O3, Fe, Al2O3, H2O(g)).
-sparkling propagation upside and outside (downside is too resistant)
-flowing of denser metal going downside (density gradient)
-the mather contraction creating gaps/cavities that collapse allowing unreacted powder to fall downside
-convection of the molten metal and flux (liquid Fe2O3/Al2O3)
-coalescence of gases, liquid flux, molten metal

All this is just way to complicated to put into simple equations.
Reality is much more chaotic ;):P

[Edited on 20-6-2016 by PHILOU Zrealone]




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 13:49


Quote: Originally posted by PHILOU Zrealone  

All this is just way to complicated to put into simple equations.
Reality is much more chaotic ;):P



If we can successfully model something like Rayleigh–Bénard convection we can probably also model temperature gradients in a thermite mixture. The question is really not 'can it be done?' but rather 'is it worth doing?', which in the thermite case I'd say is 'No'.

In summary, I'd be far more convinced by your claims if they were accompanied by good old direct evidence. :)

[Edited on 20-6-2016 by blogfast25]




View user's profile View All Posts By User
mayko
International Hazard
*****




Posts: 1218
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline

Mood: anomalous (Euclid class)

[*] posted on 20-6-2016 at 15:54


I wouldn't call it a thermite, but I was surprised to discover that sodium carbonate can act as an oxidizer; mixed with magnesium powder, it produces an impressive flare. Potassium carbonate is also used in "yellow powder":
http://www.amateurpyro.com/forums/topic/755-yellow-powder/

I just tried out a mixture of 5.5 g basic copper carbonate and 4.5 g Mg powder (ie, a 33% excess of Mg to O). Ignited with Mg ribbon, it flared up, much tamer than CuO thermite. The flame was bright but had no particular color. What was most striking was this purple-red residue it left on the ceramic I ignited the mixture on, presumably a thin deposit of copper:



copper carbonate thermite residue.jpg - 410kB




al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 17:13


Quote: Originally posted by mayko  
What was most striking was this purple-red residue it left on the ceramic I ignited the mixture on, presumably a thin deposit of copper:


Probably. Scrape some off and test with nitric acid?




View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 24-6-2016 at 05:09


As some inexpensive metals can react with steam to liberate H2, I speculate that a thermite mix with some kind of inserted funnels (possibly porous) containing a metal hydrate or hydroxide (that would liberate its H2O at a higher temperature) might be interesting (but likely unsafe due to sputtering) to test out.

I recently read a patent that could recycle Cl2 in a reaction chain by heating CuCl2 + a metal. This could serve here as a high temperature chlorine source to replace oxygen.

More generally, porous funnels consisting of chemical mix upon contact with steam could be a source of a highly flammable gas cloud that could detonate subsequently with atmospheric oxygen (a thermobaric explosion, yes extremely unsafe).

Those with more knowledge of explosives noted for their rapid hot gas production could also be included in the design.

However, as we are talking about items that could serve potentially as tools of terror as well, I think a rather vague outline is in order along with a lot more obtuse theory.
------------------------------------

Note, the prior theoretical comments concerning sustainability of the thermite mix and propagation dynamics is made more complex by my suggestion of funnel zones (of various sizes and external material compositions) forming a heterogeneous reaction system.

Note, if my funnel structure totally dissipated at the commencement of the thermite, one would have, in effect, a non-homogenuous thermite reaction mix.

[Edited on 24-6-2016 by AJKOER]

[Edited on 24-6-2016 by AJKOER]
View user's profile View All Posts By User

  Go To Top