What is the best way to clean up battery graphite rods from used batteries? I would like to do some elctro chemistry at some point. I was thinking maybe a soak in HCl then distilled water?
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 16-6-2016 at 10:48


Fucking around with battery rods rarely ends well since they're small and usually consist of compressed carbon!

Graphite rods!

View user's profile View All Posts By User
Daffodile
Hazard to Others
***




Posts: 167
Registered: 7-3-2016
Location: Highways of Valhalla
Member Is Offline

Mood: Riding eternal

[*] posted on 16-6-2016 at 11:34


Use acetone and scrubbing, there's an adhesive of some sort, or wax.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3634
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 16-6-2016 at 14:58


I recovered four carbon rods from a lantern battery together with the zinc pots and MnO2/carbon paste.
I heated the rods to red heat to burn-off the unknown stuff.
don't do it over a domestic cooker as it may get messy ... dripping wax etc.
a bbq or similar is ok.
Unfortunately this technique ruins the nice press-fit metal caps.

EDIT: after recovering the carbon rods I bought graphite rods for the length - just easier / I'm lazy.

[Edited on 16-6-2016 by Sulaiman]
View user's profile View All Posts By User
OneEyedPyro
Hazard to Others
***




Posts: 280
Registered: 7-10-2015
Member Is Offline

Mood: No Mood

[*] posted on 16-6-2016 at 16:30


HCl should do a pretty good job getting rid of MnO2.
View user's profile View All Posts By User
Xenoid
National Hazard
****




Posts: 775
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline

Mood: Comfortably Numb

[*] posted on 16-6-2016 at 18:09


Quote: Originally posted by Daffodile  
Use acetone and scrubbing, there's an adhesive of some sort, or wax.


NO!!! - Don't use solvents or heating to remove the wax sealant!

It's there for a purpose, to help prevent electrolyte penetration, and the eventual disintegration of the rod, this is especially important if the rod is to be used in chlorate cells.

I would recommend just brushing with a toothbrush and warm soapy water.
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 16-6-2016 at 22:41


Ok cheers, seems worth a go. I might buy some longer ones at some point, postage has got silly price in the UK so i wait until i have a decent order and asked for a discount and combined postage when i can :D.
View user's profile View All Posts By User
DFliyerz
Hazard to Others
***




Posts: 241
Registered: 22-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2016 at 18:27


I usually just scrape it off with a knife
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2016 at 00:30


The lantern type of cells (4 cells in bigger battery) worked ok, but the ones i tried from single cells were rubbish and just crumbled, a little HCl and a wipe with a damp cloth seemed to work fine.

Thanks i can give electrolysis a go. I got a small 12V (i think!) solar panel from a caravan off ebay, its used but seems to be working ok, not very big and not much current but FREEEEE electric for some electrolysis.