tandpasta
Harmless
Posts: 30
Registered: 13-10-2014
Member Is Offline
Mood: No Mood
|
|
Removing smell from polypropylene bottles
I have two small sauce bottles made from pp which keep smelling like their previous contents, barbecue sauce and mustard. They've been through the
dishwasher multiple times, they've soaked for extended amounts of time in cleaning vinegar, diluted sodium hydroxide, and diluted nitric acid.
The smell is still there.
Why is the smell staying there? Did the sauces leach into the polymeric structure of the bottle? And how can I remove the smell (through chemical
means)?
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Normal undiluted Bleach will probably work, although you'll need to rinse them a LOT.
The theory is that the dilute (5%) sodium hypochlorite will oxidise everything, including all organics and any bacteria/virii that took up residence.
I have no idea if it can also oxidide polypropylene - i guess you will find out.
Let us all know if this suggestion works or not.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
I thought this thread would be about the smell of the bottles themselves. I have several old empty Nalgene bottles that smell terrible inside. They
all smell the same, so I suspect it's the plastic itself that smells. I wonder why this is and if it would be detrimental to anything I store inside.
Many washes with bleach is a good option to try for your problem, though.
|
|
OneEyedPyro
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 280
Registered: 7-10-2015
Member Is Offline
Mood: No Mood
|
|
Bleach might work if allowed to soak for long periods.
PP is a fairly non reactive plastic being impervious to most bases, acids and solvents but I believe turpentine will attack it. I'm sure a few washes
with that will do the trick if all else fails.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4547
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Quote: Originally posted by MrHomeScientist ![](images/xpblue/lastpost.gif) | I thought this thread would be about the smell of the bottles themselves. I have several old empty Nalgene bottles that smell terrible inside. They
all smell the same, so I suspect it's the plastic itself that smells. I wonder why this is and if it would be detrimental to anything I store inside.
Many washes with bleach is a good option to try for your problem, though. | I've noticed that about HDPE
Nalgene bottles too, whether new or old. I store a lot of things in them though (probably at least 20% of my reagents) and I haven't had any problems
yet...
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1850
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
Try leaving them in the dishwasher for 10-15 cycles. This reduces the small of PE bottles that had contained benzaldehyde to an acceptable though
still detectable level.
|
|
tandpasta
Harmless
Posts: 30
Registered: 13-10-2014
Member Is Offline
Mood: No Mood
|
|
I will try the bleach solution and let you know the results in a few days.
|
|
tandpasta
Harmless
Posts: 30
Registered: 13-10-2014
Member Is Offline
Mood: No Mood
|
|
The smell has gone, but not fully. I guess due to the low strength of the HCl solution (<5%). Is there any way to 'concentrate' the bleach?
|
|