RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Magnesium & Aluminum turnings, filings & chips - which alloys are acceptable?
I've had a difficult time finding Mg or Al in pure form anywhere as it is all some kind of an alloy, even if it is 95-97 Al or Mg (for the higher
Al/Mg percentages). There are so many different alloys of Al that I'm wondering when Al powders are purchased whether it is of an alloy or if it is
100% Al.
Does anyone know if there are any acceptable alloys for either Al or Mg? Any idea what aluminum foil composition is, or soda cans?
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
https://en.wikipedia.org/wiki/7068_aluminium_alloy
Scroll down for an extensive list of Al alloys.
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
This might be acceptable.
"This listing is for one pure magnesium ingot (99.9%) weighing approximately 1lb. This item is manufactured in the United States, and is delivered
with a certificate of analysis."
http://www.ebay.com/itm/Magnesium-Metal-Ingot-99-9-Pure-1lb-...
"These 99.95% minimum guaranteed. Pure magnesium metal ingots are quite impressive. We have these materials in just about any form and quantity that
you might be seeking, from shavings to metric tons. This listing is for one ingot that weighs about 16-18 pounds (typically between 16 and 17 pounds)
and measures about L 21.5" x W 5.75" (base)/W 4.25" (top) x H 2.75". This will be shipped by FedEx Ground. We now allow international orders on this
item. It will be shipped by USPS International Priority Mail Flat Rate."
http://www.ebay.com/itm/Magnesium-Metal-Ingot-Large-99-95-Pu...
[Edited on 24-1-2016 by Morgan]
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3634
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Since about 80% of magnesium production is from China, eBay is your best bet.
For my electrochemistry experiments I bought magnesium
powder, 99.8%
ribbon, 99,95%
rod, 99.99%
of course by the time that you receive it there will be some surface oxidation,
the rods were oiled and clingwrapped, very little visible oxidation, but not shiny,
the most visibly oxidised was the ribbon edges,
the powder is grey, not shiny, so must also be oxidised somewhat.
So if you count oxides, it is probably very difficult to get high purity,
cutting the middle out of rods would probably be best, but I've only got two so I shall not try.
99.8% aluminium on eBay but I can't think of anything domestic that is pure aluminium
maybe cooking foil that does not include recycled aluminium,
which would contain magnesium from drink can tops.
|
|
careysub
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline
Mood: Lowest quantum state
|
|
Aluminum foil is almost all 1235 alloy which is 99.35% aluminum. This is pretty much guaranteed because the aluminum does not roll out into a foil as
easily if it has a higher alloy content, and this one alloy is produced in huge amounts for this purpose. Grocery foil is optimized for cheap
production.
There are higher alloy foils that have greater strength that are used in manufacturing, but you won't find them on a roll in your grocery store.
[Edited on 24-1-2016 by careysub]
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by RogueRose ![](images/xpblue/lastpost.gif) |
Does anyone know if there are any acceptable alloys for either Al or Mg? Any idea what aluminum foil composition is, or soda cans?
|
Define "acceptable." Your intended use dictates the grade of aluminum you need.
According to several people in this thread, soda cans use alloys in the 3000 series for the body and alloys from the 5000 series for the ends. I think actually the bottom is the
same as the walls, and only the lid uses the 5000 alloy. The 3000 series are alloyed with about 1% manganese, and the 5000 are alloyed with around 5%
of magnesium. There's a nice table here.
|
|
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
All commercially purchased metal is going to be named as an alloy. Consider alloy series 11XX aluminum. These are substantially pure aluminum metal.
The alloy number designates the acceptable levels of other metals not removed in refining. Alloy 1100 is min. 99% Al up to 99.5%. Alloy 1199 is 99.99%
which is excellent purity.
Unfortunately you are very unlikely to see 11XX series aluminum for sale anywhere common because it is mechanically weak.
As mentioned above, aluminum foil is an alloy but the drug cooks seem to have made it work fine in application as mercury amalgam at least.
For magnesium I suggest buying turnings from galliumsource or somewhere similar. Pure magnesium isn't used in consumer applications. The few places it
is used tend to be alloyed with aluminum to give more favorable mechanical properties. They do sell small blocks as a mediocre firestarter to be lit
with a flint and steel but the cost would be quite high compared to just buying bulk turnings.
|
|