Pages:
1
2 |
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
I need method to prepare magnesium chloride from magnesium silicate or any available magnesium compounds
Hi guys!!
Any method to prepare magnesium chloride from magnesium silicate or any available magnesium compounds. I found that buying magnesium chloride is
pretty expensive for me, & that's all.
[Edited on 22-11-2015 by bluamine]
|
|
morsagh
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 187
Registered: 20-2-2014
Member Is Offline
Mood: No Mood
|
|
Dissolve chalk that is used for gymnastics (it is MgCO3) in HCl.
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
Are you sûre?! I mean i know available chalk here is calcium carbonate. Any alternative magnésium chemicals?
|
|
mayko
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1218
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
Make magnesium carbonate from sodium carbonate and magnesium sulfate, proceed with hydrochloric acid?
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1476
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
epsom salt MgSO4 + janitorial ammonia NH4OH / NH3 / H2O => Mg(OH)2 ppt +
(NH402SO4
filter off the Mg hydroxide to attack with HCl later, water the lawn with the ammonium sulfate
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
I think magnesium sulfate wouls be even more expensive for me this is why I
proposed magnesium silicate (baby powder) though I don't know any method to do that.
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
I found this equation below but i am not sure if that would work or no:
Mg3Si4O10[OH]2 + 3 H2SO4 = 4 SiO2 + 3 MgSO4 + 4 H2O
If yes, any specific conditions to realize it?
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Epsom salts is pretty widely available and should not be too expensive. The problem is that it is usually a heptahydrate and so you are never getting
as much as you think you are. It's more or less half a box of water. Shop around. Garden stores, supermarkets, pharmacies, hardware stores. The
cost should not be prohibitive.
Of course, if you need MgCl2 and can access that for roughly the same price then your should buy it directly and save yourself some bother.
|
|
mario840
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 20-1-2010
Member Is Offline
Mood: No Mood
|
|
the first reply is probably the best 300g 35% hydrochloric acid and 100 ml H20 warm up and add 90 -100g MgCO3 , easy synthesis readily available
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | Epsom salts is pretty widely available and should not be too expensive. The problem is that it is usually a heptahydrate and so you are never getting
as much as you think you are. It's more or less half a box of water. Shop around. Garden stores, supermarkets, pharmacies, hardware stores. The
cost should not be prohibitive.
Of course, if you need MgCl2 and can access that for roughly the same price then your should buy it directly and save yourself some bother.
|
I am not sure if buying magnesium chloride is not regulated someway, but if I do that I would get 100 100 mg impure tablets for 18$ or more, & I
think that is a bad deal.
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by mario840 ![](images/xpblue/lastpost.gif) | the first reply is probably the best 300g 35% hydrochloric acid and 100 ml H20 warm up and add 90 -100g MgCO3 , easy synthesis readily available
|
The problem is that I don't really know how can I find magnesium carbonate, & what is it used for
|
|
mario840
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 20-1-2010
Member Is Offline
Mood: No Mood
|
|
You wrote : "any available magnesium compounds" I thought MgCO3 you can easily buy, write to what Mg compound you got access ...
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Google "site:sciencemadness.org whatever-you-are-looking for"
Top answer :
http://www.sciencemadness.org/talk/viewthread.php?tid=10374
[Edited on 22-11-2015 by aga]
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
the mineral 'magnesite' is pure MgCO3. it is quite common. I have found several pieces in railway ballast. that's about as cheap as it gets.
Beginning construction of periodic table display
|
|
mario840
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 20-1-2010
Member Is Offline
Mood: No Mood
|
|
Yes you can obtain MgCl2 from magnesite powder but after washing with boiling water couple of times
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1476
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
personally, I like the epsom salt way. its really cheap, available and the byproduct is useful. Ive seen it for roughly 1$/lb, of course some stores
are expensive. so check a couple. I wanted the magnesium hydroxide for refractory and used that method. ended up getting a nice bag of ammonium
sulfate for free. after heating the solution, it was filtered when cool to get Mg(OH)2, and I just left the solution in shallow trays in
the sun for a day or two. there were quite a few 3/8" crystals in the product. happy lawn
the filtering isn't fast or super fun, but I felt like heating it for a short while and filtering after cool reduced the amount of super fine gunk.
still not expedient.
|
|
Bert
|
Thread Moved 22-11-2015 at 21:19 |
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
I've purchased 5lb containers of MgCl2*6H2O for like $2 as driveway deicer.
|
|
ave369
Eastern European Lady of Mad Science
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 596
Registered: 8-7-2015
Location: No Location
Member Is Offline
Mood: No Mood
|
|
As far as I know, magnesium silicate reacts with acids, including hydrochloric, just fine, turning into a gel of silicic acid, and all magnesium going
into solution as chloride, nitrate or sulfate.
Smells like ammonia....
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
I dis not find in any hardware store, but u did find it in pharmacies, so it is expensive there..
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by ave369 ![](images/xpblue/lastpost.gif) | As far as I know, magnesium silicate reacts with acids, including hydrochloric, just fine, turning into a gel of silicic acid, and all magnesium going
into solution as chloride, nitrate or sulfate. |
I was thinking about that, but I was not sure because of the complicated formula of magnesium silicate Mg3Si4O10(OH)2
[Edited on 24-11-2015 by bluamine]
|
|
morsagh
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 187
Registered: 20-2-2014
Member Is Offline
Mood: No Mood
|
|
For sure chalk that is used for gymnastics is MgCO3, normal chalk for drawing on blackboard is CaCO3.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Or
CaSO4. I believe that the sulfate is more common for blackboard chalk.
|
|
bluamine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 17-8-2015
Member Is Offline
Mood: No Mood
|
|
I am mocking, but believe me this is the first time I know chalk is used for gymnastics.. I am wondering what can it be used for
|
|
karlos³
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline
Mood: oxazolidinic 8)
|
|
It is used to dry your palms.
In my country it is even called magnesia as its trivial name, and you use it before using some gymnastic equipment to prevent sliding down on it.
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 513
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by karlos³ ![](images/xpblue/lastpost.gif) | It is used to dry your palms.
In my country it is even called magnesia as its trivial name, and you use it before using some gymnastic equipment to prevent sliding down on it.
|
In my country it is called "magnesium powder" which makes it hard for me to find actual elemental magnesium powder.
|
|
Pages: