Filtration - any issue with using positive pressure instead of vacuum?
I was devising some improvised filtration devices and was wondering if I increase the pressure above the media to be filtered to like 30-60 PSI, would
that work to help increase speed of filtering?
Also, if I have a container that is 12" diameter where the air-space is and then a reduction down to 6" where the filter is located. There is more
surface area where the air pressure is, so would that increase the pressure over the filter medium? So would I get more pressure with what I just
explained vs a 6" straight pipe?
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
yes, no, no.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1702
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Short and to the point, Magpie :-)
Using high pressure rather than vacuum is a valid approach and has some benefits over vacuum as well. Filtering saturated solution with vacuum can be
a challenge as the pressure drop causes evaporation and cooling that can cause the solute to precipitate out in the filter. You can also achieve far
greater pressure differences than vacuum will permit.
We're not banging rocks together here. We know how to put a man back together.
|
|
subsecret
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 424
Registered: 8-6-2013
Location: NW SC, USA
Member Is Offline
Mood: Human Sadness - Julian Casablancas & the Voidz
|
|
Keep in mind that it's much easier to keep an apparatus together if it's under vacuum, rather than under pressure.
Fear is what you get when caution wasn't enough.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Pressure instead of Vacuum kinda makes it hard to do any washing.
|
|
Xenoid
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 775
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline
Mood: Comfortably Numb
|
|
Pressure filtering works wonderfully well, and is commonly used on an industrial scale.
Check out this thread, http://www.sciencemadness.org/talk/viewthread.php?tid=9630 a pressure filter built from PVC plumbing parts! Note the WARNING.
Cheers, Xenoid
|
|
Mesa
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 264
Registered: 2-7-2013
Member Is Offline
Mood: No Mood
|
|
Flow rates are a hell of a lot slower with positive pressure in my experience. I had the same idea in the past but quickly abandoned it.
|
|
Pumukli
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 695
Registered: 2-3-2014
Location: EU
Member Is Offline
Mood: No Mood
|
|
Once I tried applying a bit of pressure over a diethyl-ether containing solution/solid particles mixture, although not for filtering purposes, by a
hand bicycle pump. Could not even finish the first "stroke", the ether vapour "detonated" in the pressurized chamber - a plastic hypodermic syringe in
this case!
(We all know that it was not a real detonation, but this word seems to be the most accurate to describe the emotional effect it had on me.) ![:D](./images/smilies/biggrin.gif)
Based on this experince I would avoid pressurizing anything flammable with air. Maybe with inert gas it would be different.
|
|