chemical resistant film
Hello all. I've come across a plastic type film that seems to be resistant to a lot of different chemicals. The thing is, I don't have any real
strong acids, bases, solvents, etc. I was hoping that I could send some to someone that might be able to do some testing on it. I would also like to
get other opinions as to whether it is good or not. If things work out ok, then I can cut it into disks to send to other members here to seal
bottles that have plastic caps, for those that can't afford the more expensive storage bottles. Everyone knows those plastic caps don't ever last too
long. Let me know if someone is able and willing to help out their fellow scimad members. Here's a picture of the film I cut into strips for
testing.
If this is in the wrong place, please feel free to move it. Thanks everyone in advance for all the help.
![100_1165 (Medium).JPG - 79kB](https://www.sciencemadness.org/whisper/files.php?pid=416229&aid=42744)
[Edited on 17-8-2015 by alive&kickin]
[Edited on 17-8-2015 by alive&kickin]
|
|
kecskesajt
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 299
Registered: 7-12-2014
Location: Hungary
Member Is Offline
Mood: No Mood
|
|
You could also burn it.If it burns fast,it is NC.It can be used as a binder in pyrotechnics.
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Is it a polyimide film or a fluorinated polymer?
Or do you know the composition?
|
|
alive&kickin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 100
Registered: 10-11-2012
Member Is Offline
Mood: No Mood
|
|
kecskesajt, if it was NC, would it be resistant to acids and such? macckone, not sure what it is. I was hoping to find someone to test it, to see if
it's any good, and maybe venture a wild guess as to what it might be. Would probably be a long shot on that one though. If interested, let me know
and I'll get it in the mail asap.
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Honestly it looks like polyimide. Polyimide is fairly resistant to weak
acids but can be damaged by alkalis and strong acids. It will also
be damaged by long exposure to water.
Does it resist organic solvents? If it is resistant to acetone that
narrows it down considerably. Also does it burn easily?
|
|
alive&kickin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 100
Registered: 10-11-2012
Member Is Offline
Mood: No Mood
|
|
kecskeajt and macckone, doesn't burn at all, just kind of melts, also acetone does nothing to it. Like I said, if someone wants to play around with
it and let everybody know what they find out, maybe that would be quicker than a few guesses on the part of this newbie.
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
OK that pretty much means it must be polyimide or fluorinated. With leaning toward fluorinated because most polyimides don't melt. Next test would
be to measure weight gain after several hours in boiling water. Polyimide will gain significant weight and may break down completely.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4552
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Where did you "come across" this substance? Did it come as a packaging material for a product, or did you find it just lying in the street?
|
|
alive&kickin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 100
Registered: 10-11-2012
Member Is Offline
Mood: No Mood
|
|
zts16, I got it from a friend whose father was a chemist that passed away. He's not into chemistry, so when he was cleaning out the attic of his
fathers house, he came across several items that he knew I might be interested in. This was one of them. macckone, I'll try boiling it like you
suggested, but I'm not sure my scale is going to be accurate enough for it. I'll give it a try though. Thanks for all the suggestions and help.
|
|
deltaH
Dangerous source of unreferenced speculation
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline
Mood: Heavily protonated
|
|
Could it be that you stumbled onto some Nafion membrane, if so, NICE FIND!!!
|
|
alive&kickin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 100
Registered: 10-11-2012
Member Is Offline
Mood: No Mood
|
|
macckone, sorry it took so long, but when ma and grandma are canning in the kitchen, stay out of the way. I did like you said, boiled it in water for
4 hours, nothing, started with 1.1 grams, ended with 1.1 grams. Any other ideas?
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i'd just like to throw this in -- having looked into metal etching, nail polish seems somewhat resistant, although it contains nitrocellulose and some
other odd plastic, it seems to last even until the acid totally dries out, like 30% HCl with CuCl2*HCl complex
i have however seen tendencies of nitrocellulose hydrolyzing into nitric acid and the remainder somehow hydrolyzing, i'd guess when kept together with
hydrochloric acid for some time
i know personally that PTFE turns slightly clear before melting, and seems to be very hard to keep molten (i havent done much in it due to its
supertoxic nature, breathing in vapours may immediately make you faint, reference old plastic identification/safety handbook)
for figuring out metals, the most used method was observing the way the plastic would burn, whether it would crackle or soot, if it soots you could
suppose that it has some strong carbon-carbon bonds, like acetylene burning, where there isnt enough energy to break the tripple-bonds
i know PVC and PETeraphthalate can over time react with NaOH, PVC seems to somewhat crackle, where the other plastic will oftenly soften a slight
bit.. thumb rule is if a plastic is resistant to a strong base, then it wont be towards a strong acid
im getting bad at short replies..
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
It is probably some sort of fluorinated polymer.
PFA or similar, it could be nafion but there is no easy
way to tell the fluorinated polymers apart short of a
GC/MS and NMR.
|
|