vinny111
Harmless
Posts: 4
Registered: 4-6-2015
Member Is Offline
Mood: No Mood
|
|
ammonuim nitrate problem
hi i recently got ammonuim nitrate out of a few cold packs. i tested it by using lye mixed with this an and water and it produced ammonia gas. here is
the thing it produces clumps but when i go to dry it in oven it melts and turns into water again. the oven temp is at 150 degrees F so its not
decomping. why is it doing this? please let me know thanks
|
|
Loptr
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1348
Registered: 20-5-2014
Location: USA
Member Is Offline
Mood: Grateful
|
|
It doesn't decompose until well over 200C. You might be looking at either melted ammonium nitrate, or ammonium nitrate dissolved in its own water of
hydration. However, the melting point is 337.3°F, which you are no where near, so I would assume its the latter, in which case keep heating.
http://www.sciencemadness.org/talk/viewthread.php?tid=721
|
|
vinny111
Harmless
Posts: 4
Registered: 4-6-2015
Member Is Offline
Mood: No Mood
|
|
ok thanks i wasnt shure what had happened lol thanks very much
|
|
nitro-genes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1048
Registered: 5-4-2005
Member Is Offline
|
|
There is still too much water present, 10% water and ammonium nitrate forms an eutectic, melting at around 100 deg C. Just needs to dry longer...
|
|
vinny111
Harmless
Posts: 4
Registered: 4-6-2015
Member Is Offline
Mood: No Mood
|
|
ok ill keep heating it boiling out water how long does one boil?
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
until it's dry, or starts to decompose, then turn off the heat.
No, you can't leave it and go do something else in the meantime.
|
|
vinny111
Harmless
Posts: 4
Registered: 4-6-2015
Member Is Offline
Mood: No Mood
|
|
ok see i boiled it down til it was half its volume 600 ml and then cooled it in freezer to crystallize. i didnt know if an will boil right out with
the water. im new so dont judge me
|
|
Bert
|
Thread Moved 8-6-2015 at 18:15 |