'Glowstick' chemistry
Upon recently receiving a stack of glowsticks (the things that you bend, and they glow for a certain period of time), I became curious as to how they
work.
I figured they would be based on a chemical reaction with 2 components, the compound in the glass tube, and the compounds in the outer plastic tube.
I looked up and found a howstuffworks article on the subject, and found out that the compound in the glass tube is hydrogen peroxide, and the other
component is phenyl oxalate ester.
From this I thought of two things:
1. If the hydrogen peroxide is strong (say 30%+ maybe?), then it could be a potential source.
2. The article mentions a by product is phenol, so maybe phenol could be retrieved from spent glowsticks (which can be found aplenty after raves and
what not). ![:)](./images/smilies/smile.gif)
Comments?
|
|
HNO3
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 211
Registered: 10-11-2004
Location: America
Member Is Offline
Mood: No Mood
|
|
Unfortunately all light sticks aren't created the same. Some light sticks have two complex organic molecules reacting to produce light.
\"In the beginning, God...\" Wait a minute, God doesn\'t exist!!!!!!!!!! \"OK, in the beginning, ummm, hydrogen...\" Wait a minute, what about the
laws of thermodynamics? \"OK, in the beginning, ummm.....UMMMMM, what\'s left to choose from?
|
|
cyclonite4
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
Any ideas on what these molecules may be?
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
sparkgap
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline
Mood: chaotropic
|
|
I'm more inclined to the guess that the crystals in the glow-sticks are triboluminescent; that is to say, they glow when you apply stress of any
sort to the crystals.
But maybe your glow-sticks are different. I see no sloshing liquid in mine. ![:D](./images/smilies/biggrin.gif)
sparky (^_^)
[Edited on 30-3-2005 by sparkgap]
"What's UTFSE? I keep hearing about it, but I can't be arsed to search for the answer..."
|
|
Hermes_Trismegistus
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 602
Registered: 27-11-2003
Location: Greece, Ancient
Member Is Offline
Mood: conformation:ga
|
|
ahem...
If I may, I was all hot and bothered a few months back about synthing some luminescent chems. I beleive i made a boast about glowing by christmas or
some such before getting sidetracked by a somewhat poor performance in my physics midterm and cutting out the extra-curriculars.
I did do a fair bit of research, and found a sticking point in the form of pthalic anhydride...one of the pre-precursors for luminol.
I wish you the best of luck and here is a little help?
Attachment: Cyalume.doc.pdf (118kB) This file has been downloaded 6206 times
Arguing on the internet is like running in the special olympics; even if you win: you\'re still retarded.
|
|
Hermes_Trismegistus
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 602
Registered: 27-11-2003
Location: Greece, Ancient
Member Is Offline
Mood: conformation:ga
|
|
luminol synth
asdf
Attachment: luminol synth.doc (42kB) This file has been downloaded 1830 times
Arguing on the internet is like running in the special olympics; even if you win: you\'re still retarded.
|
|
cyclonite4
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
Thanks...
Thanks for the files Hermes... quite interesting. ![:)](./images/smilies/smile.gif)
Still, it seems the definition from howstuffworks sticks. Cyalume is a phenyl oxalate ester [Bis(2,4,6-trichlorophenyl)oxalate], and the
reaction involves Hydrogen Peroxide.
Noone would happen to know the concentrations of reactants in the glowsticks would they?
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Luminescent Chemosensors: from Molecules to Nanoparticles
Hopefully not off topic: I read this article and this thread came to mind......solo
--------------------------------------------------------------------
Luminescent Chemosensors: from Molecules to Nanoparticles
Luca Prodi
New J. Chem., 2005, (1), 20 - 31
DOI: 10.1039/b411758a
PDF
![](http://img49.exs.cx/img49/9764/nj0290011qy.jpg)
Abstract
The need to develop sensors for different target analytes is well-recognised and confirmed by the considerable research efforts spent for the
preparation of more and more efficient sensory devices. In our laboratories we have been working on this subject for the past few years and in this
contribution some selected examples of the systems we have studied will be presented. Through the discussed compounds, the reader will be able to
follow our step-by-step approach towards this fascinating research field. The first essential move for a fruitful strategy in the development of
efficient macroscopic sensory devices is a thorough understanding of the systems responsible for the binding event and of its consequent transduction
into a detectable signal. These species are often molecular or supramolecular structures that behave as molecular-level sensory devices, which are
usually referred to as chemosensors. Among them, fluorescence-based chemosensors present many interesting features, such as high sensitivity and
versatility. Starting from this first and fundamental step our aims and future perspectives will be presented. There is still a great demand for ever
more efficient chemosensors; nanostructured systems such as nanoparticles, in which signal amplification can be obtained, will certainly play a very
important role in this field. For this reason this contribution concludes with a section on the results obtained on nanoparticles, which are the
natural carry-over of our research work.
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
Chaoslord
Harmless
Posts: 3
Registered: 19-8-2002
Location: Lisbon/Oslo
Member Is Offline
Mood: No Mood
|
|
Luminescence
Basically (and in general) you need two things :
A (un)substituted Diphenyl oxalate + a dye
Plus H2O2 with cat. ammounts of NaOH
If needed, I can post further about this subject
Bibliopharmacophile
|
|
a_bab
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 458
Registered: 15-9-2002
Member Is Offline
Mood: Angry !!!!!111111...2?!
|
|
The luminol only lasts about 30 seconds or so.
The stuff in the light sticks is 9,10-bis(phenylethynyl)anthracene, and the glass tube has H2O2. Attached is a document with some stuff about
chemoluminiscence.
@Sparky: The triboluminiscence phenomena is very short; the light output takes just a few fractions of a ms (while the crystal is in a "bent" state)
Attachment: chem light.txt (9kB) This file has been downloaded 1980 times
|
|
EtherBunny
Harmless
Posts: 11
Registered: 2-2-2004
Member Is Offline
Mood: adrenergic
|
|
This is a little off-topic, but a_bab, where did you get that document? It says anthracene is very toxic. Actually, it's not anywhere as bad as some
other polyclic aromatic hydrocarbons (people in my lab work with anthracenes and friends a lot) and is much less reactive than benzenoids and
napthalenes.
One of the interesting things about anthracene is that it's quite fluorescent (yellow-green) in its pure form. So is phenanthrene (blue). Rubrene is
also a really neat compound. It's extremely red in its pure form, hence the name, but I do not know if it fluoresces at all...
|
|
a_bab
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 458
Registered: 15-9-2002
Member Is Offline
Mood: Angry !!!!!111111...2?!
|
|
I can't remember; it's a compilation of different stuff from the web. The antracene is so carcinogenic that it is entitled so in the chemistry manuals
from the 50's. As about the toxicity, I don't know; in the light sticks ithey use an antracene compound, which would change the matters a bit.
|
|
EtherBunny
Harmless
Posts: 11
Registered: 2-2-2004
Member Is Offline
Mood: adrenergic
|
|
Huh. I've actually never read about anthracenes being carcinogenic to any great degree. Benzanthracenes, yes, but not straight-up anthracene.
|
|