Author: Subject: Hydrolysis of Nylon 6,6 to obtain Putrescine
nelsonB
Hazard to Self
**




Posts: 71
Registered: 5-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 27-3-2015 at 01:14
Hydrolysis of Nylon 6,6 to obtain Putrescine


Hi
i have been thinking some way of making Putrescine
and i remembered that it is used in making Nylon 6,6
So i have been searching some data about Nylon
http://www.polymerprocessing.com/polymers/PA66.html
here its say its 226.32 g/mol

from that info we know how much is a moles of Nylon
what if we mix it with 1 moles of sodium hydroxide (80 gram)
with some water could we hydrolise it back to Sodium adipate and Putrescine ?
with maybe the help of some other solvent

[Edited on 27-3-2015 by nelsonB]
View user's profile View All Posts By User
Etaoin Shrdlu
National Hazard
****




Posts: 724
Registered: 25-12-2013
Location: Wisconsin
Member Is Offline

Mood: Insufferable

[*] posted on 27-3-2015 at 06:31


It's nylon 4,6 that incorporates putrescine, and you'll want acid hydrolysis. 6,6 uses hexamethylenediamine.
View user's profile View All Posts By User
subsecret
Hazard to Others
***




Posts: 424
Registered: 8-6-2013
Location: NW SC, USA
Member Is Offline

Mood: Human Sadness - Julian Casablancas & the Voidz

[*] posted on 27-3-2015 at 06:51


Yes, using acid hydrolysis won't immediately produce the amine (rather the salt), so you can isolate it when you actually want to release the stench.



Fear is what you get when caution wasn't enough.
View user's profile View All Posts By User
Praxichys
International Hazard
*****




Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline

Mood: Coprecipitated

[*] posted on 27-3-2015 at 09:24


Quote: Originally posted by Etaoin Shrdlu  
It's nylon 4,6 that incorporates putrescine, and you'll want acid hydrolysis. 6,6 uses hexamethylenediamine.

Yes. Nylon 4-n will yield putrescine, nylon 5-n will yield cadaverine, and 6-n will yield hexamethylenediamine. All pretty stinky. You may not be able to find anything less than 6-6 though.




View user's profile Visit user's homepage View All Posts By User
nelsonB
Hazard to Self
**




Posts: 71
Registered: 5-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 27-3-2015 at 10:45


Thank reminding me this Etaoin Shrdlu
Now the question is where we can find Nylon-4,6
in't that a nylon that is less used than other type.

[Edited on 27-3-2015 by nelsonB]
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 28-3-2015 at 12:14


Hexamethylenediamine isn't very stinky. It's a solid at room temperature with a peppery ammoniacal smell.



This just in: 95,5 % of the world population lives outside the USA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org