SimpleChemist-238
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 147
Registered: 28-9-2014
Member Is Offline
Mood: Chlorine Trifloride Flame Thrower
|
|
Separation of metals from Non Lead Solder
I was hoping there was a method for separating the menials in non lead solder. The main metals in solder are Tin, coper indium and silver. The solder
I have is Tin and silver. I guess That if I wanted tin I could just use it as is but can I remove the silver? Maybe adding nitric acid to make tin
oxide and silver nitrate?
[Edited on 28-9-2014 by SimpleChemist-238]
|
|
Brain&Force
Hazard to Lanthanides
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
Then you'd want to remove the silver by adding copper to the silver nitrate to get silver metal. Or you could add salt to precipitate the silver as
AgCl.
[Edited on 28.9.2014 by Brain&Force]
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
SimpleChemist-238
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 147
Registered: 28-9-2014
Member Is Offline
Mood: Chlorine Trifloride Flame Thrower
|
|
awesome thanks
|
|
SimpleChemist-238
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 147
Registered: 28-9-2014
Member Is Offline
Mood: Chlorine Trifloride Flame Thrower
|
|
I am going to try dissolving the alloy in HCl and whats left over is silver.
|
|
TheChemiKid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline
Mood: No Mood
|
|
There will also be copper left. It may be tough to see because it a very fine precipitate.
|
|
SimpleChemist-238
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 147
Registered: 28-9-2014
Member Is Offline
Mood: Chlorine Trifloride Flame Thrower
|
|
how well does it act as a electrode
|
|
Bezaleel
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 444
Registered: 28-2-2009
Member Is Offline
Mood: transitional
|
|
As far as I remember, dissolving solder in nitric acid, produces hydrated SnO, not Sn2+. This is precipitated as a white to yellowish rather
voluminous precipitate, called tin butter (SnO.xH2O). I used this procedure to separate tin and lead from a piece Sn/Pb solder wire, the lead
remaining in solution.
I imagine the same to happen with alloys of tin and silver, the silver remaining in solution.
|
|
SimpleChemist-238
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 147
Registered: 28-9-2014
Member Is Offline
Mood: Chlorine Trifloride Flame Thrower
|
|
Cool, thank you for the info.
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
https://www.youtube.com/watch?v=G1sq4hnrBgM
"Pretty Tin crystals grown by electrolysis of Tin(II) Chloride solution.
The video is in real time."
https://www.youtube.com/watch?v=Af9GAUYDrlQ
"in the upper lefthand corner (anode) is a chunk of 95/5 tin/antimony electrical solder wrapped in filter paper to catch the bits of antimony that
drop off as the tin dissolves"
|
|