Author: Subject: Making Bakelite (Periodic Videos)
Argentum
Harmless
*




Posts: 36
Registered: 18-9-2014
Location: El culo del mundo
Member Is Offline

Mood: UV light

[*] posted on 20-9-2014 at 07:17
Making Bakelite (Periodic Videos)


I just finished watching a video from Periodic Videos showing how to synthesize bakelite.

They did not mention the amount of chemicals they used, only the names. And they did not mention the temperature and the time of the reaction

As far as I know they used phenol, formaldehyde, acetic acid and hydrochloric acid.

It seems to be something easy but I could not find further information around the forum, just a post saying that ammonia was used, it was heated for 24 hs and using an inert atmosphere.

Does anybody know further details about this process? I would like to synthesize a little bit, just for experimentation.

This is the link of the video:
https://www.youtube.com/watch?v=Vlh0YDRmZ0I

(I may have some spelling or grammar mistakes, I am still learning English :))
View user's profile View All Posts By User
Mailinmypocket
International Hazard
*****




Posts: 1351
Registered: 12-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-9-2014 at 07:22


This is a nice PDF with the preparation of Bakelite and other polymers:

http://www.bc.edu/schools/cas/chemistry/undergrad/org/spring...
View user's profile View All Posts By User
Argentum
Harmless
*




Posts: 36
Registered: 18-9-2014
Location: El culo del mundo
Member Is Offline

Mood: UV light

[*] posted on 20-9-2014 at 08:35


Thank you for that pdf. Anyways, I will need concentrated ammonia which is really difficult to find here. But I will see what can I do.
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 20-9-2014 at 08:42


Distill less concentrated into a smaller volume of water.
View user's profile View All Posts By User
Argentum
Harmless
*




Posts: 36
Registered: 18-9-2014
Location: El culo del mundo
Member Is Offline

Mood: UV light

[*] posted on 20-9-2014 at 13:44


I think I will do that
View user's profile View All Posts By User
Mailinmypocket
International Hazard
*****




Posts: 1351
Registered: 12-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-9-2014 at 16:15


Try here instead: http://jnec.org/lab-manuals/fe/ec_es_lab_manual.pdf

Just search google for "Bakelite synthesis experiment" and this is one of the results. No ammonia required here apparently.
View user's profile View All Posts By User
Argentum
Harmless
*




Posts: 36
Registered: 18-9-2014
Location: El culo del mundo
Member Is Offline

Mood: UV light

[*] posted on 21-9-2014 at 10:27


Thank you again! I do not usually get to the bottom of the search list