Pd/C
Hello,
I was wanting to know if there are any definitive tests to verify if a 5% reduced Pd on carbon catalyst is active? I received some at a reasonable
price but it did not seem to function well in a K formate/alcohol CTH reduction for a nitroethane.
Could I mix a small amount with a solvent and see if it gets warm? I have washed it with NaOH soln and then water.
It did not seem to react with formic acid.
He who fights with monsters should be careful lest he thereby become a monster. And if thou gaze long into an abyss, the abyss will also gaze into
thee.
|
|
plante1999
International Hazard
   
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
Test it by putting some in peroxide.
|
|
Dr.Bob
International Hazard
   
Posts: 2806
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
Mix some with methanol without an inert atmosphere and see if it catches fire....
If you have any simple nitroaromatic, like nitrobenzene, it will reduce easily and the color change should be easy to see, plus it will be easy to see
a change in TCL or any test for amines. If you cannot reduce that, then you are wasting your time on any other chemistry.
Bob
|
|
AvBaeyer
National Hazard
  
Posts: 655
Registered: 25-2-2014
Location: CA
Member Is Offline
Mood: No Mood
|
|
Why did you wash it with NaOH? I have never known Pd-C catalysts to need such treatment.
AvB
|
|