gas phase reduction of ag2o



Hi
I have a question on reduction of ag2o - I very much appreciate your comments:

I am trying to get the (presumably) ag2o tarnish off from greyish silver micro particles. Being a physicist, I had to look it up and it seems easy: heat it in air, or n2, to 450 K or so , and the ag2o will convert to ag.

but somehow it doesn't work. I put the sample in an oven (air) at 470K, it sits there for an hour - but it doesn't change its colour a bit (measured in a spectrometer).
any ideas? is 1 hour not sufficiently long?
thanks

sippin
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 30-5-2014 at 12:16


Fine powders of substances are very often darker than their respective bulk metals.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 30-5-2014 at 12:32


Acording to wikipedia, silver oxide decomposes at 553K (starts?), so you may want to calcine it at about 600K.



Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 30-5-2014 at 14:43


Quote: Originally posted by elementcollector1  
Fine powders of substances are very often darker than their respective bulk metals.


Powdered silver is dark gray. When did you get the particles? They're probably fine, unless you really need to get rid of any and all oxides.

If you want to make silver powder, try dissolving silver metal in nitric acid, then precipitating it back out with sodium metabisulfite solution.




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 30-5-2014 at 18:46


Quote: Originally posted by Brain&Force  
try dissolving silver metal in nitric acid, then precipitating it back out with sodium metabisulfite solution.


Sounds like a good way to make a mess. Silver doesn't work like gold in this regard.




Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
APO
National Hazard
****




Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline

Mood: Refluxing

[*] posted on 31-5-2014 at 02:14


Hydrogen is good for metal oxide reduction if your positive oxides are making it dark. Some good videos are avalible on youtube. Just look around.



"Damn it George! I told you not to drop me!"
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 31-5-2014 at 02:48


Just a thought, but the tarnish that forms on silver isn't usually the oxide so this bit of the OP is
wrong
"I am trying to get the (presumably) ag2o tarnish off from greyish silver micro particles"
It's not likely to be Ag2O.
It's more likely to be Ag2S
Heating in air might oxidise the sulphide to SO2 and leave the silver behind.