metal powders?
Hi, i wanted to just ask if you guys have some idea where you can buy metal powders?
I donĀ“t need large quantities.
Thanks in advance. /Nannah.
|
|
gdflp
Super Moderator
Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline
Mood: Staring at code
|
|
What kind of metal? Metals like magnesium and aluminum can easily be bought in small quantities(a few ounces to a pound) from eBay in powdered form.
[Edited on 8-4-2014 by gdflp]
|
|
Zyklon-A
International Hazard
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
I wouldn't buy from eBay, although it is possible, you might get a knock on your front door. Buy from Skylighter or some similar site.
|
|
gdflp
Super Moderator
Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline
Mood: Staring at code
|
|
Really??? Even a few ounces. I didn't think magnesium and aluminum were too bad. How else are you supposed to make thermite?
|
|
Zyklon-A
International Hazard
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
You might get a knock on your door. Probably not, but why take the risk? Skylighter is pretty cheap.
|
|
zed
International Hazard
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Build a simple machine, and ball mill your own. Sponenberg (Sp?) provides details in his book.
Seems to me, it is available, free, somewhere online.
Otherwise, there is restricted access to large quantities of certain powdered metals, and smaller mesh sizes are a definite no-no. Even here in the
U.S., where pyrotechnic materials are pretty widely available, we've got rules.
|
|
nannah
Hazard to Others
Posts: 136
Registered: 20-12-2013
Member Is Offline
Mood: No Mood
|
|
Im looking for somewhere or someone that offers small quantities of all the metals. Mg, Ni, Al, Co, Fe, Zn, Hg and all the other elements are of
interest in the future im sure.
|
|
Metacelsus
International Hazard
Posts: 2538
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Hg powder might be hard to find .
|
|
nannah
Hazard to Others
Posts: 136
Registered: 20-12-2013
Member Is Offline
Mood: No Mood
|
|
Haha. Yeah, you got me there.
but i Think u get what i mean.
|
|