First Run: Purification of Aluminum
Hey all, I've just recently introduced myself to the wonderful world of science after several years of learning it in school and some research in the
wonderful world of Google. Right now. Other than a few flasks and a scientific calculator I only have rudimentry tools until i get some actual lab
equipment (a .01g scale and some graduated cylinders to begin with), but I have come up with a question that I cannot seem to find a Direct answer
for... How can I purify Al2 from scrap aluminum with unknown contaminents? After that, how could I purify Cu?
I have a chunk of an old radiator waiting to be ripped down and sent out to the scrap yard, and thought that instead of spending the next two days
working on it, busting my knuckles. ect., there's got to be an easier way... NaOH!
Just for kicks I decided to prepare a concentrated (but not saturated) solution of NaOH to which i added the contaminated Al and observed the
reaction. I have to wait until I get the tools to measure weight and volume to actually calculate M but I could use a little help with the theory. The
Reaction so far:
NaOH(aq)+Al(s)-->Al2(OH)3(aq)+H2(g)
After this, im lost as to what to do next... In the Bayer Process, the solution is filtered before CO2(g) is bubbled through it, precipitating out
Al203, right? http://www.elmhurst.edu/~chm/vchembook/327aluminum.html
But other sources state that the reaction goes as follows:
Al2O3 + 2 NaOH + 3 H2O → 2 NaAl(OH)4
2 NaAl(OH)4 + CO2 → 2 Al(OH)3 + Na2CO3 + H2O
2 Al(OH)3 → Al2O3 + 3 H2O when heated to 980*C
http://en.wikipedia.org/wiki/Bayer_process
But from there, I add more heat to decompose the oxide into Al and 02(g)?
Which, if either, is correct/feasible? Or, is there an easier/better way of extracting pure aluminum from the contaminated alloy?
![:(](./images/smilies/sad.gif)
*BTW, the reason I thought of NaOH over H2SO4 was to dissolve the Al without dissolving the Cu, then reacting the copper alloy with H2SO4 to yield
Copper (II) Sulfate
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
It is gonna be harder then that, aluminium needs a lot of energy to extract, something that can hardly be done at home. You could turn it to aluminium
sulfate at best.
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
Would simply melting the aluminum fins with borax be a better route then? And what about the copper? What about the process won't work, which step is
the most difficult and how can I go about trying it? I seem to learn more from my failures than successes. And please, excuse my ignorance, as I know
only a little about metalwork, and less about metallurgy. I decided for my first couple of experiments to purify/collect my own elemental metals as
well as learn how to turn what I have into what I can experiment with... Like all college students I only have access to what I have and what Home
Depot can give me (cheaply of course). I know it is a basic and foolish way to start but I have decided to start with what I can do... Au is on the
top of my list, but I'm gonna need more than just a mason jar and a hotplate for that.
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Any practical purification of aluminium is going to involve very high temperatures, so for a first experiment its a pretty bad idea. If you are
dead-set on purifying a metal, you could try to purify copper.
One way would be to purify by electrolysis of CuSO4. Another would be to displace the copper with zinc or a similar reactive metal.
To start you off in the right direction, I recommend watching the videos posted by "nurdrage" on youtube.
Also regarding melting aluminium under borax, I'm not sure what that would achieve other than contaminating the aluminium even further. Having said
that, if you can melt aluminium you should as it is great fun!
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
I would recommend you to start with copper, it is a quite noble metal (not much reactive), as such, it is easy to work with and require a lot less
energy then active metals like aluminium.
Zinc could another idea.
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
I want to play with zinc as well, but that's a little lower on the list. Is there anything I can do with the Al hydroxides, chlorides, sulfates, ect.
that is fun/worthwhile without delving into electricity? Could I use them to precipitate/isolate other metals on the list? And what would be a good
way to seperate the Cu from the copper-lead-tin-whatever alloy?
H2SO4+alloy-->CuSO4(aq)+PbSO4(s)+other impurities?
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
Does not work like that. You will have to read a bit more about chem. Not all metals react similarly, copper, lead, and many other metals do not
dissolve in sulpuric acid. Nothing to do with aluminium compounds at your skills level.
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
I havent experimented with anything other than what my chem class allows me to yet
Im past most of the basic safety and calculations, and am now learning more advanced equations and laws, but I lack practical/lab time (most of it
spent on the basics like, more recently, the dehydration of CuS04, B.P. elevation, F.P. depression and clock reactions). I want to try some more
advanced experiments, and thought that seperating these two pieces of scrap should be fairly simple. What should I try next then?
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
Buy some malachite mineral on ebay, a small cubic inch should be enough, and try to get the copper out of this ore. It should be quite hard for you,
but it is doable. Malachite is a "variety" of copper carbonate.
http://www.ebay.ca/itm/74g-Natural-Azurite-and-Malachite-Cry...
http://www.ebay.ca/itm/Rare-Malachite-Rough-Healing-Stone-Sp...
[Edited on 9-3-2014 by plante1999]
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
Wonderful! I still want to construct a simple baking soda/vinegar reactor to bubble CO2 through the concoction I made today (once decanted and
filtered, of course) just to see if anything precipitates out, even if I get nothing out of it, since I have to wait for everything I bought to ship
anyway. Is there anything I could do with the H2 gasses when I saturate my solution to an excess of NaAl(OH)4, at my skill level, anyway?
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
Burn it for heat, else then that it need expenssive catalyst, it was not the best start sadly, but it how we learn isn't it?
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
It always starts with a question, and those questions usually get me to learn what I can't do or how not to do it lol But hell, I could always hook it
up to the lawnmower, its starting to feel like springtime again. http://www.youtube.com/watch?v=lKX_4feFLnM
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
Are you just trying to separate the Copper from the Aluminum in order to get a higher price then just selling it as ACR scrap? If so I can assure you
that mechanical separation is the way to go and I could help you with that if needed as I have been scraping my entire life.
Hell my first play house as a kid was built by money made from scrap metal and I now run a business doing just that.
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
You could, although it may be dangerous, be careful as always with chemistry.
I never asked for this.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
That's what its been sitting around for, i just havent had the motivation to go freeze my a** off, so I put it off for warmer weather, but I had the
question of an easier route... And yes, I'd rather waste some spare time to get the higher price of the copper once its separated. I just had the
thought that there might be all of $2.50 worth of alum. on it, so why not dump it in a bucket (so to speak) and dissolve it off and take the copper to
the yard... but again that got me wondering if and how i could purify them (via experimentation) so that I have more pure reagents to experiment with!
Until I hit this brick wall, of course. BTW, The only pure copper I have found on the interweb, other than copper strips of course, is a 1lb ingot of
.999 pure (stamped and everything) investment/labratory grade for $30+shipping. I'm sorry, but I can't justify paying 10x scrap value for something I
don't really need.
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
Copper wire is generally highly pure as impurity reduce electrical conduction.
You could probably make alum with it, I think mrhomescientist did a video about that.
I never asked for this.
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
Use a sawzall with a very rough wood blade and run it along the top of the aluminum. It will shread the Al off and leave you with copper. Its
relatively easy compared to Chemical separation of which I have tried it all.
Perhaps a NaCl/CuSO4 bath could be useful as it would also produce Cu during the reaction but mechanical separation is still tops trust me on that.
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
My first try with a sawzall over the summer cut into all the copper i was trying to save... but then again that was with a metal blade. My thought was
to put everything into a tub and soak in lye, bc as far as i can tell there is not much of a reaction on the copper, but that is where i got suck...
if i cant do anything with the aluminates, then its not worth it at all. ideally, i want to turn a metal into a salt (or two, or three) then back into
a metal, it doesnt matter what i start with as long as its relatively easy to procure. maybe ill start a new thread about it but i would like to do a
relatively simple and reversible reaction { Ab+Cd-->Cb+Ad, Ad+Eb-->Ab+Ed } where i react a compound, then turn the new product back to the
original compound later, like with the purification of gold, but with less dangerous reagents.
*aside, do you know how many vidoes of uninformed/uneducated people are on Youtube playing with aqua regia using measuring cups and camp grills?
Excuse my ignorace, I only ask stupid questions to entertain myself and annoy everyone else around me.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by theDudeintheHat ![](images/xpblue/lastpost.gif) | *aside, do you know how many vidoes of uninformed/uneducated people are on Youtube playing with aqua regia using measuring cups and camp grills?
|
Far, far too many.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
As Plante mentioned, I do indeed have a video on making alum from scrap aluminum (soda cans, in my case): http://www.youtube.com/watch?v=WAjrjY-JQ3o . Dissolving in base first serves to separate out much of the impurity metals that aren't amphoteric
like aluminum. You can grow beautiful large crystals with this type of alum.
As for getting back to the starting metal, it's exceedingly difficult for aluminum. It takes large amounts of energy since it's really quite a
reactive metal. There's a reason that it used to be more expensive than gold! According to wiki, aluminum production alone now consumes 5% of the
electricity generated in the US.
It would be more practical to start with less reactive metals like copper or silver. I like the idea to smelt copper from malachite, and I've been
wanting to try that myself for quite a while. The 'silver tree' experiment is a fun one to get silver crystals. Elecrolytic refining would be the
penultimate purification step for most metals, but I've never tried this myself.
It's great to have grand ideas and even better to consult with those who have already tried these things, before starting down that road yourself
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
The 'silver tree' looks pretty neat, I might try that one while I'm waiting for my new stuff to ship. I found another post on refining AgNO3 from
scrap silver, so that'll be a great lead- in... I can take some scrap silver, treat it with nitric, then grow those neat crystals with some of it and
heat the rest to decompose it. Impure metal->Metallic salt-> Pure Metal, I never though that silver would be simple and aluminum so complex! Now
I just gotta figure out how to make nitric. I have a base idea but does it have to be very concentrated (vacuum distillation?) or could it be weak if
I factor the molality?
Excuse my ignorace, I only ask stupid questions to entertain myself and annoy everyone else around me.
|
|
theDudeintheHat
Harmless
Posts: 10
Registered: 8-3-2014
Location: USA
Member Is Offline
Mood: Inflated
|
|
And that video looks oddly like the bayer process where adding acid causes the al(OH)3 to drop out of the system, but what was the final product,
potassium alum or Al2(SO4)3?
Excuse my ignorace, I only ask stupid questions to entertain myself and annoy everyone else around me.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Potassium alum. Because I used KOH as the base and H2SO4 as the acid, the final solution is a mix of K+,
Al3+, and SO42- ions. These come together to form the double salt KAl(SO4)2, which precipitates
first.
There's tons of videos on nitric acid preparation. NurdRage has a very good guide to a few different routes. I've got a video as well: https://www.youtube.com/watch?v=PYDFplw8iKg . The sulfuric acid you use does need to be concentrated, but vacuum distillation isn't required.
Without vacuum you can still produce red fuming nitric acid (RFNA), like I did. That's concentrated enough for anything I plan on doing, and the
NO2 contamination that makes it red doesn't interfere with anything I use it for. If you can get some scrap silver, trying to purify it is
a great learning experience. I've got a sterling silver chain that's broken that I'd like to try my hand at refining, just for fun.
|
|