Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Local Source for Borosilicate Glass?
dorkwad
Harmless
*




Posts: 17
Registered: 23-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 04:24
Local Source for Borosilicate Glass?


Hey there, I'm a beginner glassblower and I'm looking for any local source of borosilicate glass, my issue is that U.S. pyrex isn't really boro like it's supposed to be, it's soda-lime and it pops and cracks on any contact with my torch.

I could literally use any source, such as a bakeware that's actually borosilicate and not something else, can be in any shape even if it's a dildo although this will not be fun to buy, and yes I've already tried synthesizing it myself but boric acid is very dangerous and I'm waiting on a respirator order to get here.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2687
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 07:50


I have some broken Pyrex labware which is real borosilicate glass if you just want stuff to practice on. I gave one guy a whole box of broken glassware to melt down years ago, but I have a little bit more now. Plus I have a few items that might be repairable. Do you have access to a proper glass blowing torch and annealing oven, or are you trying to do this at home?
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 08:52


What's so dangerous about boric acid? I use that all the time and it's fairly benign - only a 1 health and reactivity hazard. Just wear gloves, and maybe one of those white dust filter masks if you're concerned.
View user's profile Visit user's homepage View All Posts By User
organicchemist25
Hazard to Others
***




Posts: 136
Registered: 12-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 13:08


Boric acid? Dangerous? I guess almost all chemicals are dangerous to some degree, I just would not go eating the stuff and wear gloves and wash hands when done working with it.

I have always thought of it as fairly safe.

I have some broken glassware as well. Some pieces are thick.
View user's profile View All Posts By User
dorkwad
Harmless
*




Posts: 17
Registered: 23-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 13:13


Quote: Originally posted by Dr.Bob  
I have some broken Pyrex labware which is real borosilicate glass if you just want stuff to practice on. I gave one guy a whole box of broken glassware to melt down years ago, but I have a little bit more now. Plus I have a few items that might be repairable. Do you have access to a proper glass blowing torch and annealing oven, or are you trying to do this at home?


I am doing it at home, but i've got a DIY kiln and a 6B national torch, along with the tanks, I have everything practically,
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2687
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 13:26


That's pretty impressive. If you want broken pieces of Pyrex, I think you can get some from someone here, mostly depends where you are located, as the shipping might get expensive, unless you just want pulverized shards, which fit easier into a flat rate box.
View user's profile View All Posts By User
dorkwad
Harmless
*




Posts: 17
Registered: 23-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 13:34


Thanks, I mean since it's used for glassblowing I can manipulate it from any shape into any other shape, I'm in Northern Virginia btw
View user's profile View All Posts By User
organicchemist25
Hazard to Others
***




Posts: 136
Registered: 12-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 13:55


I am in Va too. I am in DC usually, at least two weekends a month.
View user's profile View All Posts By User
dorkwad
Harmless
*




Posts: 17
Registered: 23-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2014 at 19:02


Oh nice, what kind of pricing would you put on that boro, organicchemist25?

I found out I probably won't be making my own glass because the recipe says 800 degrees Celsius for 12 hours lol... I can't sit next to a kiln all day and risk setting my house on fire, it's also more expensive and way harder than just buying the boro already chemically formed.
View user's profile View All Posts By User