Author: Subject: gluing different tyes of plastic pipe
dash143aua
Harmless
*




Posts: 1
Registered: 24-2-2014
Member Is Offline

Mood: No Mood

smile.gif posted on 24-2-2014 at 13:38
gluing different tyes of plastic pipe


Does anyone know how to glue cpvc pipc, pvc pipe, polyethylene, vinyl beside using screws, nuts or bolts. Their will be little pressure, they will be painted but their will be lots of moisture and water. Can any one please help me with this little problem. :)
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 24-2-2014 at 13:42


PVC cement will certainly work for PVC, not sure about most of the other plastics, but I assume it would work fine.



View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 24-2-2014 at 14:41


Before moving to my current lab I had an outside lab bench for making dimethylamine and other smelly reax. I plumbed it with 3/4 " pvc. I glued it with pvc glue and it held up for 7 years and would have kept on going for another 7. When I mix PVC with ABS there's another glue that works on both.
Oh and yes acetone works too. Cyclohexanone works and lets you work a little more slowly.

[Edited on 25-2-2014 by chemrox]




"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
bfesser
Resident Wikipedian
Thread Moved
24-2-2014 at 15:38
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 24-2-2014 at 16:02


From personal experience, acetone works great for solvent welding ABS and OK for solvent welding PVC. (I ran out of dedicated cement :D). The only problem is that it evaporates very quickly, so you have to work fast.

Specifically, are you planning to use PVC?




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User