sbreheny
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 145
Registered: 30-1-2014
Member Is Offline
Mood: No Mood
|
|
Tiny capillary defect in sealed tube
Hi all,
I have just begun to try some simple glassworking by trying to make sealed tubes from cheap glass "eyedropper" pipettes. I am using a Map-Pro gas
flame (Propylene gas I believe). It seems that every time I try to seal an end by just rotating the tube in the flame and letting it "ball up", I end
up with a tiny, tiny little capillary between the inner and outer surface. This persists even if I heat the end up hot enough to begin to drip and
then let it cool in air again. Anyone seen this before? What is it called? How do you prevent it? What causes it? I have attached an image from under
a microscope. The entire image shown is about 6mm across. The channel must only be a few microns in diameter. I have tried to adjust the colors in the
region right around the channel to make it more visible. It joins with a pronounced funnel-like shape at each end where it meets the surfaces.
Thanks for your help!
|
|
Nickdul
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 96
Registered: 13-2-2012
Location: Bulgaria
Member Is Offline
Mood: No Mood
|
|
I'm not at all knowledgeable of glassblowing, but I have had a similar issue a few days ago and I've had time to consider the reasons. I believe the
main cause of this is low flame temperature, or at least a slow heating Δ, which results in some modified characteristics of the glass. So, even
if you can reach sag or drip temperatures, maybe they are not sufficient.
The other guess is that the glass may not be cleaned up well, and residue from burning/pyrolysis on the glass prevents it from coming together.
Like I said, I am not well versed in glassblowing, although I find it one of the most challenging and beautiful crafts, and only for a lack of
resources have I not begun learning in, apart from sealing capillary tubes
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
As Nickdul said keep it clean, especially inside the tube. Do not hold it in a portion of the flame highly reducing, keep gas pressure away from the
end. Anneal properly (I love the box of Kaowool Fleaker provided me years ago). Get the glass to wet itself and seal just below the tip first to avoid
pressure from the gas flame getting inside the tube. Then work to seal the end. Keep it turning nonstop until a second before you stick it in Kaowool
to cool slowly with no air currents against the hot glass.
Study the link(s) below.
http://www.ilpi.com/glassblowing/tutorial_intro.html
http://www.ilpi.com/glassblowing/
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|