alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
Quote: Originally posted by Brain&Force ![](images/xpblue/lastpost.gif) | What was the process for plating Mg? If you did it in water, the metal would not reduce - it would convert to the hydroxide instead because the water
already releases enough protons to reduce the metal. You'd need an anhydrous solvent like THF or pyridine. |
I certainly did not do that, I was really beginning when I did this one. If my memory is good, I dissolved magnesium in HCl, then electroplated with a
magnesium strip as the anode. I took a look at the theory and it looks like you are right and I made hydroxide :p I'll have to redo this one. I still
wonder what is on the coin however.
[Edited on 4-2-2014 by alexleyenda]
|
|
ParadoxChem126
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 104
Registered: 5-4-2013
Location: USA
Member Is Offline
Mood: No Mood
|
|
Nothing special, just iodine sublimating and depositing onto a round-bottom flask full of ice.
|
|
kristofvagyok
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
The blood red reaction product is poured on ice-water to quench the reaction and to decompose the red colored iminium ion what was made by a
Vilsmeier–Haack reaction.
At the bottom of the water the yellowish impure reaction product separates what will be recrystallized to yield white snowflake like crystals.
If anyone would like to buy this picture, please visit: http://society6.com/labphoto/Blood-in-the-flask_Print#1=45
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
@kristofvagyok, that looks awesome!
@alexleyenda, Thanks, I wont to start a electro-deposited coin collection as well. Maybe I'll post a picture as soon as it gets big enough. I don't
know, I just never thought of putting weights on my stand.![;)](./images/smilies/wink.gif)
@ParadoxChem126, I'm to scared to sublimate any of my Iodine, scared that I might lose some that is. I have ~30 grams, that I bought a while ago, but
I don't think that I'll be able to buy any more. (Because of the drug war.) I know how to make it of course, but what I have is very pure, and was
quite expensive.
[Edited on 4-2-2014 by Zyklonb]
|
|
Brain&Force
Hazard to Lanthanides
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
alexleyenda, for the plated coin collection, why not use silver? That should work fine. Other ones that may work include chromium, cobalt, and gold
(if you can get your hands on a gold compound).
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
For silver I would need nitric acid to dissolve it to make the aqueous solution (at my knowledge it is the only way to dissolve it), but I don't have
nitric acid. It is impossible to find nitric acid or nitrates to make it in Canada (omg, explosives, fear, terrorism, let's ban all the nitrates, next
step is water, dangerous solvent!), I know how I could get some but it'll take some time :p Gold I can't now for the same reason and I'll take a look
at chromium and cobalt.
@ Kristof, your christmas ball over snowflakes synthesis looks really great :p
[Edited on 5-2-2014 by alexleyenda]
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
@alexleyenda, dissolve silver without HNO3.
[Edited on 5-2-2014 by Zyklonb]
|
|
Simbani
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 50
Registered: 12-12-2012
Member Is Offline
Mood: No Mood
|
|
Sorry no picture from me, but I can´t help myself, I have to link this video ![:D](./images/smilies/biggrin.gif)
Some incredible looking highspeed footage of a "christmas tree" made out of detcord!
Det Cord Christmas Tree
|
|
Hegi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 199
Registered: 27-9-2013
Member Is Offline
Mood: No idea.
|
|
not chemistry, but anyway...
<img src="http://chem.pieceofscience.com/wp-content/uploads/2014/02/js6.jpg" width="800" />
<img src="http://chem.pieceofscience.com/wp-content/uploads/2014/02/js4.jpg" width="800" />
and potassium hexacyanochromate(III), could always be find on wiki...
<img src="http://chem.pieceofscience.com/wp-content/uploads/2014/01/hexacyanidochromate-II.jpg" width="800" />
<!-- bfesser_edit_tag -->[<a href="u2u.php?action=send&username=bfesser">bfesser</a>: reduced
image size(s)]
[Edited on 7.2.14 by bfesser]
Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
|
|
Adas
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline
Mood: Sensitive to shock and friction
|
|
Not very pretty, but still.. Something with copper sulfate and sodium hydroxide.
Rest In Pieces!
|
|
alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
Zinc flame
While I was trying to extract zinc from batteries the other day, I had to test if the metal really was zinc. I thought a good first test would be to
try to melt it with a blowtorch. My first attempt did not melt the metal, it was probably a steel case. On my seconth attempt however (with metal from
another brand and kind), it was zinc and I learned by surprise that zinc did burn in a beautiful cyan color! Chemistry is so awesome for these "oh, I
didn't expect that" moments Anyways, I took some pictures of burning zinc
after that. The quality kind of sucks, but it is still acceptable.
![zinc1.bmp - 654kB zinc1.bmp - 654kB](https://www.sciencemadness.org/whisper/files.php?pid=318267&aid=29592)
![Zinc2.bmp - 392kB Zinc2.bmp - 392kB](https://www.sciencemadness.org/whisper/files.php?pid=318267&aid=29593)
![zinc3.bmp - 376kB zinc3.bmp - 376kB](https://www.sciencemadness.org/whisper/files.php?pid=318267&aid=29594)
![zinc4.bmp - 605kB zinc4.bmp - 605kB](https://www.sciencemadness.org/whisper/files.php?pid=318267&aid=29595)
[Edited on 7-2-2014 by alexleyenda]
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
Cool, I just took apart two zinc-carbon batteries two days ago, the zinc yields were pretty good, I haven't weighed them yet though.
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
Been handling lots of bromine lately. I stored it in the freezer to find these pretty crystals on the walls
<img src="http://i1329.photobucket.com/albums/w541/mmpchem/Mobile%20Uploads/photo_zpscecc7722.jpg" width="800" />
<!-- bfesser_edit_tag -->[<a href="u2u.php?action=send&username=bfesser">bfesser</a>: reduced
image size(s)]
[Edited on 7.2.14 by bfesser]
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
That looks awesome, I just ordered a condenser, so I might make some bromine myself.
|
|
alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
Yep, I'm like a child in frond of red cristal candies :p
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
I'm going to electro-plate some coins today(at least one today). Will post some pictures later.
[Edited on 8-2-2014 by Zyklonb]
|
|
alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
My Québec version of the famous blue bottle experiment ; the beer bottle I
used our maple syrup as a source of glucose as I didn't manage to find pure glucose but it's even better ! It really looks like beer :p
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
That's hilariously cool! Nice job!
[Edited on 8-2-2014 by Mailinmypocket]
|
|
Hegi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 199
Registered: 27-9-2013
Member Is Offline
Mood: No idea.
|
|
Sodium ferrioxalate
<img src="http://chem.pieceofscience.com/wp-content/uploads/2014/02/picture.jpg" height="597" width="900">
Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
|
|
Brain&Force
Hazard to Lanthanides
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
Hegi, you must show us what the sodium ferrioxalate looks like under UV light!
Here's the spectrum of a sodium lamp. The D line is visibly split. I don't know whether this is caused by the absorption of the light or by the actual
splitting of the D line into D1 and D2 components. It's only visible when the lamp is at full power.
<img src="http://brainforce.weebly.com/uploads/5/5/1/3/5513329/228592_orig.jpg" width=800>
[Edited on 16-2-2014 by Brain&Force]
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
alexleyenda
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline
Mood: Busy studying chemistry at the University
|
|
A sealed test tube I made today to contain Iodine for the pleasure of safely subliming it. Works like a charm! Resists the pressure, no flaw.
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
Nice, I sublimated and condensed some iodine yesterday.
[Edited on 21-2-2014 by Zyklonb]
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Some copper aspirinate I made the other day. Also, an improvised dean-stark trap. It worked just fine for my synth of p-toluenesulfonic acid.
![IMG_20140221_150501 (2).jpg - 393kB](https://www.sciencemadness.org/whisper/files.php?pid=320139&aid=30006)
|
|
bfesser
Resident Wikipedian
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
That's a damned nice product—beautiful color! What are your plans for such a large quantity, though?
|
|
Hegi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 199
Registered: 27-9-2013
Member Is Offline
Mood: No idea.
|
|
Hey man, thank you for the idea, i´ve almost totally forget about that... soon... Now it´s being recrystallised..
<img src="http://chem.pieceofscience.com/wp-content/uploads/2014/02/chromalum21.jpg" width="900" height="600">
Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
|
|
Pages:
1
..
5
6
7
8
9
..
76 |