Drying Sodium Hydroxide


Any thoughts on drying hardware store bought NaOH ?
View user's profile View All Posts By User
alexleyenda
Hazard to Others
***




Posts: 277
Registered: 17-12-2013
Location: Québec, Canada
Member Is Offline

Mood: Busy studying chemistry at the University

[*] posted on 13-1-2014 at 15:40


I guess heating it to 130°C and letting it cool in a dessicator should get the job done.
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 13-1-2014 at 15:43


Don't bother, the only good way to dry it is to heat it while molten after which you still have to grind it up again. Most uses of sodium hydroxide will tolerate a few percent of water. You're better off titrating it and adjusting the amount used. Most preps will also tolerate excess and 5-10% excess should cover for any water content.



Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
ScienceSquirrel
International Hazard
*****




Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline

Mood: Dogs are pets but cats are little furry humans with four feet and self determination! :(

[*] posted on 13-1-2014 at 15:59


If it is little dry white pellets or flakes I guess it is at least 95%, probably more.
I buy 98% food grade sodium hydroxide as mini pellets for use in brewery cleansing from an approved brewery supplier.
It is a free flowing solid that does not stick together if kept dry.
Things to look out for are sticking together or white efflorescence.
This shows the absorption of water and / or carbon dioxide.
Molten sodium hdroxide is evil stuff and best avoided.