Grignard SS compatibility?
I haven't been able to find any data about compatibility of 304 or 316 stainless steels with grignard reaction when used as a vessel for reaction.
Does anyone have any data, are metallic vessels compatible or is glass vessel a mandatory?
|
|
eidolonicaurum
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 2-1-2014
Location: Area 51
Member Is Offline
Mood: Hydric
|
|
You could make a grignard on a small scale, and add a peice of relevant stainless steel. If the grignard decomposes, it is incompatible.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by eidolonicaurum ![](images/xpblue/lastpost.gif) | You could make a grignard on a small scale, and add a peice of relevant stainless steel. If the grignard decomposes, it is incompatible.
|
Considering just how hard it is to set up a Grignard reaction, that's rather a difficult way of testing it. And it still not the same as having a
reaction vessel made of SS.
If you can't do it with glass I would try an inert plastic like PP or HDPE.
|
|
JAVA
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 9-1-2014
Member Is Offline
Mood: No Mood
|
|
This is not the way of performing a experiment. You soon get corrosion of Mg to MgO and nothing will happen. Why you don't buy borosilicate glasswork
like any other chemist?
PP or HDPE? = madscience
|
|
UnintentionalChaos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
The original question was posed in October of last year and was only replied to today. I suspect the OP either doesn't care anymore or has found his
answer.
As a serious answer, I'd avoid steels as both nickel and iron salts are known to catalyze various reactions involving grignard reagents (such as the
Kumada coupling) that would be side products in the event you are running a normal grignard + carbonyl.
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
In what way? Both are very resistant to many organic chemicals and Grignards don't run at high temps. PP withstands 140 C easily.
|
|