Yellow stain on glassware
I bought a second hand chemglass reflux condenser a while ago. When it arrived, it had a yellow stain on the inside of the cooling coil.
Even though this is on the inside of the coil and doesn't effect its usability at all (It works amazingly), I was wondering what this was caused by,
whether it could be removed (I know cleaning things is already a thread, but since I don't know what this is, I don't know how to clean it), and
whether it is a problem or not.
PS: Would it be possible for the cleaning method to not be caustic or toxic?
I will be posting pictures soon.
When the police come
\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
|
|
papaya
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 615
Registered: 4-4-2013
Member Is Offline
Mood: reactive
|
|
Obviously a rust.
|
|
TheChemiKid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline
Mood: No Mood
|
|
Why would that be?
When the police come
\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
It is simply minerals deposited from the water that has passed through it.
You might be able to remove it with dilute hydrochloric or nitric acid, but me I'd just whip up some aqua regia and let the whole thing soak in it for
a day or two. I like my glass spotless, and as such a KOH/ethanol wash would follow the aqua regia soak...
Acetic acid or citric acid might remove the stain too, but I suspect a prolonged soak would be needed, even boiling perhaps..
Any sufficiently advanced technology is indistinguishable from magic.
|
|
TheChemiKid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline
Mood: No Mood
|
|
Thank you, I will try different methods and say how they perform.
When the police come
\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
Iron stains are very hard to remove from glassware. If it doesn't get removed by HCl you might want to try aqua regia.
|
|
Sublimatus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 108
Registered: 8-6-2011
Member Is Offline
Mood: No Mood
|
|
You might try a mix of dilute hydrochloric acid and hydrogen peroxide. That mixture removes many otherwise tenacious stains, in my experience, and is
a lot safer than aqua regia.
|
|
Zephyr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 341
Registered: 30-8-2013
Location: Seattle, WA
Member Is Offline
|
|
I usually clean rust off of my glassware buy soaking the dirty equipment in a hot solution of oxalic acid. This method has the perks of being
efficient as well as non toxic.
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
I acquired a lot of condensers that all had yellow stains in them, I found HCl to be of limited use. Chromic acid cleaned it right up though, and I
prefer chromic acid as it doesn't fume like HCl and HNO3!
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
For really dirty glassware, I usually use saturated sodium chlorate solution and 31% hydrochloric acid. The chloric acid/chlorine oxides produced will
oxidize away all the dirt. (It's like chromic acid, but no heavy metals.) Fumes, however, are a problem, so I do it outside.
Don't try using concentrated sulfuric acid instead of the hydrochloric acid. I did, and I'm lucky the resulting explosion didn't crack my glassware.
[Edited on 29-12-2013 by Cheddite Cheese]
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
thats true, but I hate HCl fumes!
have you tried that mix on orgo crap left over from distillation? those terrible tars that stick to everything.
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Actually, I first tried it on tar (aldol condensation crap impurities) left over from distilling crude chloroacetone. After a soak overnight, it came
right off.
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
it takes all night? well, I guess I'm just lazy (must be why my lab is so damn tidy )
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Quote: Originally posted by Pinkhippo11 ![](images/xpblue/lastpost.gif) | I usually clean rust off of my glassware buy soaking the dirty equipment in a hot solution of oxalic acid. This method has the perks of being
efficient as well as non toxic. |
Oxalic acid is actually toxic to humans.
More so than HCl.
However it is a very good cleaner for rust stains and
is sold for that purpose.
|
|
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
If it is iron, oxalic acid is usually your best bet. I remember watching a video in YouTube some months ago about cleaning rust... check it in case
it's there.
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Brain&Force
Hazard to Lanthanides
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
I've never tried this, but if you can get ahold of EDTA, that may work to chelate the iron away. Acidic citrates also work, they're probably the least
toxic solution.
There's also stuff called naval jelly, it's mostly phosphoric acid. It seems to work pretty well, as does ammonium dihydrogen phosphate.
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
Zephyr
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 341
Registered: 30-8-2013
Location: Seattle, WA
Member Is Offline
|
|
Quote: Originally posted by macckone ![](images/xpblue/lastpost.gif) |
Oxalic acid is actually toxic to humans.
More so than HCl.
However it is a very good cleaner for rust stains and
is sold for that purpose. |
Yes you are right, isn't the oxalic acid in rhubarb leaves that make them poisonous?
I think this is the video you were thinking about Eddygp?
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Yes and it is a cumulative toxin.
If forms kidney stones which in sufficient quantity cause
the kidneys to shut down.
Spinach also contains oxalic acid but it binds with
calcium also found in spinach to prevent it from being
absorbed. You have to eat pounds of rhubarb
to actually poison yourself. Antifreeze (ethylene glycol)
is converted to oxalic acid which makes it toxic.
http://helios.hampshire.edu/~nlNS/mompdfs/oxalicacid.pdf
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
While on the subject of oxalic acid toxicity.
My uncle almost died as a kid from rhubarb wine (which he stole from my grandfather) that had not been "calcified", in other words added a soluble
calcium salt, most likely Ca(OH)2
I have no idea what they did to save him though...
Any sufficiently advanced technology is indistinguishable from magic.
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Quote: Originally posted by bahamuth ![](images/xpblue/lastpost.gif) | While on the subject of oxalic acid toxicity.
My uncle almost died as a kid from rhubarb wine (which he stole from my grandfather) that had not been "calcified", in other words added a soluble
calcium salt, most likely Ca(OH)2
I have no idea what they did to save him though...
|
Probably pumped his stomach, balanced his blood ph and calcium levels with fluids
Most poisoning is not fatal but does lead to kidney stones.
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i found it that Fe3O4 reacted very well with concentrated citric acid + H2O2
as i heated it it gave off a nearly explosive decomposition
the Fe3O4 was 'beach magnetite' and some of might be iron aswell
but ofcourse, the more dangerous the chemical is, the more reactive it is, so the more dangerous stuff you use for it, the bigger the chances are it
will get rid of it (:
|
|
Arthur Dent
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 553
Registered: 22-10-2010
Member Is Offline
Mood: entropic
|
|
THe idea of oxalic acid is interesting, although this chemical is pretty hard to find at reasonable prices in my neighborhood.
As for the HCl + bleach solution, it is indeed very efficient to remove most ferrous stains, but to my dismay, it also destroyed the company logo off
of my expensive Ace Glass Soxhlet... The red logo turned dark brown, and while washing with soapy water and a brush, just disappeared! I thought that such a prestigious labware maker would make their logo a wee bit
more resistant to mineral acids.
LOL
Robert
--- Art is making something out of nothing and selling it. - Frank Zappa ---
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Bar Keepers friend contains Oxalic acid as well as other scrubbing agents. There are also sulfamic acid cleaners (ZEP CLR for one). And of course
the good old cheap standby of vinegar and hydrogen peroxide. One of the sulfamic acid cleaners may be better as they
are specifically formulated to remove rust stains from ceramics.
|
|