Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: solder trouble
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 5-10-2013 at 14:43
solder trouble


I put 50% Lead 50% tin solder in vinegar and an odd percipitate formed any idea whatit is?

[Edited on 5-10-2013 by bismuthate]




I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-10-2013 at 15:04


Lead may dissolve out of the solder but tin will not so if your ppt is grey I suspect it is tin. I would have thought that the reaction of solder with vinegar (4-5% acetic acid) would be very slow even if heated. I must admit I have never tried it!
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 5-10-2013 at 15:07


It took a month. My percipitate is tan powder.



I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 6-10-2013 at 03:01


I'm going to hazard a guess. I might be wrong but I would suspect tin oxide. Lead acetate is soluble at room temperature. Any tin acetate that would form would decompose to tin oxide.

[Edited on 6-10-2013 by hyfalcon]
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 6-10-2013 at 08:47


A month! In that case I go with hyfalcon's suggestion. The colour suggests a mixture of stannic oxide (white) and stannous oxide (dark brown).
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 6-10-2013 at 08:55


thanks! this is a good way to seperate solder.



I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 14-10-2013 at 07:52


I would think the reaction could be sped up by bubbling air through the mix. That might speed things up enough to make it practical.
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 14-10-2013 at 08:08


That may be what I will do with my next batch of lead acetate thanks.
lead iodide is amazing I just love making it so I've made a lot of acetate lately..




I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2542
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 14-10-2013 at 13:48


You can probably find lead sinkers at a local fishing store, which are almost pure lead (they are banned in some states, due to waterfowl poisoning ). This would save you the trouble of extracting lead from solder. Be careful and don't get lead poisoning!



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 14-10-2013 at 14:00


The solid may also contain considerable amounts of basic lead acetate unless your acetic acid is in excess.



Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 14-10-2013 at 14:25


UnintentionalChaos the product is of no concern as long there is a soluble lead salt impurities in the percipitate are no problem, but thanks for the tip.:)

Chedite Cheese I did look at sinkers, but ironicly they were 50% lead.
The rest was said to be "other" which is concerning. I remember once I saw rat poison labled 99% other.




I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
ScienceSquirrel
International Hazard
*****




Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline

Mood: Dogs are pets but cats are little furry humans with four feet and self determination! :(

[*] posted on 14-10-2013 at 15:34


In my experience, European fishing sinkers are mainly lead but I think thay can contain small amounts of tin and antimony as they are made up from scrap lead from old pipes, recovered bullets, wheel weights, etc.
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 14-10-2013 at 16:22


Shame that I live on the island of stability here the sinkers are made of super heavy elements.;)



I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2013 at 09:32


I once slowly dissolved Lead/Silver solder in a mixture of vinegar/dilute H2O2 in a course of a few days (refresh the H2O2). There still was a small amount of a black residue.

Note, Silver acetate is soluble in acetic acid, but in more neutral solutions, it forms a white (cottage cheese like) precipitate.

Also, Lead acetate presents a higher poisoning risk via skin absorption than other insoluble Lead salts (where, I suspect, dust inhalation and direct ingestion are primary concerns).


[Edited on 18-10-2013 by AJKOER]