Use KClO3 instead of NaClO3 as the first is much easier to separate due to its low solubility in water.
|
|
Marvin
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
*claps*
Brilliant suggestions metalresearcher.
Curious about one thing though. Why do you want him dead?
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
I would be surprised if it wouldn't simply oxidize back to CaSO4.
As for aggressiveness, rapid decomposition seems to depend on transition metal contamination (besides reaction energy already). Gypsum should be
fairly pure if it's white, but even off-white sand can contain a significant amount of FeOx and such.
Tim
|
|
testimento
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 351
Registered: 10-6-2013
Member Is Offline
Mood: No Mood
|
|
Metalresearcher, you obviously didn't notice my other thread concerning about evaporation. One can churn up to 30 liters of concentrated sodium
chlorate solution and evaporate off the water within couple of days and make a final drying phase in oven at mild temperature to obtain quite pure,
technically anhydrous NaClO3. But anyway, I still strongly think that aside from reacting CaS with CaSO4 to produce CaO and SO2, chlorate method would
be quite wasteful.
Btw, check out ebay and other marketplaces for chinese ozone generators. As we speak, one can make sulfuric acid directly by bubbling ozone through
the tank containing SO2.
3 SO2 + 3 H2O + O3 → 3 H2SO4
This is quite an interesting since cheapest ozone generators produce several dozens of grams of ozone in an hour and with this reaction, 20% solution
of SO2 will yield 40-60% of H2SO4 concentrations. It'd be probably possible to engage the reaction in gas phase, but then the efficiency will be
reduced by order of 2/3.
|
|
Ulfsaar
Harmless
Posts: 1
Registered: 3-12-2013
Member Is Offline
Mood: No Mood
|
|
I wonder if monocalcium phosphate (or various poly- or metaphosphates) could be used to expel sulfuric acid and/or sulfur trioxide from calcium
sulfate. I guess that process would go at moderate temperatures (300-500 C) so that decomposition of sulfur trioxide would be avoided.
[Edited on 3-12-2013 by Ulfsaar]
|
|
Pulverulescent
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 793
Registered: 31-1-2008
Member Is Offline
Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!
|
|
Quote: | This is quite an interesting since cheapest ozone generators produce several dozens of grams of ozone in an hour |
That should read; "milligrams per hour" . . .
"I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones"
A Einstein
|
|
Mr.Chemical1
Harmless
Posts: 3
Registered: 27-8-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Pulverulescent ![](images/xpblue/lastpost.gif) | Quote: | This is quite an interesting since cheapest ozone generators produce several dozens of grams of ozone in an hour |
That should read; "milligrams per hour" . . . |
There are several relatively cheap($20-30) ozone generators that can produce several grams of ozone per hour that can be found on ebay. Though
generators producing several dozen grams are significantly more expensive. I don't how long they can be run without overheating or
burning out though.
Scientia est potentia
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Better to use nitric oxides to oxidize the sulfur dioxide solution to sulfuric acid. A relatively small amount acts as a catalyst in the presence of
air.
|
|