Iron Oxide color
Hi there
I've searched the forum to see if I could find a topic dealing with the multitude of colors you can find Fe2O3, but couldn't find none so made a new
topic.
So far I was able to see blue, red, yellow and "natural" (brownish) color.
Now, the Fe2O3 obtained from the reaction between Fe3(SO4)2 and NaOH, filtered and dryed was blackish/brownish but the one my father bought somewhere
for some unknown reason was blue.
The thing is, the reactivity of the two was well different: the one I synthetized reacted according to what I learnt from theory: it readily dissolved
in HCl, yelding a strong yellow solution of FeCl3. Also tried oxidizing it (to see if there were traces of reducing agents) with a diluite solution of
H2SO4 and K2Cr2O7, but nothing happened.
However, when I tried to dissolve the blue Iron oxide in HCl, it didn't dissolve; a part of it lost its former blue color and a smelly gas was
emitted. A blue/gray powder remained in the bottom of the beaker. I tried with H2SO4 but nothing again.
I'm 100% positive it wasn't prussian blue. The blue powder looks like this
![](http://img.bosscdn.com/photo/product/ba42ec3fbabbaa2c3e83aba96555fcf0/iron-oxide-blue-5605.jpg)
Any idea of what kind of silly pigment was put in there? Are all the colored iron oxides sold basically everywhere so unreactive like this? In that
case, what kind of Iron Oxide would be appropriate for thermite? Yellow, red, blue, black... what does change?
Thanks for your attention
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i know that Fe3O4 is magnetic, cover a magnet in plastic and run it over the powder, spikes should be observed if there is Fe3O4 in it, also Fe3O4 +
HCl seemingly gives off 2FeCl3 and FeCl2, in which i recall as differing from Fe2O3, which doesnt produce (AS I REMEMBER!!) any FeCl3
so already with the HCl you could have found a hint towards what it is..
but why dont you just go ahead and see if it will react as thermite oxidizer?
i could be wrong, i could be very wrong.. but it could potentially be an organic substance that gives the blue colour, and most organics decompose at
a relatively low temperature (dont wanna say ALL, as that might be wrong at some point in history of chemistry)
oh another thing, Fe3O4 should if heated in the presence of oxygen turn into Fe2O3, this happens just around 200*C IIRC
btw could you try to put some in a bottle, then shake it alot, with water, and then see if some of it settles before some of the other, and then
perhaps try to have it fractionally decanted?
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
I don't believe that's iron oxide. A smelly gas with HCl? It might be something in a high oxidation state that's giving off chlorine, or it might be
a sulphide.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Metallus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 16-5-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid ![](images/xpblue/lastpost.gif) | I don't believe that's iron oxide. A smelly gas with HCl? It might be something in a high oxidation state that's giving off chlorine, or it might be
a sulphide. |
I've worked with HCl and chlorine so much that I can detect their smell from distance and that wasn't any of those. It was closer to sulphide...
Also, when I put this blue oxide in water, it precipitates but the water is no longer limpid. When adding HCl, the powder loses some of its blue
color, turning a bit on the gray side and releasing this smelly gas. It looks like a bit of it dissolves but I can't really understand what's exactly
going on since the solution is too torbid. Most of it stays in the bottom anyways.
@ Antiswat:
Shouldn't Fe2O3 react with HCl according to the following?
Fe2O3 + 6HCl --> 2FeCl3 + 3H2O
By the way, as I currently don't have powdered Al, I tried using some "home-grinded" Al, but miserably failed to ignite it (Tried using black powder
or KNO3 + sugar. I don't have a blowtorch).
Putting a lighter near the powder doesn't lead to any noticeable change.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
If it reacts with acid to give crap, try reacting it with aqueous ammonia instead. That colour doesn't look like any iron compound I can think of,
but it might be a cobalt compound (isn't that the colour of cobalt(II) thiocyanate?).
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Metallus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 16-5-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid ![](images/xpblue/lastpost.gif) | If it reacts with acid to give crap, try reacting it with aqueous ammonia instead. That colour doesn't look like any iron compound I can think of,
but it might be a cobalt compound (isn't that the colour of cobalt(II) thiocyanate?). |
Nothing happens; it's just like it was clear water. By the way, I did some more research and found what the blue pigment could be http://en.wikipedia.org/wiki/Ultramarine
If it's indeed this compound, then that would explain the smelly gas: the sulphide would react with HCl to give out H2S.
|
|
ElectroWin
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 224
Registered: 5-3-2011
Member Is Offline
Mood: No Mood
|
|
yes: ultramarine.
(Na<sub>8-10</sub> Al<sub>6</sub> Si<sub>6</sub> O<sub>24</sub> S<sub>2-4</sub>
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
When I read the OP this also was the first thing I was thinking about. Ultramarine gives off H2S when added to acid and it looses its blue color.
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
how did they manage to sell ultramarine as iron oxide anyways? ohwell it has been seen theyre stating their product contains no chemicals
seemingly i was very wrong about Fe2O3 with HCl, it should give pure FeCl3
|
|