Cleaning Zinc Cells
I just dismantled a Lantern battery to get the zinc. I've removed the Manganese Dioxide out of it so I'm now left with a empty zinc cell, but a lot of
manganese dioxide is still on the sides of the zinc. Is there a way i can remove the manganese dioxide with out dissolving the zinc? any acid or base?
or should i just scrub it off?
|
|
ScienceSquirrel
International Hazard
   
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Go and see a friendly roofer, he will sell or give you a piece of zinc sheet, 99% pure.
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by toothpick93  | I just dismantled a Lantern battery to get the zinc. I've removed the Manganese Dioxide out of it so I'm now left with a empty zinc cell, but a lot of
manganese dioxide is still on the sides of the zinc. Is there a way i can remove the manganese dioxide with out dissolving the zinc? any acid or base?
or should i just scrub it off? |
Just scrub it and sand it down till it gleams (for not very long). With an MP of 419 C it can be easily ingoted, most oxidic impurities will then
float on top of the molten metal. Ingots tarnish less than sheets of course (less surface area per gram).
Note also that what you deferentially called 'Manganese Dioxide' over here we call 'battery crud' because it contains often less than 30 % MnO2 (and
usually as mixed Mn oxides) and is contaminated with large amounts of graphite (conductor), almost always some ferric oxide, some zinc oxide or zinc
chloride etc.
[Edited on 20-6-2013 by blogfast25]
|
|
papaya
National Hazard
  
Posts: 615
Registered: 4-4-2013
Member Is Offline
Mood: reactive
|
|
Try oxalic acid.
|
|
toothpick93
Harmless
Posts: 44
Registered: 26-2-2013
Member Is Offline
Mood: No Mood
|
|
I new that the manganese dioxide is very crude, so much iron its not funny. Would oxalic acid only dissolve the dioxide?
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by toothpick93  | I new that the manganese dioxide is very crude, so much iron its not funny. Would oxalic acid only dissolve the dioxide? |
It's likely to dissolve also some, if not all, of the iron. I used the oxalic acid method once to reduce the battery crud 'MnOx' to Mn2+
(the oxalic acid oxidises to CO2) and found considerable amounts of iron in the leachate. It might seem strange because ferric oxalate is
poorly soluble but oxalic acid isn't the only acid in the mix: the reduction needs to be carried out in the presence of H2SO4, which largely
suppresses to dissociation of the oxalic acid. No oxalate ions, no ferric oxalate.
Iron and manganese can be separated in ways that have basically already been discussed to death on this forum. Use the search facility...
It's likely to attack the zinc.
True but zinc metal and MnSO4 from dry batteries... that's a bit of a rite of passage! The graphite just gets everywhere if you're not diligent, especially when wet.