How much chemical to use to minimize unused reactants?


I'm doing the reaction 2 CuO + C = 2 Cu + CO2. How many grams of CuO and C should I mix together to make sure there's none left, and all I have left is pure copper powder? 2 grams of CuO and 1 gram of carbon?

I made the carbon with sugar and sulfuric acid BTW
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 5-6-2013 at 11:39


http://theodoregray.com/PeriodicTable/MSP/BalanceReactions for the easy method.
For the harder method, you'll need the molar mass of carbon, the molar mass of CuO, and the gram weight of one of these that you intend to use (say, 50). Using the molar masses, convert your grams of A to moles of A (where A can be either one). Then, using the balanced equation, convert moles of A to moles of B (ex: 5 moles CuO for every 3 moles carbon - whatever the balanced numbers are). Finally, convert moles of B to grams of B. Make sure to write these down as fractions (ex. 50g CuO x 1 mole CuO/999g CuO), making sure each unit *except* your final unit (g of B) is on both the top and the bottom of any fraction at least once to properly cancel out the units.
And that's stoichiometry in a nutshell. This ensures that, to a reasonable degree, both reactants are used up equally, and close to no unused reactants will be left mixed with the products.

On to the reaction itself:
You do know that reactions with carbon typically take place at 1000 Celsius in blast furnaces designed to withstand molten metal? If your reaction works at all, you won't have any copper powder: You'll have a lump of copper metal.
To get a decent grade of copper powder, dissolve your CuO in any acid (even vinegar will work, and you can do the stoichiometry for this too if you wish). Then, add a piece of aluminum foil and wait (probably overnight). What was formerly a blue solution of a soluble copper salt should be clear, the Al should be gone or severly degraded (stoichiometry here too, why not? You don't want aluminum in your copper), and copper powder should be left on the bottom of the container. You can clean this with almost any acid, except for HNO3, as copper metal is resistant (though not quite immune) to chemical attack by most major acids.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Cou
National Hazard
****




Posts: 958
Registered: 16-5-2013
Member Is Offline

Mood: Mad Scientist

[*] posted on 5-6-2013 at 11:58


Well on this video he does it over a fire: http://www.youtube.com/watch?v=g3ar6zGcTQY

He used copper carbonate though, does that make a difference?
View user's profile View All Posts By User
ElizabethGreene
Hazard to Others
***




Posts: 141
Registered: 15-10-2012
Member Is Offline

Mood: No Mood

[*] posted on 12-6-2013 at 13:24
Two answers.


Quote: Originally posted by Cou  
I'm doing the reaction 2 CuO + C = 2 Cu + CO2. How many grams of CuO and C should I mix together to make sure there's none left, and all I have left is pure copper powder? 2 grams of CuO and 1 gram of carbon?

There are two answers to this question.

The first answer is the theoretical one, where everything works perfectly.

In this world you need 2 moles of CuO plus one mole of Carbon.

From the Periodic table, we get the following weights per mole:
Cu = 63.5
O = 16

Adding those up, a mole of CuO weighs 79.5 grams. We said we needed 2 moles of this, so 79.5 * 2 = 159.

Next we look up the carbon.
C = 12

So, we need (63.5 + 16) * 2 = 159 grams of CuO plus 12 grams of C.

Physicists refer to this wonderland where everything works perfectly as "A frictionless vacuum". In real life they don't exist. The second answer to your question is the "real world" answer.

In the real world you'll use a gross excess of Carbon to reduce the CuO, and the reaction needs to be in a crucible that seals out atmospheric Oxygen. Three to five times the amount required by the theoretical answer is not unreasonable. The excess Carbon is required to consume the atmospheric Oxygen in the crucible plus any extra oxygen that sneaks into the crucible.

When your reaction is done, you'll have a lump of copper metal and unreacted carbon. The excess carbon can be converted to CO and CO2 by heating while exposed to air.


There are two key concepts here:
1. The atomic weight from the periodic table is the weight in grams of one mole of an element. Add these weights up to get the perfect world amounts of reactants you need for a reaction.

2. The real-world amounts can vary wildly from the the theoretical amounts due to side reactions and Murphy's law. This is what makes chemistry fun!
View user's profile Visit user's homepage View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 12-6-2013 at 14:25


I did the carbothermal reduction a few months back with basic copper carbonate (made by mixing solutions of CuSO4 and Na2CO3) and charcoal. I had to heat the crucible (covered, but not airtight, so as to let the evolved gas escape) until the bottom started to glow red, and I got my copper in the form of fine powder. I used the stoichiometric amount of reactants, and I got significant unreacted basic copper carbonate which decomposed to copper oxide. I was able to dissolve the copper oxide in hydrochloric acid, leaving fine copper powder. My yield was slightly less than 50%.

Carbon is cheap. Use an excess.




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 12-6-2013 at 16:25


Quote: Originally posted by Cou  
I'm doing the reaction 2 CuO + C = 2 Cu + CO2
It's basically impossible to do this reaction without also doing the reaction CuO + C → Cu + CO, and furthermore, you'll have very little control over the ratio between these two reactions.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 12-6-2013 at 16:39


boudouard reaction logic, every metallurgy chemist knows that.



I never asked for this.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 13-6-2013 at 03:09


Nicely explained by Elisabeth there.

There exist of course reactions that proceed perfectly stoichiometrically. See e.g. acid/base neutralisations in acidometry. An excess of one of the reagents is thus not always a requirement.

For more fun, heat the CuO/excess carbon mixture to over the MP of Cu. The excess carbon then ends up floating on top of the molten Cu, slowly glowing away.

This also works with SnO2 (and Sn has a much lower MP) and it needs basically red heat to proceed at appreciable rate. When I did this years ago, the SnO2/C mixture behaved like a 'fluidised bed' because the escaping CO/CO2 caused 'bubbles' to form in the reagent mix. Interesting to watch.

[Edited on 13-6-2013 by blogfast25]




View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 13-6-2013 at 05:30


Quote: Originally posted by Cou  
Well on this video he does it over a fire: http://www.youtube.com/watch?v=g3ar6zGcTQY

He used copper carbonate though, does that make a difference?


That's actually my video, and there were several things wrong with it that I'd like to revisit. You saw I did get some copper, but it was really just a dusting. Two things are key that I didn't do:

1) Powdering the reactants. This provides lots of surface area for the reaction to occur, and is generally a good idea for just about any chemical reaction.

2) Cover the crucible. As watson.fawkes mentioned, production of CO will also occur. This gas can act as an intermediate which, if trapped by a loose lid, can react again with the reactants to free more elemental copper.

Changing those two things would have improved my yield quite a bit, I think. My charcoal burner setup doesn't get near to the melting point of copper, though - I've only just barely melted aluminum with it. A good backyard furnace is something I've wanted for a long time.
View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 13-6-2013 at 12:13


Quote: Originally posted by MrHomeScientist  

2) Cover the crucible. As watson.fawkes mentioned, production of CO will also occur. This gas can act as an intermediate which, if trapped by a loose lid, can react again with the reactants to free more elemental copper.



That would barely, if at all, have made a difference. This reaction is largely driven by the volatility of CO/CO2, which leave the reaction product mix, thus driving the equilibria:

CuO(s) + C(s) < === > Cu(s) + CO(g)
and CuO(s) + 1/2 C(s) < === > Cu(s) + 1/2 CO2(g)

... to the right. At very high temperatures it's mainly the first reaction that takes place.

Your 'failure' was largely due to far too low temperature. Had you sat this directly onto the red hot coals of a barbecue, with good fanning or bellowing below the pan, it would have proceeded much better. Powdering and using an excess C also are important... Try it again with a smaller crucible (and reagent mix), straight onto a blazing BBQ (using lump charcoal, not 'briquettes').

[Edited on 13-6-2013 by blogfast25]




View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4299
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 13-6-2013 at 12:36


You might be better off heating the copper oxide in a stream of natural gas.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 13-6-2013 at 12:57


Well, bear in mind the next reactions.
Being β and λ rational numbers, the reactions A and B are as follow:
A= 2 CuO + C ==> 2 Cu + CO2
B= CuO + C ==> Cu + CO

Your final reaction will be β*A + λ*B so it is
(2β+λ) CuO + (β+λ) C ==> (2β+λ) Cu + β CO2 + λ CO
Control the parameters β and λ somehow to control the reaction or just add a lot of carbon in excess, like 4 times the needed amount. Pulverize both the CuO and C for best results and if you would like even better results, do it in an inert atmosphere.

Actually, you can add a C reaction that would occur if the reaction B happens:

C= CuO + CO ==> Cu + CO2

Being ω any number, apart from the other two previously defined, we get that:

(2β+λ+ω) CuO + (β+λ) C ==> (2β+λ+ω) Cu + (β+ω) CO2 + (λ-ω) CO

Which of course is absolutely crazy to perfectly work with it but correct to a certain extent. The (λ-ω) CO is because you would put ω CO on the other side and you can just pass it over, depending on which coefficient is larger.

[Edited on 14-6-2013 by Eddygp]




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2013 at 03:58


One way of determining whether a metallurgical reduction reaction can proceed and at which temperature is by using Ellingham Diagrams. These plot the Gibbs Free Energy change ΔG in function of temperature, for the reactions involved in the process.

Intro to Ellingham diagrams:

http://www.doitpoms.ac.uk/tlplib/ellingham_diagrams/user_gui...

Interactive page (generates Ellingham diagrams of your choice):

http://www.doitpoms.ac.uk/tlplib/ellingham_diagrams/interact...

For the CuO/C system, select ‘oxides’ and tick Cu and C on the periodic table, then ‘see Ellingham Diagram’.

The rules are:

1) If the line for C to CO lies below the oxidation line of the element, then the oxide of the element can be reduced by C, yielding CO. For CuO that is the case from roughly 500 K onwards.

2) If the line for C to CO2 lies below the oxidation line of the element, then the oxide of the element can be reduced by C, yielding CO2. For CuO that is the case across the board.

3) If the line for CO to CO2 lies below the oxidation line of the element, then the oxide of the element can be reduced by CO, yielding CO2. For CuO that is only possible at very high temperature.

Of course it also works for other combinations of oxides/reducing agents, as well as compounds other than oxides.

Try CuO + H2 for instance…



[Edited on 14-6-2013 by blogfast25]




View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 14-6-2013 at 12:35


Actually, I think you could just forget my Freudian slip.



there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 14-6-2013 at 12:35


Actually, I think you could just forget my Freudian slip.



there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2013 at 12:36


Freudian slip? You've truly lost me now...



View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 16-6-2013 at 13:42


Quote: Originally posted by blogfast25  
Freudian slip? You've truly lost me now...

Hahaha I couldn't think of a better way to say that.




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 16-6-2013 at 13:42


Quote: Originally posted by blogfast25  
Freudian slip? You've truly lost me now...

Hahaha I couldn't think of a better way to say that.




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User