Chart of Plastic Resistances to Chemicals
Found this great chart for a quick reference on how resistant certain plastics are vs common chemicals:
http://www.tedpella.com/company_html/PlasticsChemResistance....
Hopefully it's useful for others out there as well.
[Edited on 5-6-2013 by binaryclock]
Current Project: Playing with my new Laboy advanced distillery kit!
|
|
HOLYMOLYBDENUM
Harmless
Posts: 3
Registered: 10-4-2013
Member Is Offline
Mood: No Mood
|
|
Much obliged, this is indeed a very helpful chart!
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
nice! I can now find a container that isn't dissolved by MEK
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
Here is another chart I scanned a while back from a catalog, in case it is of use.
|
|
binaryclock
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 9-4-2013
Location: Canada
Member Is Offline
Mood: Organic
|
|
Amazing chart. Thanks for that!
Current Project: Playing with my new Laboy advanced distillery kit!
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i have a few others..
first off with metals and commonly used 'acid resistant alloys'
http://www.haynesintl.com/pdf/h2114.pdf
second some steel and some plastics (some not even listed on your link)
http://www.vp-scientific.com/Chemical_Resistance_Chart.htm
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
Here's more.
http://www.sciencemadness.org/talk/viewthread.php?tid=21503
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
The Alfa Aesar catalogue can easily be ordered and shipped to individuals, free of charge. It too has a very wide variety of information which is very
useful in the lab, including a large section listing very detailed properties of many/most of the elements, a compilation of CAS numbers, full lists
of R and S statements, conversion charts for a huge varitety of units for many different measurements, chemical bond length data, tables of multiples
of element weights, chemical shift data for NMR spectra, a table of different heating and cooling baths and their maximum/minimum temperatures, metal
compositions of common electroplating salts, average bond energies/strengths, and many, many more. It is also perfect for looking up structures
quickly, especially for some of the more unusual compounds which the internet may not have reputable data/information for.
It is an invaluable tool for any chemist and I would strongly recommend everyone orders one for free from Alfa.
[Edited on 7-6-2013 by Hexavalent]
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
chemcam
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 423
Registered: 18-2-2013
Location: Atlantis
Member Is Offline
Mood: I will be gone until mid-september, on a work contract.
|
|
Is that catalog available to all countries? If so do you have a link to order?
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
http://www.alfa.com/en/gl110ah.pgm
The one I am referring to is the first one, the blue "2013-2015 Catalog". I filled in all my details, just giving "JA Laboratories" (my initials) as
the company name. My catalog arrived a few weeks later, in a lovely Alfa Aesar box.
I can only assume it is available in all countries, but I had no issues at all having it delivered here in the UK.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Hexavalent ![](images/xpblue/lastpost.gif) | http://www.alfa.com/en/gl110ah.pgm
The one I am referring to is the first one, the blue "2013-2015 Catalog". I filled in all my details, just giving "JA Laboratories" (my initials) as
the company name. My catalog arrived a few weeks later, in a lovely Alfa Aesar box.
I can only assume it is available in all countries, but I had no issues at all having it delivered here in the UK. |
I got mine in Canada, same thing... Invent a name. It's like a Christmas wishbook
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
Absolutely! Did they send you a Canadian dollars version? I got a GBP edition, which is nice, as many international companies may only give their
catalog prices in USD.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
It was the CAD version- actually while on the topic of catalogs, Cole-Parmer will send samples of all their tubings (3 inch pieces) for chemical
resistance testing. You just need to go to the catalog request section of their site and do the same thing with a company name. Pretty neat!
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
Do you know which tubings they send? What materials? I've sent an "order" for them ![:P](./images/smilies/tongue.gif)
[Edited on 7-6-2013 by Hexavalent]
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
Mailinmypocket
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1351
Registered: 12-5-2011
Member Is Offline
Mood: No Mood
|
|
Oh gee... Off the top of my head I don't remember- There were quite a few varieties of silicon, one for petrochemicals and a few others
|
|
chemcam
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 423
Registered: 18-2-2013
Location: Atlantis
Member Is Offline
Mood: I will be gone until mid-september, on a work contract.
|
|
Oh I love the direction this thread is going! Does anyone have any other free sample/catalog type information? I have just ordered what has been
discussed so far also. Thank you all! I ordered a sigma catalog as well, not like it will do me any good other than fuel my dreams.
|
|
Lambda-Eyde
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 859
Registered: 20-11-2008
Location: Norway
Member Is Offline
Mood: Cleaved
|
|
I got a free 250 mL Azlon beaker and 250 mL Azlon wash bottle plus two lab posters from scilabware.com a few years back. Don't know if they still do
that. I too have a buttload of catalogs from Fisher, Carl Roth, Acros, Alfa and others. They look good and make excellent labjacks...
This just in: 95,5 % of the world population lives outside the USA
You should really listen to ABBAPlease drop by our IRC channel: #sciencemadness @ irc.efnet.org
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
I was just going to mention that!
http://www.scilabware.com/
I also got their free labware (250 mL Azlon beaker and 250 mL Azlon iPrOH wash bottle), posters (very informative - one was on plastics resistances'
to various solvents and reagents, and the other on glassware heating, safety and maintenance) and their glassware catalog, which is excellent
nerd-porn and very useful when you aren't sure what something is.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
platedish29
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 76
Registered: 2-9-2012
Member Is Offline
Mood: absorbing CO2
|
|
Common PET vials or bottles are attacked by aqueous lime so that fissures causes the liquid to leak, as observed by personal experience.
|
|