Cyanamide process demonstration


I made a cyanamide process demonstration, by changing a few parameter, it could be used to make usable cyanamide. Picture added soon.

The cyanamide process was, for a long time the main source of ammonia and nitrogen fixation. The process consisted in heating calcium carbide at 1000 C in a flow of nitrogen. Then the cyanamide was hydrolyzed to ammonia and calcium carbonate.

4g of calcium carbide is ground to a fine powder, and put in a 50ml aluminia crucible. The crucible is heated to yellow heat for 3 minutes. After cooling, the crucible contain a white part and a carbon black part. The content are poured in 50 ml of cold water. Caution, it is very exothermic. Ammonia smell can be observed, then, the solution is filtered, and tested with tincture of mercury in the usual way. The test is positive for ammonia.

Notes:
The white part correspond to the first part of the carbide that become hot, as such it is used to remove the oxygen from the crucible, foming carbon monoxide and calcium carbonate. The black part is the cyanamide, mixed with carbon.

CaC2 + N2 -) CaCN2 + C




I never asked for this.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2013 at 15:51


Quote: Originally posted by plante1999  
The cyanamide process was, for a long time the main source of ammonia and nitrogen fixation. The process consisted in heating calcium carbide at 1000 C in a flow of nitrogen.
It's also called the Frank–Caro process after its inventors.
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 6-5-2013 at 08:39


Yes, I forgot to mention it, I should add the picture in a few hours.



I never asked for this.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 6-5-2013 at 13:26


A nice bit of history in a crucible. Could be interesting to so some quantitative tests on...



View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 6-5-2013 at 14:26


Pictures!

What have you in mind, blogfast?







I never asked for this.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 7-5-2013 at 03:10



Quote: Originally posted by plante1999  
Pictures!

What have you in mind, blogfast?



Oh, just a quantitative determination of how much NH3 you obtained.

Looks like you could do with a clay pipe triangle!

[Edited on 7-5-2013 by blogfast25]




View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 7-5-2013 at 12:25


There is also an alternative method for producing pure calcium cyanamide uncontaminated with carbon and at a lower temperature of the red-orange heat range, which involves pyrolytic decomposition of calcium cyanurate. Some toxic fumes of cyanic acid will be produced as the byproduct during the first stage of the pyrolysis which should be be done mindful to flare off these fumes or otherwise provide for safe ventilation.

http://www.sciencemadness.org/talk/viewthread.php?tid=8594&a...

http://www.sciencemadness.org/talk/viewthread.php?tid=2762&a...

http://www.sciencemadness.org/talk/viewthread.php?tid=14267&...

Reaction of nitrous acid and a guanidine salt is a possible cold method which reportedly produces cyanamide in 80% yield. There is some more about this in the sticky tetrazole thread.

@plante1999 You should edit your picture pixel width to a lower value like 650 because it messes up the text formatting when these large pictures are attached inline.