filtration media
What is the difference between "kenite" and celite? I tried two search engines and got a bunch of stone age crap about ancient hebrew tribes. Sorry,
bad mood today tired of the cold dark days.
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
luckybot
Harmless
Posts: 17
Registered: 10-2-2013
Member Is Offline
Mood: No Mood
|
|
Kenite is a finer particle size according to the datasheets for both products. That's the only difference I see when glancing over the two.
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Thanks lucky. Perchance would you have a ref?
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
luckybot
Harmless
Posts: 17
Registered: 10-2-2013
Member Is Offline
Mood: No Mood
|
|
For Kenite 22um median size.
For Celite 38um median size.