Author: Subject: Raney Nickel with Pd/C - how clean and re-activate?
R.Esposito
Harmless
*




Posts: 11
Registered: 1-6-2012
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2013 at 08:01
Raney Nickel with Pd/C - how clean and re-activate?


Hi. I'm working with Raney Nickel (300g) and Pd/C 10% (10g). After two uses this catalyst no working. I wash some distilled water but this no good results.

Please, how I clean and re-activate this mixture catalyst? Thanks for reply.
View user's profile View All Posts By User
EdMeese
Harmless
*




Posts: 16
Registered: 25-1-2013
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2013 at 14:49


depends entirely on what you did with it, but lacking any and all details, first guess is to cook it. 300 °C in a 5%H2/N2 atmosphere maybe.
View user's profile View All Posts By User
R.Esposito
Harmless
*




Posts: 11
Registered: 1-6-2012
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2013 at 01:34


Pd/C 10% can be cleaned by NaOH to pH 7. Palladium lost activity at the 2 times using.
Problem is mixture this 2 types of catalyst. I got some reference, must read and try.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 29-1-2013 at 19:15


What are you doing with the catalyst? You didn't say.

Assuming it is hydrogenation. You could try cautiously soaking it in 3% hydrogen peroxide, with acetic acid, with warming.

This might partially reactivate your catalyst, or not.

As always, eventually....you will have to redissolve the Palladium content, and use the resulting Pd salt, to form fresh catalyst.