lead styphnate synth failure


what is the likely failure points in this reaction

produces what looks like styphnic acid, very pale yellow ppt.

above reacts with mag carbonate suspended in water to give clear solution, dil nitric acid added, followed by lead acetate solution at ~70c.

this produces a pale yellow ppt. which is a flammable solid, not explosive.

any ideas anyone?

dave321
View user's profile View All Posts By User
badabooom
Harmless
*




Posts: 24
Registered: 10-8-2012
Location: running around the nucleus
Member Is Offline

Mood: bangin

[*] posted on 9-1-2013 at 00:32


Hi there,

Have a look at my thread. http://www.sciencemadness.org/talk/viewthread.php?tid=21124

I would suggest you use Lead Nitrate rather than Lead Acetate.

I hope his helps.
View user's profile View All Posts By User
caterpillar
Hazard to Others
***




Posts: 472
Registered: 8-1-2012
Member Is Offline

Mood: No Mood

[*] posted on 9-1-2013 at 01:17


I can give you the link to russian book on primaries: http://pirochem.net/index.php?id1=3&category=chemvvisost... . Here author recommends to use lead nitrate, not acetate. But most likely problem was caused by what you think is styphnic acid. Try its MP at least. I made this compound, but finally converted it to ammonium salt and blew up, using TATP as detonator



Women are more perilous sometimes, than any hi explosive.
View user's profile Visit user's homepage View All Posts By User
Microtek
National Hazard
****




Posts: 849
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 10-1-2013 at 09:04


"Very pale yellow" doesn't sound like styphnic acid (mine was dark orange, almost reddish) and my Mg-styphnate soln was a deep red, very strong colour. I also used lead nitrate for the precipitation of Pb-styphnate.
View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 10-1-2013 at 12:24


Pure styphnic acid is extremely pale yellow even lighter than picric acid, and a yellow about like the color of a legal pad is as dark as it will be if it is pure.

See a picture at the following link

http://www.sciencemadness.org/talk/viewthread.php?tid=4457&a... pictoral of synthesis by pdb

http://www.sciencemadness.org/talk/viewthread.php?tid=4457&a... synthesis described by Rosco

[Edited on 10-1-2013 by Rosco Bodine]