Author: Subject: Nitric acid/silver nitrate stains
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 3-12-2012 at 17:53
Nitric acid/silver nitrate stains


I just had a glove leak today when I was working with my silver purification. My right glove leaked and I didn't realize it at first, now I have black and brown stained fingers and hand. Is there anything but time that will remove these stains?
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 3-12-2012 at 17:58


Sandpaper?



Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
kristofvagyok
National Hazard
****




Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline

Mood: No Mood

[*] posted on 3-12-2012 at 18:16


Sandpaper +1.

But be happy, there are several things that can color your hand and looks much worse;)




I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:

"You can’t become a chemist and expect to live forever."
View user's profile Visit user's homepage View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 3-12-2012 at 18:28


i am going on a week with stained hands and at least eight of my fingernails blackened by nitric acid. its common for me to go about with one or two damaged nails but 8 is going to be pretty bad.right now i got my nails covered with white nail polish and it has slowed my nails from cracking all the way.if the nail polish doesnt work then i will have it pretty bad for a week or so of painful raggety nails as nitric will weaken nails. i have had my nails crack all the way down passed the middle and have waited until they grew out again,it really sucks because they snag on everything. i just plain forgot about gloves and i dont even want to know what people think about me when they see my hands.
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 4-12-2012 at 18:14


Luckily, my solution was pretty loaded down with silver and base metals at the time or it would have been worse. I was only working with ~33% nitric to begin with and it had been working on 350 grams of sterling for a while.
View user's profile View All Posts By User
kuro96inlaila
Hazard to Self
**




Posts: 96
Registered: 21-6-2010
Location: Malaysia
Member Is Offline

Mood: Quietly thinking

[*] posted on 5-12-2012 at 07:10


I don't think there is other efficient way to remove the stains than time and skinning.:P
Because the stains it self is reacted keratin.Silver react with keratin to form light sensitive compound and nitric acid nitrated the keratin.




http://www.youtube.com/user/kuro96inlaila

Genetic assortment is the dices of God
View user's profile Visit user's homepage View All Posts By User
zed
International Hazard
*****




Posts: 2284
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 7-12-2012 at 14:56


Nope! We've all had 'em. The stains will be with you until the skin eventually wears off. You will have a nice long time being reminded of your negligence.

This experience helped me enormously when I was actively playing with chemicals. Made me really cautious about contamination. And thus, even at my fairly advanced age, I do not have the shakes, the heebie jeebies, or the creeping crawling internal crud we call cancer.

Silver Nitrate contamination on skin, produces a flashy but benign condition, that reminds us of our mortality, and the power of an invisible amount of a chemical to have a profound effect upon us.
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 7-12-2012 at 15:46


Had to take the Pediapaw to my own nails instead of the dogs. Sheesh, I'm getting more use out of it then she does.
View user's profile View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 7-12-2012 at 17:06


one week has passed since i damaged eight of my fingernails and have to say that nail polish has helped a lot.my nails will begain to crack almost immediately if a chunk of nail polish breaks off and leaves the nail exposed. i think i'm gonna beat this and am starting to love nitric again... and revlon.
View user's profile View All Posts By User

  Go To Top