Titanium Electroplating!
Can I plate Titanium from a solution of Ti sulfate, chloride, nitrate or other!?
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
I had figured no since titanium is usually won as the free metal not by electroplating but by a cumbersome process involving titanium tetrachloride,
here is a link, that for the most part says the same thing though it does give some pointers on possibilities:
Titanium Plating
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Bromic I really wish I had your knowledge of chemistry. Since I do not this may be a stupid question, is the problem of reduction of hydrogen before
the reduction of titanium able to be overcome by using some type of conductive organic solvent rather than some type of water chemistry. The reason I
ask is I have lots of titanium metal and always wondered what the hell can I do with it, and this all sounds very interesting!
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Really, what form is it in? One of these days I'm going to melt and cast titanium, providing of course I get a source of argon and am somehow able to
sinter magnesium oxide for the crucible AND mold...
Tim
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Yeah, in the non-aqueous mediums it may be possible to plate titanium. As was mentioned in that thread I linked to, aluminum can be electroplated in
toluene. The exact method involves the use of aluminum bromide, anhydrous of course, with toluene (I think a 6 M solution can be made) and an
additive Quote: | an additive selected from the group consisting of aromatic hydrocabons having at least two rings; alkylated monocyclic or polycyclic aromatic
compounds, aminosubstituted and halosubstituted mono- or polycyclic aromatic compounds, dialkyl aniline, trialkyl amine; D. Bromides or iodides
selected from the group consisting of alkali metal halides, alkaline earth metal halides, boron halides, ammonium halides, aliphatic and aromatic
quaternary ammonium halides and mixtures of any of these. | Also a small amount of ionic bromide such as
potassium bromide is added. I think the additive is just to help remove any free bromine being produced. The patent is 3,997,410. So by entention
it may be possible to do something with titanium, something covalent like titanium tetrachloride might be useful, similarly titanium tetrachloride is
also a lewis acid. However doing a quick patent search revealed no patents to give titanium metal via electrolysis in any phase but a molten salt
phase. Never the less there may be reasons for this beyond if it is feasible or not, the price of titanium tetrachloride being prohibitively high
with respect to aluminum bromide, so it may be possible to preform an anologous reaction, it may just be that no one has tried it yet.
[Edited on 12/12/2005 by BromicAcid]
|
|
futiant
Harmless
Posts: 1
Registered: 10-9-2006
Member Is Offline
Mood: No Mood
|
|
NO, Bromide. you can see jappanese patent JP1031990 for TITANIUM ELECTROPLATING. I had not try this, BUT I'd very interested of this.
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Reference Information
TITANIUM ELECTROPLATING BATH AND PLATING METHOD USING SAME
Publication number: JP1031990
Publication date: 1989-02-02
Inventor: TAKAHASHI SETSUKO
Applicant: NISSHIN STEEL CO LTD
Classification:
- international: C25D3/54; C25D3/02; (IPC1-7): C25D3/54
- european:
Application number: JP19870189564 19870729
Priority number(s): JP19870189564 19870729
Abstract
PURPOSE:To form a dense and uniform Ti plating film at low temp., by carrying out electroplating in a dry and oxygen-free atmosphere by using a
plating bath composed of Ti chloride, alkylpyridinium halide, and specific organic solvent and also using direct current or pulse current.
CONSTITUTION:Electroplating is applied to the cathode to be treated in an oxygen-free atmosphere of dry N2, Ar, etc., by means of direct or pulse
current in 0.1-10A/dm<2> current density by using a soluble anode made of Ti and also using, as a plating bath for Ti electroplating, a molten
salt plating bath consisting of 50-80mole%, in total, of one or two kinds among Ti chlorides, such as TiCl3 and TiCl4, 20-50mole% of 1-4C
alkylpyridinium halide of alkyl proup, and <=75vol.% of organic solvent, such as toluene, xylene, and benzene. At this time, by using the plating
bath of the above composition, the dense and uniform Ti plating film can be formed by means of a plating bath with a relatively low temp. of 20-150
deg.C without causing oxidation.
[Edited on 11-9-2006 by solo]
[Edited on 11-9-2006 by solo]
Attachment: titanium electroplating.pdf (67kB) This file has been downloaded 1312 times