trinitrotoluene
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 142
Registered: 17-10-2002
Location: California
Member Is Offline
Mood: paranoid
|
|
Preparation of Barium
I am curious about this method.
Reacting barium oxide BaO with Al or Si
3 BaO+2Al > 3 Ba+Al2O3
Correct me if i am wrong. I think its like the thermite reaction.
[Edited on 26-3-2005 by chemoleo]
TNT
|
|
rikkitikkitavi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 192
Registered: 17-6-2002
Member Is Offline
Mood: No Mood
|
|
that means that for the reaction deltaH is
-31kJ as written (or -10,33 kJ/mole Ba)
Hr = -1675 - (3* - 548) = - 31 kJ
I wouldnt call it a thermite reaction, since the reaction only produces very little heat compared to a standard thermite reactiion.
You have to look at the Gibbs free energy for those compounds to se if it is a spontaneous reactionn (i e possible)
The same calculation is made with Gibbs free energy for the compounds. If Gr > 0 it is a spontaneous reaction, i e it progree to the right as written
in the text.
Spontaneous doesnt mean that the reaction starts by itself, you need to add enough activation energy to get it started, f e x by a external heat
source, then the heat released will make the reaction progress.
In this case, since the heat output is so low, I would assume that the reaction will quench immetiately if the heat source is removed. How much heat
and more important, how high temperature I cant tell. But I guess you have to heat it to atleast 1000 C before anything happens.
/rickard
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
You'll need protective and totally inert (noble gas, Ba reacts with N2) from begin to end, as barium reacts with all gasses in the atmosphere, even at
room temperature. That's why it's often used to create extreme low pressure vacuum.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
BASF
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 282
Registered: 5-11-2002
Member Is Offline
Mood: hydrophilic
|
|
You need quartz glass(up to 1710°C).
It´s not that expensive as one would think.
|
|
trinitrotoluene
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 142
Registered: 17-10-2002
Location: California
Member Is Offline
Mood: paranoid
|
|
Is there different way to get Barium like electrolysis of Barium Salts? If so which ones would you suggest?
TNT
|
|
Jstuyfzand
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline
Mood: Learning, Sorta.
|
|
From the wiki, Barium Chloride.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Electrolysis of a barium salt aqueous solution with a mercury cathode, followed by distilling off the mercury from the amalgam (under vacuum or argon)
should work.
[Edited on 11-7-2016 by blogfast25]
|
|