Aluminum Powder
What can I use for thermite?
-Aluminum foil, ball milled until fine powder: Failed every time for me so far, don't know why.
-Powdered metal lumps: Haven't tried, will probably work better.
-Official source (e.g. Elemental-Scientific, etc.)
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
hyfalcon
International Hazard
   
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
http://alphachemicals.com/aluminum_powder
Works quite well with all my regular thermite reactions I've tried. I'm going to start working on the TiO2 thermites next.
|
|
siegfried
Harmless
Posts: 18
Registered: 15-8-2012
Member Is Offline
Mood: No Mood
|
|
Use 3 parts by weight of Technical grade Ferric(ous)Oxide Fe3O4 and 2 parts by weight of Aluminum powder 100 mesh for the best results. Ignite by
magnesium ribbon or KClO4/Mg mix using a fuse (flash powder). Can be stored dry in a glass bottle for many years.
Example: 60g Fe3O4 + 40g Al = 100g Thermite
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Well, I'm not so much interested in the classical iron thermite as in the other possible thermites, like chromium, or manganese. I want to know either
if there's something wrong with my existing stock, or if I'm igniting it wrong.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
triplepoint
Hazard to Others
 
Posts: 127
Registered: 11-4-2012
Location: U.S.
Member Is Offline
Mood: in equilibrium
|
|
So, you're interested in exotic thermites? Perhaps you should take alook at the exotic thermite thread: http://www.sciencemadness.org/talk/viewthread.php?tid=10249&...
|
|
platedish29
Hazard to Self

Posts: 76
Registered: 2-9-2012
Member Is Offline
Mood: absorbing CO2
|
|
Thats much mote way liker exodia o0
..
seems proud of blender volcano
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
I guess I'll try cutting through some aluminum scrap I have, then. Aluminum should be able to ignite on its own, correct?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Poppy
Hazard to Others
 
Posts: 294
Registered: 3-11-2011
Member Is Offline
Mood: † chemical zombie
|
|
Drop iron oxide inside molten aluminum. You don't have to put your head right above the demonstrating reaction.
It's denser, and will submerge.
Bro tip: add coating to the oxide.
|
|
hyfalcon
International Hazard
   
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
You trying to get someone hurt?! Don't EVER drop anything into molten aluminum! As far as ignition goes, I just use a common sparkler. A lot
cheaper than Mg ribbon.
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Well, with a proper heat sink mixed in, you could do it the other way around and drip molten aluminum into the crucible.
Molten aluminum isn't scary. It's like gallium, only painfully hot to touch. No sputtering, splashing, sloshing, etc.
What kind of coating?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Poppy
Hazard to Others
 
Posts: 294
Registered: 3-11-2011
Member Is Offline
Mood: † chemical zombie
|
|
Some coating to make sure the dripped oxides won't clump like chocolate powder in milk when they reach the molten aluminium.
In fact I think its suicidade, but as you working with chromium that would be somehow slow and controllabe. o0?
Blogfast gave me a good idea in the neodymium thread. Use some low heat of formation Cr3+ compound other than the oxide, this will slow even more the
process. Choose a suitable anion as to proceed to the reaction with vigorous heating, sufficient to melt elemental chromium, but low enough to evade
explosions/ boiling
Just use ropes and hooks to stay very much away from it
[Edited on 9-4-2012 by Poppy]
|
|
MadHatter
International Hazard
   
Posts: 1352
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Ignition
I've used cheap sparklers to ignite thermite. Use a propane or MAPP gas torch to ignite
the sparkler. You'll wear out a butane. If it's warm enough I suggest potassium
permanganate with a couple drops of glycerine. That's more than hot enough to get
the reaction started. KMnO4 is still available at some Sears stores for use in iron
water filters. Won't be cheap but it was a convenient source and you don't need too
much.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
ItalianChemist
Hazard to Others
 
Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline
Mood: No Mood
|
|
Only powder works well for thermite! You can buy it from ebay!
|
|
Poppy
Hazard to Others
 
Posts: 294
Registered: 3-11-2011
Member Is Offline
Mood: † chemical zombie
|
|
Why don't you start making your own aluminium powder?
Make a high melting point metallic cilinder, plug a pressurizing on top, nozzle at bottom. Open nozzle valve: you should get aluminium spray. collect
in a closed container filled with CO2. Let cool
Find a way to separate it according to mesh size.
|
|
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Well, you could try using Al from a different source, just until you get your bearings.
The folks at http://www.firefox-fx.com/ would probably be happy to sell you anything the law allows.
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Uh, Poppy, I have no idea how to build one of these, and even if I got all that, the Al produced would be pyrophoric.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Poppy
Hazard to Others
 
Posts: 294
Registered: 3-11-2011
Member Is Offline
Mood: † chemical zombie
|
|
Yea. It wouldn't be THAT expensive. Just find a proper workshop to prepare the fittings for you.
As for the Al being pyrophoric, the powder should be allowed to form an oxide layer which passivates the action of the enviroment preventing it from
burn, melt furthermore explode. The process of passivation must be slow and cold, controllabe.
Does water bring you anything into mind?
Ever experienced dripping molten lead into water?
Again, use pulley and belts to stay behind the walls! Good luck!
Best regards, Poppy.
[Edited on 9-12-2012 by Poppy]
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Ever reacted aluminum with water? I'm pretty sure it reacts.
So, it would be like an extruder with a fine particle size mesh, made entirely of stainless steel?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
triplepoint
Hazard to Others
 
Posts: 127
Registered: 11-4-2012
Location: U.S.
Member Is Offline
Mood: in equilibrium
|
|
What are you using as your ignition method?
Ball milled foil should be fine enough to give reliable results.
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Blowtorch. Don't have any reliable chemical methods on hand, and just somehow lost my newly made stock of sodium nitrate.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Poppy
Hazard to Others
 
Posts: 294
Registered: 3-11-2011
Member Is Offline
Mood: † chemical zombie
|
|
Quote: Originally posted by elementcollector1  | Ever reacted aluminum with water? I'm pretty sure it reacts.
So, it would be like an extruder with a fine particle size mesh, made entirely of stainless steel? |
Sorry I couldn't get to the point of yours.
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Aluminum reacts with water when fine enough, forming aluminum hydroxide and hydrogen. This ruins the powder as it builds up more oxide than actual
aluminum.