Lithium and nitrogen
Simple question :
According to http://en.wikipedia.org/wiki/Lithium
Lithium is the only metal which reacts with nitrogen under normal conditions.
So, it can't be stored in pure N2 otherwise it forms a layer on nitride on its own?
|
|
Kalium
Harmless
Posts: 33
Registered: 21-6-2012
Location: Australia
Member Is Offline
Mood: No Mood
|
|
"Crystalline lithium nitride, stable in air, characterized by a sodium content of less than 5×10^-2 weight-percent, a potassium content of less than
10^-2 weight-percent, a magnesium content of less than 1×10^-2 weight-percent, and a silicon and iron content of 10^-2 to 10^-3 weight-percent each;
is obtained by heating lithium having a purity of at least 99.9% in a vessel made of tungsten, niobium, ruthenium or tantalum in a nitrogen atmosphere
at a pressure of at least 250 mm Hg in the absence of oxygen and water at a temperature of from 300° C. to the melting point of lithium nitride."
Under room temperature, I think only a negligible amount of lithium nitride will form.
|
|
Nicodem
Super Moderator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
It can be stored under nitrogen, but such storage is of no use, because the nitrogen will react with lithium in few days. You need to use
argon if you want it clean from the nitride and oxides.
…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being
unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their
scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)
Read the The ScienceMadness Guidelines!
|
|
vmelkon
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
Quote: Originally posted by Nicodem ![](images/xpblue/lastpost.gif) | It can be stored under nitrogen, but such storage is of no use, because the nitrogen will react with lithium in few days. You need to use
argon if you want it clean from the nitride and oxides. |
Thanks.
|
|
Vargouille
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 380
Registered: 16-4-2012
Member Is Offline
Mood: No Mood
|
|
There's a video where a piece of cut lithium begins to darken fairly quickly from reaction with nitrogen.
[Edited on 4-8-2012 by Vargouille]
|
|
vmelkon
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
That is odd. I assume it forms a mixture of oxide (white) and nitride (red purple?).
According to wikipedia, the nitride is red purple but on the video, it seems brown.
|
|