Sodium fluoride attacks glass?
According to it's MSDS, sodium fluoride is incompatible with glass. Does this mean that solid sodium fluoride should not be stored in glass containers, or would
the corrosive effects only be significant in solution?
Also, how would it attack glass? Would it attack the silica, or another component of the glass? If it is the silica, could sodium fluoride and
finely divided silica be used to prepare silicon tetrafluoride, without having to use (insanely dangerous) hydrofluoric acid?
1f `/0u (4|\\| |234d 7|-|15, `/0u |234||`/ |\\|33d 70 937 0u7 /\\/\\0|23.
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
This is due to hydrolysis, F- is a weak base as HF is a weak acid:
F<sup>-</sup> + H<sub>2</sub>O <---> HF + OH<sup>-</sup>
The HF attacks the glass and is removed from the equilibrium, which then shifts..etc.
[Edited on 13-8-2004 by vulture]
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
bennator
Harmless
Posts: 12
Registered: 19-6-2004
Location: Ohio, USA
Member Is Offline
Mood: No Mood
|
|
I would assume that such attack would only occur in large amounts in solution, however, powdered NaF could react with water vapor in the air to form
HF which could also attack glass. I don't think it would be something to worry about too much, but the risk could still be there.
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Sodium fluoride is sold in poly bottles according to my Fisher catalog. I'm assuming that this isn't due to poly being cheaper than glass
but to prevent attack from the HF that would be formed from water vapor in the air. My chemistry text says HF has the unusual property of attacking
glass:
4HF + SiO2 -> 2H2O + SiF4
If you pumped moist air through the powdered reactants perhaps some SiF4 would form. You would still have HF present, just in smaller, more
controllable amounts. And if the reaction was prompt it would all be consumed in situ. But I wouldn't want to try this without a lot
more homework, and proper safeguards.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Polverone
Now celebrating 21 years of madness
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline
Mood: Waiting for spring
|
|
Go to a pottery supply place and get yourself the finest-powdered silica and calcium fluoride they have. Mix, add sulfuric acid, and (optionally)
warm, in an expendable or HF-resistant vessel. SiF4 for your chemical pleasure! Lungs? You don't need any steenkin' lungs.
Or you could do this with NaF, if you already have it on hand. But I'm pretty sure you need the acid to have a decent rate of production, and you
want it to be a water-hungry acid to keep the SiF4 dry.
PGP Key and corresponding e-mail address
|
|
Marvin
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
I think the hydrolysis explanation is a little stretched. Particually when NaF is the salt of a strong base and a weak acid (making it basic) and
SiO2 is an acidic oxide.
I would have though the first product would be a salt of fluorosilic acid. Its quite plausable heating this would produce SiF4.
|
|
Theoretic
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 776
Registered: 17-6-2003
Location: London, the Land of Sun, Summer and Snow
Member Is Offline
Mood: eating the souls of dust mites
|
|
The way NaF could dissolve glass (although I think it would proceed at a reasonable rate at high t only) is like this:
6NaF + 3SiO2 => Na2SiF6 + 2Na2SiO3
Then (maybe):
Na2SiF6 + 2Na2SiO3 <=> 3Na2SiO2F2 (the complex anion SiO2F2--, akin to AlO2F2---, that froms when Al2O3 dissolves in cryolite, also NaF will
corrode alumina in a similar way)
Or directly:
2NaF + SiO2 => Na2SiO2F2
|
|
GreenD
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
I recently attemped this on borosilicate glass. NaF + H2O -> nothing after 10 minutes.
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
Nothing? What do you consider as "anything"?
If you had a mass spectrometer, you'd see quite a bit of changes in the solution. It doesn't have to visibly gulp the glass in a speedy fashion.
Dilluted hydrofluoric acid doesn't do that, either, yet it eats glass.
|
|
DJF90
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline
Mood: No Mood
|
|
Not quite what this thread is about, but a saturated solution of KHF2 in a 1.75ml glass vial has shown very little corrosion/etching over the past
couple of months (I made the solution to check whether a glass vessel should be used for the intended preparation of a potassium trifluoroboronate
salt).
|
|
GreenD
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
No expected observations, smart ass.
|
|
Zan Divine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 170
Registered: 3-12-2011
Location: New York
Member Is Offline
Mood: Wishing all the worst that life has to offer to that SOB Wayne Lapierre
|
|
I have a sample of NaF which has been stored in a glass bottle with a PE/Phenolic closure since 1997. The glass has no visible signs of attack.
The vial is borosilicate, however, not soft glass as found in most bottles.
|
|
Zan Divine
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 170
Registered: 3-12-2011
Location: New York
Member Is Offline
Mood: Wishing all the worst that life has to offer to that SOB Wayne Lapierre
|
|
The equilibrium constant for HF + NaOH <--> NaF + H2O is obviously a large number.
Where that equilibrium lies isn't the only factor. Removal of HF by the glass guarantees that more HF will result.
The shifting of equilibriums is a very powerful force.
You could use a loosely analgous argument to say that you can't reduce cesium compounds with carbon. But, the fact is, you can.
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
OH, let me get this right. You guys think soluble fluorides could be stored in glass containers? That the whole corrosion is an overblown myth?
Do you know why threy are stored in plastic? Because if something is a "reagent", it has a declaration on the bottle, saying something like "This
sample contains a reagent X and impurities Y. The amount of impurities Y is Z(Y) and the manufacturer guarantees that until the date of
expiration."
The salt doesn't have to chew the fuck up its container (or even etch it visibly) in order for the manufacturer to put it in another one, made from
different materials. It only has to be altered beyond the manufacturer specification, and that's what happens with soluble fluorides in glass jars.
They get contaminated.
The whole issue here is so... elementary school level or lower.
|
|
GreenD
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
Read the title, lol. I really don't like you Quote: Originally posted by Endimion17 ![](images/xpblue/lastpost.gif) | OH, let me get this right. You guys think soluble fluorides could be stored in glass containers? That the whole corrosion is an overblown myth?
Do you know why threy are stored in plastic? Because if something is a "reagent", it has a declaration on the bottle, saying something like "This
sample contains a reagent X and impurities Y. The amount of impurities Y is Z(Y) and the manufacturer guarantees that until the date of
expiration."
The salt doesn't have to chew the fuck up its container (or even etch it visibly) in order for the manufacturer to put it in another one, made from
different materials. It only has to be altered beyond the manufacturer specification, and that's what happens with soluble fluorides in glass jars.
They get contaminated.
The whole issue here is so... elementary school level or lower. |
|
|