darkflame89
Hazard to Others
 
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Separating borax from a mixture?
I need a little help: does anyone have any idea how to separate borax from a mixture of powdered borax and powdered hand soap?
Ignis ubique latet, naturam amplectitur omnem.
|
|
|
guy
National Hazard
  
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
From my searching, it seems that borax only dissolves 6grams/100grams of water.
So maybe dissolve all the soap and then collect the borax
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
If this doesnt work:
1. Dissolve all your borax/soap in water, make it as concentrated as possible.
2. Add HCl conc, and preciptate the fatty acids AND H3BO3.
3. Filter precipitate.
4. Shake up the precipitate with acetone. The fatty acids will dissolve, while H3BO3 won't. Do that 2-3 times to get completely rid of the fatty
acids. Dont use ethanol, as it will react with the H3BO3 to a small extent - particularly if HCl is still present.
Then you can do whatever you want with the boric acid - i.e. backreact it with the appropriate amount of NaOH to get your borax back.
That should definitely work
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
darkflame89
Hazard to Others
 
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Must it be conc. HCl? I understand that acids are required to hydrolyse the soap to fatty acids, but i don't have such acids. The strongest
concentration of HCl OTC is 9%. Could some other be used to convert all that soap to insoluble salts in water?
Ignis ubique latet, naturam amplectitur omnem.
|
|
|
fvcked
Harmless
Posts: 45
Registered: 11-4-2004
Member Is Offline
Mood: Groggy
|
|
"The strongest concentration of HCl OTC is 9%. "
Go to a pool supply house, they have 35% HCl. I have also found it by the paint supplies at a wal mart and a menards.
EDIT, didnt know you live in singapore, but for others in different countries the above stands.
[Edited on 11-8-2004 by fvcked]
|
|
|
darkflame89
Hazard to Others
 
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
The country where i live in ain't have any pool supply house. because there's only public pool in Singapore, and common people don't
buy such chemicals as there are no private pools or such. Such pool supplies must be obtained directly from the manufacturer. As such this is a big
problem to me for i do not know where the manufacturer is.
[Edited on 11-8-2004 by darkflame89]
Ignis ubique latet, naturam amplectitur omnem.
|
|
|
guy
National Hazard
  
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
You can always make your own HCl
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Use dilute HCl, then evaporate off the water, leach the fatty acids out with acetone then wash the salt off with as little water as possible.
|
|
|