[*] posted on 15-7-2012 at 20:00
ZnSO4 or ZnO


If i boil down a Zinc Sulfate solution or a Zinc Chloride solution will it just be a zinc sulfate powder or will it decompose to Zinc Oxide?

-AMchemistry
View user's profile Visit user's homepage View All Posts By User
DoctorOfPhilosophy
Hazard to Others
***




Posts: 130
Registered: 12-6-2012
Location: Ontario, Canada
Member Is Offline

Mood: enthralled

[*] posted on 15-7-2012 at 20:07


if you heat zinc sulfide, any bonded water will evaporate. Once it's anhydrous, is can be heated to 680 °C before it decomposes to the oxide.
Zinc chloride will melt and then boil on heating.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8003
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 15-7-2012 at 22:30


TheAMchemistry87 talks about sulfate, not sulfide. The sulfate indeed is stable and can be evaporated to dryness and loose its bonded water.

The chloride is less stable. From aqueous solution you can prepare the hydrate, but the pure anhydrous salt cannot be formed by simply heating. The chloride will loose HCl, besides water, and an insoluble mix of zinc hydroxide/oxide and zinc chloride will remain behind. Maybe even all chloride is lost as HCl and zinc oxide remains behind, but I'm not sure about that.


[Edited on 17-7-12 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
DoctorOfPhilosophy
Hazard to Others
***




Posts: 130
Registered: 12-6-2012
Location: Ontario, Canada
Member Is Offline

Mood: enthralled

[*] posted on 15-7-2012 at 22:54


Oops, that's a typo. But here is the MSDS saying that zinc sulfate does decompose

link
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8003
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 15-7-2012 at 23:35


Zinc sulfate is stable at ordinary temperature, but at sufficiently high temperature, it indeed can be decomposed, like most sulfates. Some sulfates loose SO3, others loose SO2 or a mix of both.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
weiming1998
National Hazard
****




Posts: 616
Registered: 13-1-2012
Location: Western Australia
Member Is Offline

Mood: Amphoteric

[*] posted on 16-7-2012 at 03:57


Quote: Originally posted by TheAMchemistry87  
If i boil down a Zinc Sulfate solution or a Zinc Chloride solution will it just be a zinc sulfate powder or will it decompose to Zinc Oxide?

-AMchemistry


To answer your question, first we need to know what zinc sulfate and zinc chloride solutions are made of.

Both zinc sulfate and zinc chloride are in the form of Zn2+ and SO4(2-) ions. The Zn2+ ions are Lewis acidic, and forms an adduct with water, [Zn(H2O)6]2+, which hydrolyzes further to produce [ZnOH(H2O)5]+ and H+ ions, making the solution mildly acidic. This causes very small amounts of HCl to exist in equilibrium with the other species in a zinc chloride solution and very small amounts of H2SO4 and HSO4- to exist in a solution of zinc sulfate.

The two acids are different, HCl being far more volatile, so when zinc chloride solution is boiled dry, the small amounts of HCl escape, causing a shift in the equilibrium, with all the HCl finally leaving only dry ZnO left. Approximate equation: [Zn(H2O)6]2+(aq) + 2Cl-(aq)=====>ZnO(s)+2HCl(g)+5H2O(g).

Sulfuric acid, on the other hand, is less volatile than water, and will not boil off even when the temperature is enough to dehydrate the ZnSO4 hydrate to ZnSO4 anhydrous. So nothing happens when you dehydrate it. You just get anhydrous ZnSO4. At much higher temperatures though, it can decompose to SO3, which all sulfates except reducing sulfates (like iron (II) sulfate and ammonium sulfate) decompose to.
View user's profile View All Posts By User
bbartlog
International Hazard
*****




Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline

Mood: No Mood

[*] posted on 16-7-2012 at 08:02


Quote:
with all the HCl finally leaving only dry ZnO left. Approximate equation: [Zn(H2O)6]2+(aq) + 2Cl-(aq)=====>ZnO(s)+2HCl(g)+5H2O(g).


Not so simply, though. The first decomposition (after the monohydrate ZnCl2.H2O is obtained) is roughly to Zn(OH)Cl,
ZnCl2.H2O -> Zn(OH)Cl + HCl,
then to ZnO plus ZnCl2,
2Zn(OH)Cl -> ZnO + ZnCl2 + H2O (somewhere around 300C)
...and then finally if enough heat is applied the ZnCl2 is also vaporized, presumably somewhere around the boiling point of 756C. At which point you would have ZnO, but only because you'd vaporized the remaining ZnCl2.