[*] posted on 13-7-2004 at 20:12
Electrolysis of MgSO4


Ok, I tried something new and I think it worked. I put about a half cup of MgSO4 (Epsom Salt) and a 2 tablespoons of water in a cup then mixed them. Next, I placed 2 wires in the cup. These had 18 volts going through them. Several different things seemed to be produced, but the one that caught my attention may have been sulfur. The water was the exact same color as sulfur. So, I tried to filter the solution several times, and every time nothing stayed in the filter. I expected some sulfur to be left behind because it is nonsoulable in water. Does anybody know: If sulfur really was produced, and if it was, why didn't any stay behind? Thanks.

[Edited on 5-8-2004 by chemoleo]
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3255
Registered: 13-7-2003
Location: Wisconsin
Member Is Online

Mood: Rock n' Roll

[*] posted on 13-7-2004 at 20:16


One key question, these two wires placed in solution, what material were they? Copper, iron, nickel...?



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
tommy1641
Harmless
*




Posts: 3
Registered: 13-7-2004
Member Is Offline

Mood: No Mood

[*] posted on 13-7-2004 at 20:18


The wires were copper. Sorry for not saying earlier.
View user's profile View All Posts By User
darkflame89
Hazard to Others
***




Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline

Mood: No Mood

[*] posted on 14-7-2004 at 01:04


Copper wires? Then the color of the solution might have been due to the dissolved Copper..



Ignis ubique latet, naturam amplectitur omnem.
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 14-7-2004 at 02:20


The solution would turn bluish if it was copper, not yellow :o

And how does 1/2 a cup of epsom salt dissolve in 2 table spoons of water? Or did you electrolyse a bowl of soggy crystals :o




"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to... satisfy any applicable law, regulation or legal process"
View user's profile View All Posts By User
frogfot
Hazard to Others
***




Posts: 212
Registered: 30-11-2002
Location: Sweden
Member Is Offline

Mood: happy

[*] posted on 14-7-2004 at 02:21


CuOH is yellow, and insoluble in water (it should dissolve in HCl, making complexes.. might be a good test).

[Edited on 14-7-2004 by frogfot]
View user's profile Visit user's homepage View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 14-7-2004 at 02:26


Oops, my bad. Ive never managed to make or see CuOH, only Cu(OH)2 :P



"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to... satisfy any applicable law, regulation or legal process"
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


[*] posted on 16-7-2004 at 14:29


I would expect magnesium hydroxide to be produced at the cathode (negative terminal); this would have the color of precipitated sulfur (white). Not sure where the yellow would come from, though.
View user's profile View All Posts By User
Sarevok
Harmless
*




Posts: 33
Registered: 16-12-2003
Member Is Offline

Mood: No Mood

[*] posted on 17-7-2004 at 18:27


Aqueous electrolysis of this salt will merely produce oxygen and hydrogen. Sulfur will not be formed.

EDIT: The yellow color is probably due to the presence of cuprous hydroxide (Cu+ from the oxidation of your electrodes and OH- from the reduction of water).

[Edited on 18/7/2004 by Sarevok]
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 5-8-2004 at 00:02


It's very unlikely it is sulphur, indeed. I am not aware of an easy electrolytical process that reduces sulphate to sulphur.
I imagine all you'd get is H2 and O2, as the gasses coming off the electrodes.
As to the colour.... impurity!
Cuprous hydroxide CuOH was mentioned, but like the cupric hydroxide Cu(OH)2 both are insoluble. Additionally, CuOH undoubedly reacts either to Cu2O (insoluble once again), or it is oxidised with AIR, to form green/turquoise Cu2+ salts (or rather, as Saerynide says, blue, as CuSO4 would be formed)
So I doubt its down to the copper. More likely it's some other impurity.

In addition it does help if you get your weight units sorted. Cups and spoons dont really help :o
WAs the final solution cloudy yellow, or clear yellow? Precipitates at all?




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5130
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 5-8-2004 at 12:31


Copper (I) oxide is yellowish or reddish, and, like sulphur, would form a precipitate.
It's low solubillity means that suspensions of it in water are fairly stable.
My money is definitely on Cu2O, possibly hydrated.
Most impurities in copper wire are not popular because they reduce the conductivity.
If the MgSO4 was pharmaceutical grade it would be pretty pure too.
Why postulate some "impurity" when Cu2O is reasonably probable?
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 5-8-2004 at 12:46


Yes i wonder that myself now.
I am just not aware of ever having prepared Cu2O with a colour 'exactly like sulphur'. The commercial batch I have is a deep red, and some preps I did brought it up to orange red, but definitely not sulphur yellow. Who knows... I guess colour depends on the manner it was prepared :)

Anyway, tommy, the issue can be easily solved if you subject your yellow precipitate (which you should filter off) to HCl(aq). If it is Cu2O, it will react with it, forming initially a white precipitate, which, on air, will slowly solubilise and turn dark green (CuCl2).




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1349
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 5-8-2004 at 19:43
Electrolysis


Tommy1641, if you decide to do it again I suggest using "gouging" rods,
then check your results. I use these for chlorate/perchlorate production.
Metal anodes and cathodes are likely to combine with the products
they produce.




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User

  Go To Top