Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Hydrazine Sulfate As A reducing Agent For Electroless Plating
jpsmith123
National Hazard
****




Posts: 764
Registered: 24-6-2005
Member Is Offline

Mood: No Mood

[*] posted on 27-8-2005 at 14:06
Hydrazine Sulfate As A reducing Agent For Electroless Plating


Does anyone know if hydrazine sulfate can replace the sodium hypophosphite or borohydride used as a reducing agent in electroless plating? Apparently its use in this manner is mentioned in some patents, but there's not a lot of practical information on it.

Regards,
Joe
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5115
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2005 at 06:57


well, this site
http://66.102.9.104/search?q=cache:pMhyPEJzZr8J:boyles.sdsmt.edu/cumirror/cumirr.ppt+%22copper+mirror%22+hydrazine&hl=en
says you can plate copper using hydrazine as a reductant.
View user's profile View All Posts By User
jpsmith123
National Hazard
****




Posts: 764
Registered: 24-6-2005
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2005 at 17:33


Thanks for the interesting link.

Based on the little tidbits of information I've seen, it seems that hydrazine sulfate may also work.

Just in case it doesn't, though, I wonder what would be the best way to get a dilute aqueous hydrazine solution from the sulfate?

Regards,
Joe
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 29-8-2005 at 17:43


Add a strong base, e.g. NaOH.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5115
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2005 at 02:38


BTW, you do know that hydrazine is volatile and a suspect carcinogen, don't you?
View user's profile View All Posts By User
jpsmith123
National Hazard
****




Posts: 764
Registered: 24-6-2005
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2005 at 02:13


In water or alcohol or some other solvent? What's the rest of the process?
The devil's in the details...what are they?

Quote:
Originally posted by neutrino
Add a strong base, e.g. NaOH.
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 31-8-2005 at 03:43


Something like this should happen:

N<sub>2</sub>H<sub>6</sub>SO<sub>4</sub> + 2 NaOH -> N<sub>2</sub>H<sub>6</sub>(OH)<sub>2</sub> + Na<sub>2</sub>SO<sub>4</sub>

N<sub>2</sub>H<sub>6</sub>(OH)<sub>2</sub> -> N<sub>2</sub>H<sub>4</sub> + 2 H<sub>2</sub>O

The spectator ions should be ignorable, although you know more about plating than I do. If they do pose a problem, see Rosco's posts in the hydrazine thread.
View user's profile View All Posts By User
ScienceSquirrel
International Hazard
*****




Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline

Mood: Dogs are pets but cats are little furry humans with four feet and self determination! :(

[*] posted on 15-11-2011 at 05:14


Quote: Originally posted by unionised  
BTW, you do know that hydrazine is volatile and a suspect carcinogen, don't you?


Cold dilute aqueous solutions of hydrazine should be relatively harmless though.
If he is making up the plating solution, doing the plating and then disposing of the solution safely he should be OK.


[Edited on 15-11-2011 by ScienceSquirrel]
View user's profile View All Posts By User
Jor
National Hazard
****




Posts: 950
Registered: 21-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2011 at 08:42


I've done it by dissolving copper(II) acetate in water, add ammonia until all initially formed Cu(OH)2 dissolves, add hydrazine hydrate and heat on a water bath.

http://amateurchemie.nl/viewtopic.php?f=20&t=404
View user's profile View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 15-11-2011 at 18:03


Jor does your method plate regular carbon steel ?or is this just for silver mirror type plating?

[Edited on 16-11-2011 by cyanureeves]
View user's profile View All Posts By User
Jor
National Hazard
****




Posts: 950
Registered: 21-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2011 at 03:21


I don't know. You should try it.
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1021
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 16-11-2011 at 06:00


is there some alternative to hydrazine here?
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1021
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 16-11-2011 at 06:00


is there some alternative to hydrazine here?
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6277
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 15-12-2015 at 04:49


I was thinking about creating a copper mirror. I have spotted a youtube video showing a method using hydrazine -- which is essentially the same as the method above. https://www.youtube.com/watch?v=tkFOzFNODUE

However, I do not have access to hydrazine and synthesising it will be a new step for me. I could go there but wondered if alternatives to the hydrazine exist.




View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 15-12-2015 at 06:30


Hydrazine is rather nasty - carcinogenic, explosive, low-boiling, and poisonous; I don't think playing with it in an amateur lab is a good idea.
View user's profile View All Posts By User