[*] posted on 2-11-2011 at 13:31
Which elements do you have in its pure state ?


With this question I mean 98+ % unalloyed, so 18ct gold is not considered unmixed 'elemental gold', but plain (non stainless) steel can be considered as elemental iron as its content is more than 99% Fe.

Lets kick off:

Li (in lithium batteries), C (in the wood stove or bbq charcoal, graphite electrodes, diamonds on grinding tools) , Na (tiny amounts made by NaOH + Mg) Mg, Al, Si (some old wafers) , S, K (tiny amounts made from KOH + Mg), Ti, Fe, Ni, Cu, Zn, Ag, Cd (small amounts) , Pt (one of the two type S thermocouple wires) Au, Hg, Pb.

When mixed (but still elemental) , a lot more: N,O,Ar (in air), P (matchboxes), V, Cr, Co (tool and stainless steels, Kanthal wire, type K thermocouple wires), Rh (in type S thermocouples), Pd (some white golds), Nd (in magnets).


[Edited on 2011-11-2 by metalresearcher]

[Edited on 2011-11-2 by metalresearcher]
View user's profile View All Posts By User
Adas
National Hazard
****




Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline

Mood: Sensitive to shock and friction

[*] posted on 2-11-2011 at 13:41


Acetone, butane, probably KMnO4, N2O, Sulfur, Diethyl ether, KNO3, NH4NO3, maybe Zn.
View user's profile Visit user's homepage View All Posts By User
kmno4
International Hazard
*****




Posts: 1495
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2011 at 13:58


Aha.
Don't forget about S-H-I-T (T=tritium)
View user's profile View All Posts By User
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 2-11-2011 at 14:19


You can't really say you've got nitrogen just because you've got air... Either you're talking about reasonably pure elements of mixtures.

I'll include the ones stored in pure state, not the ones I can isolate, like hydrogen, oxygen, nitrogen, or buy (helium).
Lithium, carbon, neon, sodium, magnesium, aluminium, phosphorus, sulphur, chlorine, calcium, iron, copper, zinc, arsenic, bromine, cadmium, tin, tellurium, iodine, mercury, lead.

I think that's all.




View user's profile Visit user's homepage View All Posts By User
phlogiston
International Hazard
*****




Posts: 1378
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 2-11-2011 at 17:17


Gasses: H2, He, Ar, N2, O2
Alkali metals: Li, Na, K
Alkaline earth: Mg, Ca, Sr
D-block: Y, La, Ti, Zr, V, Ta, Cr, Mo, W, Fe, Ru, Co, Ni, Pd, Pt, Cu, Ag, Eu, Zn, Cd, Hg
Halogens: Cl2, Br2, I2
f-block: Ce, Pr, Eu
Other: S, Se, Te, As, Sb, Bi, P, Ge, Si, C, Sn, Pb, Al, In

Still a long way to go to complete the table. I haven't bought any of those (either prepared them myself or they were kind gifts).




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8011
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-11-2011 at 23:53


I have most elements, of the stable elements I only miss F, Rb, U, Rh. A few other samples are only small pieces. I have pictures of all elements I have on my website:

http://woelen.homescience.net/science/chem/compounds/index2....

[Edited on 3-11-11 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
rstar
Hazard to Others
***




Posts: 138
Registered: 22-9-2011
Location: Besides valence shell
Member Is Offline

Mood: Dark

[*] posted on 3-11-2011 at 01:50


Anyone got F2 ?? ;)



"A tidy laboratory means a lazy chemist "
- Jöns Jacob Berzelius
View user's profile Visit user's homepage View All Posts By User
Chemistry Alchemist
Hazard to Others
***




Posts: 403
Registered: 2-8-2011
Location: Australia
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2011 at 01:52


Pretty sure my Elements are Sulfur, Aluminum, Cobalt, Lithium, Lead, Copper, Iron, Silver, Gold, Phosphorus, Zinc, Bismuth, Iodine, Magnesium, Carbon, Mercury, Silicon, Nickel, Neodymium (in magnet), Boron (in Magnet) and maybe Samarium from a magnet, still need to confirm if it is or not



View user's profile Visit user's homepage View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 3-11-2011 at 04:04


Woelen, that's a mighty nice collection!

The only elemental stuff that's a bit exotic, aside from the common metals and off-the-shelf materials, would be an ounce of reagent-grade silver, a square foot of titanium metal sheet, and about 2 or 3 grams of elemental arsenic. i used to have reagent grade bromine and iodine but the iodine evaporated completely and the bromine was way too corrosive and oxidizing even in its original 100 ml bottle so I got rid of it.

Robert





--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
LanthanumK
Hazard to Others
***




Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2011 at 04:40


I have pure H, Li, Mg, Co, Fe, Ni, Cu, Zn, Cd, Hg, Cr, Mo, I2, S, O2, He, Ne, Ar, Kr, Xe, W, Pt, Au, Ag, Al, C, Si, Ge, Sn, Pb, Bi, N2, and Sb.



hibernating...
View user's profile Visit user's homepage View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2011 at 09:42


So far I've got the following pure elements in my collection:
Alkali & Alkaline Earth Metals: H (not an alkali, but it's in this column), Li, Na, Mg
Transition Metals: V, Cr, Mn, Fe, Ni, Cu, Zn, Zr, Ag, W, Au, Hg
Metalloids: B, C, O, Al, Si, P, S, Ga, In, Sn, Pb, Bi
Halogens: I
Noble Gases: He, Ar, Kr, Xe
Lanthanides & Actinides: Po - U (represented by my uranium ore sample, generated through decay of the U), Am

That's 35 total, if you don't count the ones I claim through decay chains.

My Cu, In, Bi, Pb, and Ga samples are all semiconductor grade very high 6N purity (99.9999%) kindly donated by a coworker. Many of the other transition metals I made myself through thermites and other experiments, so probably aren't terribly pure. I'm trying to make as many of these as possible myself, because it's boring to just go buy everything.

I'm currently working on extracting Nd from magnets, so hopefully will be adding that soon!

I'm also building a large display unit for all this, and once that's done I'll make a video about it as well as the collection itself. Lots of work ahead of me though!
View user's profile Visit user's homepage View All Posts By User
metalresearcher
National Hazard
****




Posts: 755
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 3-11-2011 at 10:09


Nice to read these reactions.

@woelen: Where did you get your samples ? It seems they are from www.smart-elements.com ?

@MrHomeScientist: You got the U by a thermite reaction of uranium ore with Al powder ? When Po is a decay product you can also include Th and Rn. And also Ar as that is a decay product of K-40 of which your body alone has about 20mg.

@LanthanumK: I miss La in your list :-)

[Edited on 2011-11-3 by metalresearcher]
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2011 at 11:35


Quote: Originally posted by metalresearcher  
@MrHomeScientist: You got the U by a thermite reaction of uranium ore with Al powder ? When Po is a decay product you can also include Th and Rn. And also Ar as that is a decay product of K-40 of which your body alone has about 20mg.

No unfortunately I don't have pure U metal yet, just a sample of its ore. So I use that one sample to basically count for every element in uranium's decay chains - for some of them this is the only way to collect (like astatine), and others I just don't have a good sample of yet (like thorium).

I've never heard of a uranium thermite, it might work but the raw ore would have lots of impurities in it. I'd be reluctant to try anyway it because of the possibility of spewing radioactive dust out of the reaction as it burns!
View user's profile Visit user's homepage View All Posts By User
Endimion17
International Hazard
*****




Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline

Mood: speeding through time at the rate of 1 second per second

[*] posted on 3-11-2011 at 11:44


Yellowcake thermite works. That's how first samples of the metal were made, afterall. And it's an old textbook example of thermite reaction.

But I advise you strongly not to do it. Ever.




View user's profile Visit user's homepage View All Posts By User
Wizzard
Hazard to Others
***




Posts: 337
Registered: 22-3-2010
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2011 at 12:15


I would consider pure salts in the collection for those hard-to-get elements (I have a very small amount of pure thorium salt in my posession). But Iron, I wouldn't consider 99% iron as elementally pure- Those impurities change the characteristics of the substance substancially :) Iron is soft like gold when 9 5's pure, I believe.

My favorite pure substances in my collection is a few KG single crystal silicon dioxide, and all my crystals of Au, Ag, Pt, Pd, Rh, Re, Mg, S, Os and V :) Everything else is just a chunk of element.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8011
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 3-11-2011 at 23:50


Quote: Originally posted by metalresearcher  

@woelen: Where did you get your samples ? It seems they are from www.smart-elements.com ?
No, I hardly purchased anything from www.smart-elements.com. From them I only purchased some compounds (e.g. Rb2CO3). The elements are either from eBay, or from diverse people, who offered me samples of elements for very good prices. I even got some for free, just because of my website :o

I also had a few elements from the USA-based company Emovendo (beryllium, selenium, silver, tellurium) for exceptionally good prices (e.g. 30 grams selenium 99.999% for only $8, 30 grams silver 99.95% for just $12.50, 30 grams beryllium 99% for just $30), but unfortunately this company stepped out of the elements business and now they only sell science toys and lots of magnets in all kinds of shapes.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
LHcheM
Harmless
*




Posts: 37
Registered: 20-2-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-11-2011 at 01:59


Hydrogen, Helium, Lithium, Carbon, Nitrogen, Oxygen, Neon, Magnesium, Aluminium, Phosphorus (btw, what can I do with this? it's Red P), Sulphur, Chlorine, Argon, Iron, Copper, Zinc, Silver, Gold, Lead, Molybdenum, Tungsten (again, what can I do with this?), Bromine, Iodine, Barium =P
View user's profile View All Posts By User
Ephoton
Hazard to Others
***




Posts: 463
Registered: 21-7-2005
Member Is Offline

Mood: trying to figure out why I need a dark room retreat when I live in a forest of wattle.

[*] posted on 10-11-2011 at 18:25


sexium :)

sorry couldnt help my self




e3500 console login: root
bash-2.05#

View user's profile View All Posts By User
mr.crow
National Hazard
****




Posts: 884
Registered: 9-9-2009
Location: Canada
Member Is Offline

Mood: 0xFF

[*] posted on 11-11-2011 at 08:57


I have a nice little collection

Home made:
Iodine (my favorite, so beautiful), S, Ag powder

Purchased:
Na, Mg, Si, Ge, Pd, Pt, Au, Hg

I plan on making Cu powder sometime soon

Most of the elements are silvery metals, not too interesting

yellowcake thermite, lol




Double, double toil and trouble; Fire burn, and caldron bubble
View user's profile View All Posts By User
Wizzard
Hazard to Others
***




Posts: 337
Registered: 22-3-2010
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2011 at 09:02


Mr.crow, do you have crystalline Sulfur? It's very beautiful, and a sample is clear/yellow and doesn't damage easily due to handling/air. Highly recommended :)