Loading [MathJax]/jax/output/HTML-CSS/fonts/TeX/fontdata.js
Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Calcium Nitrate Production
chipster1234
Harmless
*




Posts: 10
Registered: 5-7-2011
Member Is Offline

Mood: No Mood

smile.gif posted on 5-7-2011 at 17:27
Calcium Nitrate Production


Im trying to make calcium nitrate in the lab. Based on customer requirements they would like to synthesis calcium nitrate using nitric acid as their base raw material

1) im using nitric acid to react with calcium carbonate
unfortunately im experiencing a huge amount of sludge/precipitate formation.

based on the equation : CaCO3 + 2HNO3 = Ca(NO3)2 + CO2 + H2O. (i just cant see where the sludge would come from???)
can anyone help me please?

2) is there any other material that i can use where sludge doesnt appear? i have tried using Ca(OH)2 but there is huge amounts of precipitation

3) could the precipitate actually be calcium nitrate itself?


View user's profile View All Posts By User
barley81
Hazard to Others
***




Posts: 481
Registered: 9-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 17:56


Are you sure that your reactants are pure? Calcium nitrate is very soluble, so this shouldn't happen. Did you add any water to the reaction?
View user's profile View All Posts By User
chipster1234
Harmless
*




Posts: 10
Registered: 5-7-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 18:22


the HNO3 is ~54% purity
whereas the Calcium Carbonate is >90% pure

so to answer your question, yes we do have water coming from the HNO3 source as it is only 54%. (*smile*)
may i know why you ask if i have added water?

From what im doing is that, i will react the reactants and then allow the sludge to settle down before decanting/seperating the liquid from the sludge. the liquid would be calcium nitrate of approximately 55% strength.

the sludge would be disposed off. my main task would be to eliminate this sludge if possible. any ideas?
View user's profile View All Posts By User
barley81
Hazard to Others
***




Posts: 481
Registered: 9-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 18:37


I have no idea then. I asked if you added water because if the nitric acid were 70% calcium nitrate would ppt. Maybe you could test the sludge for its composition? I don't have very much lab experience thus far, I'm only thinking of some possibilities.
View user's profile View All Posts By User
hkparker
National Hazard
****




Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 18:44


>90% pure isn't saying much. My first thought is that because nitric acid is an oxidizing agent it could oxidize the CaCO3 to CaO but if that was possible it would probably need to involve RFNA.

Probably impurities. Wikipedia says calcium nitrate can be produced this way without problem (followed by neutralization with ammonia).

Try dissolving some of you CaCO3 in HCl and see if you can get it all to dissolve. If not, its almost certainly an impurity.




My YouTube Channel

"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
View user's profile Visit user's homepage View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 5-7-2011 at 18:48


Are you using a stoichiometric excess of calcium carbonate? Have you neutralized the precipitate with NH<sub>3</sub>(aq)?

What are the characteristics of the sludge and of the decanted liquid and its residue after evaporation? (mass, solubility, ph, melting point, etc.)

Calcium nitrate tetrahydrate solubility in water:
102 g/100 mL (0 °C)
129 g/100 mL (20 °C)
363 g/100 mL (100 °C)

edit: damn, beat me to it HK! ;)

[Edited on 6-7-2011 by Bot0nist]




U.T.F.S.E. and learn the joys of autodidacticism!


Don't judge each day only by the harvest you reap, but also by the seeds you sow.
View user's profile View All Posts By User
hkparker
National Hazard
****




Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 18:59


Hey this aint no race Bot0nist ;)

I would agree more info in needed.




My YouTube Channel

"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
View user's profile Visit user's homepage View All Posts By User
chipster1234
Harmless
*




Posts: 10
Registered: 5-7-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 19:21


thank you so much for your response

HK: will be sure to test out the CaCo3 with HCl But wont this give us a ppt as well seeing as CaCl2 is produced?


Botonist:

1) i am using HNO3 in excess about 2.2 moles excess to CaCO3.
2) will be sure to test out the sludge and its properties.
3) the whole reaction was not neutralised with NH3. may i know why is the neutralisation of HNO3 necessary? Can we use Ca(OH)2 instead of NH3?
View user's profile View All Posts By User
hkparker
National Hazard
****




Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 19:53


CaCl2 is soluble.

CaNO3 might be much less soluble in acidic conditions due to Le Chatelier's principle. As nitric acid produces NO3- ions, the solution will adjust by precipitating Ca(NO3)2, but I'm not sure if that would be true at these dilutions.

EDIT:

I would use ammonia or sodium carbonate solution as they are liquid. Sodium carbonate will let you know when the solution is neutral by no longer off gassing. See if the solid dissolves in a neutralized or very slightly acidic solution.

[Edited on 6-7-2011 by hkparker]




My YouTube Channel

"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
View user's profile Visit user's homepage View All Posts By User
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
*****




Posts: 1986
Registered: 2-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 5-7-2011 at 20:44


Yes, I rather suspect the "common ion effect" is at work. For example, sodium chloride is not very soluble in 20% concentrated hydrochloric acid. The best solution would be to dilute the nitric acid to a 5% concentration with water before reacting.




I'm not saying let's go kill all the stupid people...I'm just saying lets remove all the warning labels and let the problem sort itself out.
View user's profile Visit user's homepage View All Posts By User
Intergalactic_Captain
Hazard to Others
***




Posts: 228
Registered: 4-9-2004
Location: somewhere where i don\'t know where i am
Member Is Offline

Mood: frabjous

[*] posted on 5-7-2011 at 23:49


Sounds like you're in an industrial setting and someone's trying to use waste HNO3 from some other process. If that's the case, was it used in a nitration process?

The only contaminants in your CaCO3 should be CaO and Ca(OH)2. If it's raw, both should react just fine - If it's been calcined, you might have some fused chunks that seem like "sludge" but in reality are just reacting incredibly slowly.

If the acid is waste from a nitration process, it may contain some amount of H2SO4 or some soluble sulfates. If that's the case, your sludge is most likely precipitated CaSO4.

...Without knowing more about your raw materials, those are the two most plausible possibilities I can think of...




If you see me running, try to keep up.
View user's profile View All Posts By User
497
National Hazard
****




Posts: 778
Registered: 6-10-2007
Member Is Offline

Mood: HSbF6

[*] posted on 6-7-2011 at 04:01


CaSO4 seems very likely. It forms some of the sludgiest precipitates I've ever seen. It's terrible.
View user's profile View All Posts By User
Megamarko94
Hazard to Self
**




Posts: 68
Registered: 31-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 6-7-2011 at 05:33


it will take forever to cristalize it out since its hygroscopic.



View user's profile View All Posts By User