Harmless
*




Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline

Mood: Hard on... working!

thumbup.gif posted on 21-12-2005 at 07:23
good rubber solvent


Hi there!

Anyone can tell of good rubber solvent/solvents? (Just in case there is misunderstanding, I'm referring to the actual material (vulcanised cautchouc), not condoms!).

Found out that formaldehyde works, and I remember trementine could damage rubber seriously. Pentane/hexane/heptane are also on my list.

Cheers

Stricnine
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 21-12-2005 at 07:32


Try N-methyl pyrrolidone (NMP), butyrolactone.
Havent tested it, but NMP dissolves PVC flooring, so it might do the job with rubber, too.




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
garage chemist
chemical wizard
*****




Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 21-12-2005 at 09:17


Chloroform is also a good solvent for rubber as I found out accidentally.
If chloroform is not available, dichloromethane could be used as a substitute, the solvent properties of the two are roughly the same.
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 21-12-2005 at 14:46


What exactly are you trying to do here? Are you after a solution of rubber in some solvent or are you just trying to get rid of some pesky rubber in an annoying place? If you want the latter, nitric acid might be worth a try.
View user's profile View All Posts By User
stricnine
Harmless
*




Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline

Mood: Hard on... working!

[*] posted on 22-12-2005 at 03:48


Yeah, acqua regia is my favourite, but I want to partially dissolve rubber to more or less get a solution of it - but agaion not dissolve it completely
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 22-12-2005 at 08:48


There are hundreds of different kinds of rubber from natural rubber to Kalrez (perfluoroelastomer). The kind of rubber will highly influence the selection of solvent. Please be more specific.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
stricnine
Harmless
*




Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline

Mood: Hard on... working!

[*] posted on 22-12-2005 at 10:20


It is simple rubber: 'ol natural vulcanised latex or SBR = car tyres broken down into chips. There ain´t no fluorine as far as I know. That's why I mentioned at the beginning "vulcanised caoutchouc".
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 22-12-2005 at 11:53


I missed your reference to cautchouc. I guess I am just too used to questions being asked in English on this forum.

My reference says that "oil, gasoline, kerosene, benzene, toluene, halogenated solvents, and diester lubes" will all attack SBR. I don't know which would be a good solvent, however.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
kazaa81
Hazard to Others
***




Posts: 368
Registered: 30-4-2004
Member Is Offline

Mood: ok

[*] posted on 22-12-2005 at 13:26


Maybe phosphorous oxychloride will work...
If I remember right, it was used in war first of using blistering agents (or similar) to damage the rubber of gas masks
View user's profile View All Posts By User
NERV
Hazard to Others
***




Posts: 152
Registered: 22-9-2002
Location: USA
Member Is Offline

Mood: Fluorinated

[*] posted on 22-12-2005 at 22:35


I personally wouldn’t use POCl3 as it is fairly hard to come by, and it’s defiantly not an armature chemist friendly compound. Plus a quick google search didn’t yield anything about it being able to dissolve rubber although I may be wrong about that.



Vir sapit qui pauca loquitur.
View user's profile View All Posts By User
stricnine
Harmless
*




Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline

Mood: Hard on... working!

[*] posted on 27-12-2005 at 18:05


I will be trying with Thioglycolate - permanent hair waving disulphide bond braeaker.

I will report on the results.

Keep on supporting!!

Stricnine




I am getting old. I used to push it aside with one hand... now I need both!
View user's profile View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 16-7-2010 at 23:21


US patent 4465535

Adhering Cured polymers or Prepolymers
To High Natural Rubber Elastomer

Reports that 1,2-Dichloroethane preps the surface well.

.
View user's profile View All Posts By User
aonomus
Hazard to Others
***




Posts: 361
Registered: 18-10-2009
Location: Toronto, Canada
Member Is Offline

Mood: Refluxing

[*] posted on 17-7-2010 at 05:04


I've recently learned the hard way, that toluene over 24h does indeed make suba-seal septa swell and soften into sticky messes.
View user's profile Visit user's homepage View All Posts By User
The WiZard is In
International Hazard
*****




Posts: 1617
Registered: 3-4-2010
Member Is Offline

Mood: No Mood

[*] posted on 17-7-2010 at 05:15


Quote: Originally posted by aonomus  
I've recently learned the hard way, that toluene over 24h does indeed make suba-seal septa swell and soften into sticky messes.



----
Stamp collectors use toluene to remove glue.
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 17-7-2010 at 05:15


Halocarbon solvents like CCl4, CHCl3, CH2Cl2, CH3CCl3, etc., should do the job, although they are mostly more expen$ive and may be liver toxins, and have largely gone out of favor for damaging the ozone layer when their vapors are released to the atmosphere.
View user's profile View All Posts By User
Vogelzang
Banned





Posts: 662
Registered: 26-4-2008
Member Is Offline

Mood: No Mood

[*] posted on 17-7-2010 at 08:07


Perchloroethylene (tetrachloroethylene) is used as a dry cleaning solvent. How hard is that to get OTC, ie. not from a chemical company? Butyl acetate is used as a solvent for rubber cement.
View user's profile View All Posts By User
Melgar
Anti-Spam Agent
*****




Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline

Mood: Estrified

[*] posted on 17-7-2010 at 10:34


Nonflammable paint strippers can be distilled to get CH2Cl2. They're only around $20 a gallon too.
View user's profile View All Posts By User
redox
Hazard to Others
***




Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline

Mood: Chalcogenetic

[*] posted on 10-6-2011 at 16:10


Quote: Originally posted by Vogelzang  
Perchloroethylene (tetrachloroethylene) is used as a dry cleaning solvent. How hard is that to get OTC, ie. not from a chemical company?


Tetrachloroethylene is sold as a grease-remover in electronics. I bought a can of it today in Home Depot for 8 dollars.




My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs

Newest video: Synthesis of Chloroform

The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
View user's profile Visit user's homepage View All Posts By User
Random
International Hazard
*****




Posts: 1021
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 11-6-2011 at 01:18


is there a way to extract elemental sulfur from rubber?
View user's profile View All Posts By User
redox
Hazard to Others
***




Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline

Mood: Chalcogenetic

[*] posted on 11-6-2011 at 08:27


Quote: Originally posted by Random  
is there a way to extract elemental sulfur from rubber?


Why would you want to do that? :o




My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs

Newest video: Synthesis of Chloroform

The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
View user's profile Visit user's homepage View All Posts By User
Mr. Wizard
International Hazard
*****




Posts: 1042
Registered: 30-3-2003
Member Is Offline

Mood: No Mood

[*] posted on 11-6-2011 at 15:14


Try a search on that poopular search engine using " rubber cement thinner " and see if will give you what you need. It might be best.
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1021
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 13-6-2011 at 00:17


Quote: Originally posted by redox  
Quote: Originally posted by Random  
is there a way to extract elemental sulfur from rubber?


Why would you want to do that? :o


I have rubber, but I odn't have enough sulfur.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2699
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 16-6-2011 at 13:02


It is not possible to extract sulfur from vulcanized rubber, as it is crosslinked chemically to the rubber polymer chains. You can buiy sulfur cheap at most drugstores or agrocultural supply stores, as it kills fungus well, and is used as "snake repellent".

Toluene is a common solvent for rubber cement, which is a solution of rubber in solvent. Mixtures of Toluene, Xylene, hexanes, and such are all used. If you want to be able to remove the solvent, like for a glue, that is a good solution. Chloronated solvents also work well, but are very volatile and more hazardous.

NMP and other high boiling solvents will slowly dissolve rubber and many other materials, but the resultant goo is hard to do anything further with.
View user's profile View All Posts By User
Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 20-6-2011 at 18:28


Quote: Originally posted by Dr.Bob  
It is not possible to extract sulfur from vulcanized rubber..........


Care to rephrase that? lol




View user's profile View All Posts By User
barley81
Hazard to Others
***




Posts: 481
Registered: 9-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 21-6-2011 at 04:22


I read somewhere that gasoline can be used to make rubber cement, but it was used with "natural rubber". I'm not sure it would dissolve vulcanized rubber as well or at all.
View user's profile View All Posts By User