minimal gallium to prevent aluminum oxidation?
There has been a little bit of talk about generating hydrogen from aluminum/gallium alloys... The thing is gallium is a little expensive.. One
researcher uses 20%/80% gallium/aluminum to keep the aluminum reactive. Seems like that ratio might be a little high, you only need just enough
gallium to prevent the oxidation, so could 1% work also?
Can anyone speculate on the minimum amount of gallium in an aluminum/gallium alloy required to keep the aluminum reactive?
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
You're not preventing oxidation, you're encouraging it with the gallium. The surface layer of Al2O3, dry or hydrated, slows down further oxidation.
Gallium or mercury cause defects in this surface, allowing oxidation to continue. An old demo was to paint a little solution of a mercury compound
onto a piece of Al, which would then oxidises away with the growth of a powdery growth of Al2O3. This is also the reason shipping gallium by air is a
hassle, it penetrates Al and its alloys, weakening the inter-grain boundaries and allowing oxidation of the bulk metal.
So you need enough gallium to insure that a coherent layer of Al2O3 does not form. As some of the gallium gets trapped in the oxide flaking off the
bulk Al, you need enough of it to always be interfering with the formation of good quality films of Al2O3.
Don't know the minimum required, from what I've read it is a fairly large proportion. This might be of interest: http://www.slideshare.net/cimon9999/e-keane-journal-paper-on...
and this one as well
http://www1.eere.energy.gov/hydrogenandfuelcells/pdfs/alumin...
[Edited on 7-5-2011 by not_important]
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
Can Gallium salts not be used simular to how HgCl2 is used to lower the requirments of Mercury needed.
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
beergod
Harmless
Posts: 23
Registered: 19-2-2011
Member Is Offline
Mood: No Mood
|
|
Well it seems industry standard is 20% gallium 80% aluminum. Anything less will give very unsatisfactory results.
|
|