Pthtalic acid OTC
I saw on some threads that phtalic acid can be obtained by saponification of ester whihc is in vinyl gloves. I Tried to find those gloves, but I can
only find white latex gloves everywhere.
Now, is there some other PVC product that has a lot of that ester, maybe PVC wire isolation or something else?
|
|
Megamarko94
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 68
Registered: 31-12-2010
Member Is Offline
Mood: No Mood
|
|
you saw it on nurdrage's channel
and i don't know where you can find something like that.
I probably wont be able to find them either
|
|
ItalianChemist
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 172
Registered: 26-1-2011
Location: Italy
Member Is Offline
Mood: No Mood
|
|
I obtained pthalic acid from hydrolisys of pthalic anhydride!
I put some phtalic anhydride in a few ml of water and I refluxed the mixture until the phtalic anhydride disappeared. Then I cold the solution in an
ice bath and the pthalic acid precipitated.
I think that with other PVC materials the extraction and basic hydrolisys doesn't work, because diethylexylphtalate is used in gloes to make them more
soft!
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Quote: Originally posted by Random ![](images/xpblue/lastpost.gif) |
Now, is there some other PVC product that has a lot of that ester, maybe PVC wire isolation or something else? |
PVC shower curtain.
Also see:
http://www.sciencemadness.org/talk/viewthread.php?tid=6573&a...
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
hkparker
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline
Mood: No Mood
|
|
Shower curtains can be really inefficient to extract from. See UnintentionalChaos's youtube video about it.
Part 1, 2 and 3:
http://www.youtube.com/watch?v=cooRCFa3J3s
http://www.youtube.com/watch?v=qESSbS2EM-I
http://www.youtube.com/watch?v=zlf4kbs0y7Q
My YouTube Channel
"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I have to agree. I checked my notebook and see that the yield was terrible.
--------
I watched the U-tube videos: wonderful! But I don't remember a yield of PA being stated - did I miss it?
[Edited on 10-4-2011 by Magpie]
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
redox
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline
Mood: Chalcogenetic
|
|
Well, it might be possible (if you had the time, money, apparatus, etc) to oxidize o-xylene to phthalic acid, no?
Mixed isomer xylene can be had at any well-stocked hardware store (Lowe's, Home Depot, Ace)
Just a suggestion, however inconvenient. ![;)](./images/smilies/wink.gif)
[Edited on 11-4-2011 by redox]
|
|
hkparker
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 601
Registered: 15-10-2010
Location: California, United States
Member Is Offline
Mood: No Mood
|
|
I don't think it was stated, but this was adressed because he doesn't know for sure what fatty alcohol groups were attached the the phtalate group, so
yield cannot be calculated. When he titrates to find out what fatty alcohol group it was then I bet we'll hear what the yeild was.
My YouTube Channel
"Nothing is too wonderful to be true if it be consistent with the laws of nature." -Michael Faraday
|
|
jamit
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 18-6-2010
Location: Midwest USA
Member Is Offline
Mood: No Mood
|
|
Where do you get PVC gloves? Does it have to say PVC or can it be any vinyl gloves? thanks.
|
|
kuro96inlaila
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 96
Registered: 21-6-2010
Location: Malaysia
Member Is Offline
Mood: Quietly thinking
|
|
Is there a way to get phthalic acid from potassium hydrogen phthalate?
Potassium hydrogen phthalate is easier to get than phthalic acid (well,some people may having these problem.).
|
|
ItalianChemist
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 172
Registered: 26-1-2011
Location: Italy
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by kuro96inlaila ![](images/xpblue/lastpost.gif) | Is there a way to get phthalic acid from potassium hydrogen phthalate?
Potassium hydrogen phthalate is easier to get than phthalic acid (well,some people may having these problem.). |
It's very simple, you have to add some concentrated HCl to a solution of potassium hydrogen pthalate and then pthalic acid crystallize out!
|
|
kuro96inlaila
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 96
Registered: 21-6-2010
Location: Malaysia
Member Is Offline
Mood: Quietly thinking
|
|
I never expect it to be so simple!![:)](./images/smilies/smile.gif)
Thanks ItalianChemist!
|
|
ItalianChemist
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 172
Registered: 26-1-2011
Location: Italy
Member Is Offline
Mood: No Mood
|
|
If you want I can try and take some photographs! ![;)](./images/smilies/wink.gif)
EDIT:
Ok, I've just tried!
I used:
-Phtalic acid(made from pure pthalic anhydride and water)
-Potassium hydroxide
-Bromotymol blue
-Sulphuric acid 95%
![1.JPG - 52kB](https://www.sciencemadness.org/whisper/files.php?pid=206628&aid=13560)
I neutralized te phtalic acid with a concentrate solution of potassium hydroxide, I add a drop of bromotymol blue to take the pH acid.
![2.JPG - 55kB](https://www.sciencemadness.org/whisper/files.php?pid=206628&aid=13562)
Then I filtered the solution to remove unreacted pthalic acid and I add 5ml of concentrated sulphuric acid, The pthalic acid cristallized out!
[Edited on 12-4-2011 by ItalianChemist]
[Edited on 12-4-2011 by ItalianChemist]
|
|