separation of lead from tin in ppm level
I have pure tin (99.9%). I want to electrolytically refine it to 99.999%. Main aim is to remove Pb(which is in ppm quantity) from the pure
tin(99.9).Also want to remove Bismuth from 99.9% tin.
Any suggestions how to do this.
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
generaly the lead and the bismuth is more chemicaly resistan than the tin
you can rafine it electrochemicaly.
|
|
kumarsriit
Harmless
Posts: 5
Registered: 3-1-2011
Member Is Offline
Mood: No Mood
|
|
how to separate tin and lead at ppm level
|
|
kmno4
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1495
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by kumarsriit ![](images/xpblue/lastpost.gif) | I have pure tin (99.9%). I want to electrolytically refine it to 99.999%. Main aim is to remove Pb(which is in ppm quantity) from the pure
tin(99.9).Also want to remove Bismuth from 99.9% tin.
Any suggestions how to do this. |
I know that by electrolysis (Sn anode/cathode, SnSO4 sol.) easily you can get 99,995% Sn. Possibly, repeated (few times) process can give you higher
Sn content.
If you want to remove ppm Pb, the only "simple" method I know is zone melting.
I have just found free article about zone melting and tin:
Code: | http://www.informaworld.com/smpp/ftinterface~content=a762701496~fulltext=713240930~frm=content |
[Edited on 7-1-2011 by kmno4]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by kmno4 ![](images/xpblue/lastpost.gif) | I know that by electrolysis (Sn anode/cathode, SnSO4 sol.) easily you can get 99,995% Sn. Possibly, repeated (few times) process can give you higher
Sn content.
If you want to remove ppm Pb, the only "simple" method I know is zone melting.
|
You say ‘easily’ but I think that’s true only as in ‘theoretically easily’. When I electrolysed a solution of SnCl2 (12 V, 4 A) I got quick
formation of what you could call a ‘tin tree’ but while the tin in there may well be highly pure it’s more like tin sponge, with loads of
electrolyte locked into it. To properly obtain solid tin metal specific conditions of voltage and current densities are required, or so I believe. If
you have any information/experience with those conditions I’m all ear.
Interesting stuff about zone refining… Good luck with rotating to 3000 rpm though!
[Edited on 7-1-2011 by blogfast25]
|
|
kmno4
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1495
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline
Mood: No Mood
|
|
The method I gave is normal practical procedure. Exact formula you can find in Karakin and Angelov (page 435). There is also variant with SnCl2 but in
this case Sn is obtained as thick powder.
[Edited on 7-1-2011 by kmno4]
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Karakin and Angelov (page 435): if you have those conditions at hand could you post a summary here?
|
|
kumarsriit
Harmless
Posts: 5
Registered: 3-1-2011
Member Is Offline
Mood: No Mood
|
|
purifying tin
Is "karaklin,angelov" name of the book. If it is what is the complete name of the book. Also can give the condition (composition, current etc) to get
99.999% tin by electrolysis in stannous sulphate-sulphuric acid system.
Thanks
|
|
kmno4
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1495
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline
Mood: No Mood
|
|
Ю.В. Карякин, И. Ангелов -
"Чистые химические
вещества"
(in Russian of course). You can find it freely available in DJVU format, however it seems to me that I have seen also PDF version of this book.
|
|
kumarsriit
Harmless
Posts: 5
Registered: 3-1-2011
Member Is Offline
Mood: No Mood
|
|
@Kmno4
The russian language book you mentioned in djvu format has 402 pages. how to get the process u mentioned in page 435. Is there english version of
this book available. please respond.
thanks
|
|
kmno4
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1495
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline
Mood: No Mood
|
|
I gave page number from another edition of this work.
You have to search a word "oлово" = tin in Russian and possibly it is on page 295. In another case - use index and search
"oлово". Unfortunately I know nothing about English edition.
The most possibly it is not translated at all.
Very pity, because I know only few words in Russian language. ![:mad:](./images/smilies/mad.gif)
However, translation of this particular preparation is not very difficult.
|
|
kumarsriit
Harmless
Posts: 5
Registered: 3-1-2011
Member Is Offline
Mood: No Mood
|
|
@KMno4
can you please get the russian translation of that particular page mentioned in earlier post regarding tin refining. It not be necessary in chaste
english. at least paste the translation of brief summary of process.
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
Just post the link here, and I will translate the text (from Russian of-course).
|
|