Platinum Recovery
All,
This is my first post and very first time here. I have heated an automobile catalysts in concentrated Aqua Regia for 5hrs and stannous chloride tested
positive for Pt. Here is the picture of the solution after 10mins of boiling in AR.
Then I tested it with stannous chloride and here is the result
The same solution after being left outside over night, it changed color as you can see here.
Just to test, 20ml of the solution is being evaporated on steam bath to get rid of NOxx and added 20ml of HCl after it turned to syrup. This step
repeated 2 times
Solution after being on steam bath for few mins
After hydration the syrup with HCL I added half of its volume water.
I added ammonium chlorate to dilute solution while being on steam bath, and all i got was some small amoutn of white fine powder at the bottom at the
picture
Now can someone tell me what I do wrong here? I mean how can i get the yellow powder that is pt?
Thanks
Kev
|
|
hissingnoise
International Hazard
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Your solution is likely to contain several different metal ions and separation will almost certainly be difficult.
Chloroplatinic acid, BTW, is readily reduced by strong heating.
http://herkules.oulu.fi/isbn9514269543/html/x382.html
|
|
Fleaker
International Hazard
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
You would do well to avoid heating chloroplatinic acid if you want to avoid metal losses.
See my thread here:
http://www.sciencemadness.org/whisper/viewthread.php?tid=972...
[Edited on 2-1-2011 by Fleaker]
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|